High temperature proton exchange membranes based on polybenzimidazoles for fuel cells

被引:1174
|
作者
Li, Qingfeng [1 ]
Jensen, Jens Oluf [1 ]
Savinell, Robert F. [2 ]
Bjerrum, Niels J. [1 ]
机构
[1] Tech Univ Denmark, Dept Chem, Energy & Mat Sci Grp, DK-2800 Lyngby, Denmark
[2] Case Western Reserve Univ, Dept Chem Engn, Cleveland, OH 44106 USA
关键词
High temperature proton exchange membrane; Fuel cell; Polybenzimidazole (PBI); Phosphoric acid; Cross-linking; Durability; ACID-DOPED POLYBENZIMIDAZOLE; POLYMER ELECTROLYTE MEMBRANE; PRESSURE ELECTRICAL-CONDUCTIVITY; POLY(ARYLENE ETHER SULFONE); POLYARYL-BLEND-MEMBRANES; REDUCTION REACTION ORR; MICRO-COMBINED HEAT; PHOSPHORIC-ACID; INTERMEDIATE TEMPERATURE; OXYGEN REDUCTION;
D O I
10.1016/j.progpolymsci.2008.12.003
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
To achieve high temperature operation of proton exchange membrane fuel cells (PEMFC), preferably under ambient pressure, acid-base polymer membranes represent an effective approach. The phosphoricacid-doped polybenzimidazole membrane seems so far the most successful system in the field. It has in recent years motivated extensive research activities with great progress. This treatise is devoted to updating the development, covering polymer membrane casting, physicochemical characterizations and fuel cell technologies. To optimize the membrane properties, high molecular weight polymers with synthetically modified or N-substituted structures have been synthesized. Techniques for membrane casting from organic solutions and directly from acid solutions have been developed. Ionic and covalent cross-linking as well as inorganic-organic composites has been explored. Membrane characterizations have been made including spectroscopy, water uptake and acid doping, thermal and oxidative stability, conductivity, electro-osmotic water drag, methanol crossover, solubility and permeability of gases, and oxygen reduction kinetics. Related fuel cell technologies Such as electrode and MEA fabrication have been developed and high temperature PEMFC has been Successfully demonstrated at temperatures of up to 200 degrees C Under ambient pressure. No gas humidification is mandatory, which enables the elimination of the complicated humidification system, compared with Nafion cells. Other operating Features of the PBI cell include easy control of air flow rate, cell temperature and cooling. The PBI cell operating at above 150 degrees C can tolerate up to 1% CO and 10 ppm SO2 in the fuel stream, allowing for simplification of the fuel processing system and possible integration of the fuel cell stack with fuel processing units. Long-term durability with a degradation rate of 5 mu V h(-1) has been achieved Under Continuous operation with hydrogen and air at 150-160 degrees C. With load or thermal cycling, a performance loss of 300 mu V per cycle or 40 mu V h(-1) per operating hour was observed. Further improvement Should be done by, e.g, optimizing the thermal and chemical stability of the polymer, acid-base interaction and acid management, activity and stability of catalyst and more importantly the catalyst support, as well as the integral interface between electrode and membrane. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:449 / 477
页数:29
相关论文
共 50 条
  • [21] Acid doped polybenzimidazoles based membrane electrode assembly for high temperature proton exchange membrane fuel cell: A review
    Haque, M. Ahsanul
    Sulong, A. B.
    Loh, K. S.
    Majlan, E. Herianto
    Husaini, T.
    Rosli, R. Emilia
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (14) : 9156 - 9179
  • [22] Synthesis of soluble polybenzimidazoles for high-temperature proton exchange membrane fuel cell (PEMFC) applications
    Chen, Jyh-Chien
    Chen, Ping-Yen
    Lee, Shih-Wei
    Liou, Geng-Lun
    Chen, Chun-Jung
    Lan, Yi-Hsin
    Chen, Kuei-Hsien
    REACTIVE & FUNCTIONAL POLYMERS, 2016, 108 : 122 - 129
  • [23] Catalyst Degradation in High Temperature Proton Exchange Membrane Fuel Cells Based on Acid Doped Polybenzimidazole Membranes
    Cleemann, L. N.
    Buazar, F.
    Li, Q.
    Jensen, J. O.
    Pan, C.
    Steenberg, T.
    Dai, S.
    Bjerrum, N. J.
    FUEL CELLS, 2013, 13 (05) : 822 - 831
  • [24] Preparation and Properties of Composite Proton Exchange Membranes from Troger's Base-based Polyimides/Polybenzimidazoles for Fuel Cells Operating in a Wide Temperature Range
    Zhong, Jian-Ming
    Dai, Jun-Ming
    Zhang, Yu
    Zhao, Qing-Mei
    Zhang, Xu
    Zhuang, Yong-Bing
    ACTA POLYMERICA SINICA, 2024, 55 (04): : 452 - 461
  • [25] New polybenzimidazoles for producing medium-temperature proton-exchange membranes
    Leikin, A. Yu.
    Rusanov, A. L.
    POLYMER SCIENCE SERIES C, 2009, 51 (01) : 8 - 11
  • [26] New polybenzimidazoles for producing medium-temperature proton-exchange membranes
    A. Yu. Leikin
    A. L. Rusanov
    Polymer Science Series C, 2009, 51 : 8 - 11
  • [27] Sulfonated Polybenzimidazoles for High Temperature PEM Fuel Cells
    Mader, Jordan A.
    Benicewicz, Brian C.
    MACROMOLECULES, 2010, 43 (16) : 6706 - 6715
  • [28] Highly durable proton exchange membranes for low temperature fuel cells
    Tang, Haolin
    Pan, Mu
    Wang, Fang
    Shen, Pei Kang
    Jiang, San Ping
    JOURNAL OF PHYSICAL CHEMISTRY B, 2007, 111 (30): : 8684 - 8690
  • [29] Dimensionally-stable phosphoric acid-doped polybenzimidazoles for high-temperature proton exchange membrane fuel cells
    Li, Xiaobai
    Ma, Hongwei
    Shen, Yanchao
    Hu, Wei
    Jiang, Zhenhua
    Liu, Baijun
    Guiver, Michael D.
    JOURNAL OF POWER SOURCES, 2016, 336 : 391 - 400
  • [30] Oxidative Degradation of Polybenzimidazole Membranes as Electrolytes for High Temperature Proton Exchange Membrane Fuel Cells
    Liao, J. H.
    Li, Q. F.
    Rudbeck, H. C.
    Jensen, J. O.
    Chromik, A.
    Bjerrum, N. J.
    Kerres, J.
    Xing, W.
    FUEL CELLS, 2011, 11 (06) : 745 - 755