Microstructure and Mechanical Properties of Laser-Welded DP Steels Used in the Automotive Industry

被引:21
|
作者
He, Hanbing [1 ]
Forouzan, Farnoosh [1 ]
Volpp, Joerg [2 ]
Robertson, Stephanie M. [2 ]
Vuorinen, Esa [1 ]
机构
[1] Lulea Univ Technol, Div Mat Sci, S-97187 Lulea, Sweden
[2] Lulea Univ Technol, Div Prod & Prod Dev, S-97187 Lulea, Sweden
关键词
laser welding; dual phase steel; similar; dissimilar welded joints; microhardness; tensile properties; fatigue;
D O I
10.3390/ma14020456
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aim of this work was to investigate the microstructure and the mechanical properties of laser-welded joints combined of Dual Phase DP800 and DP1000 high strength thin steel sheets. Microstructural and hardness measurements as well as tensile and fatigue tests have been carried out. The welded joints (WJ) comprised of similar/dissimilar steels with similar/dissimilar thickness were consisted of different zones and exhibited similar microstructural characteristics. The trend of microhardness for all WJs was consistent, characterized by the highest value at hardening zone (HZ) and lowest at softening zone (SZ). The degree of softening was 20 and 8% for the DP1000 and DP800 WJ, respectively, and the size of SZ was wider in the WJ combinations of DP1000 than DP800. The tensile test fractures were located at the base material (BM) for all DP800 weldments, while the fractures occurred at the fusion zone (FZ) for the weldments with DP1000 and those with dissimilar sheet thicknesses. The DP800-DP1000 weldment presented similar yield strength (YS, 747 MPa) and ultimate tensile strength (UTS, 858 MPa) values but lower elongation (EI, 5.1%) in comparison with the DP800-DP800 weldment (YS 701 MPa, UTS 868 MPa, EI 7.9%), which showed similar strength properties as the BM of DP800. However, the EI of DP1000-DP1000 weldment was 1.9%, much lower in comparison with the BM of DP1000. The DP800-DP1000 weldment with dissimilar thicknesses showed the highest YS (955 MPa) and UTS (1075 MPa) values compared with the other weldments, but with the lowest EI (1.2%). The fatigue fractures occurred at the WJ for all types of weldments. The DP800-DP800 weldment had the highest fatigue limit (348 MPa) and DP800-DP1000 with dissimilar thicknesses had the lowest fatigue limit (<200 MPa). The fatigue crack initiated from the weld surface.
引用
收藏
页码:1 / 14
页数:14
相关论文
共 50 条
  • [41] Effects of Heat Input on Microstructure and Mechanical Properties of Laser-Welded Mg-Rare Earth Alloy
    Dai, Jun
    Huang, Jian
    Li, Zhuguo
    Dong, Jie
    Wu, Yixiong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (01) : 64 - 70
  • [42] Microstructure, mechanical and electrical properties of laser-welded overlap joint of CP Ti and AA2024
    Kuryntsev, S. V.
    OPTICS AND LASERS IN ENGINEERING, 2019, 112 : 77 - 86
  • [44] Effect of laser power and welding speed on microstructure and mechanical properties of fibre laser-welded Inconel 617 thin sheet
    Kumar, Prabhat
    Saw, Kanhaiya
    Kumar, Uday
    Kumar, Ratnesh
    Chattopadhyaya, Somnath
    Hloch, Sergej
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2017, 39 (11) : 4579 - 4588
  • [45] Effect of laser power and welding speed on microstructure and mechanical properties of fibre laser-welded Inconel 617 thin sheet
    Prabhat Kumar
    Kanhaiya Saw
    Uday Kumar
    Ratnesh Kumar
    Somnath Chattopadhyaya
    Sergej Hloch
    Journal of the Brazilian Society of Mechanical Sciences and Engineering, 2017, 39 : 4579 - 4588
  • [46] Microstructures and Mechanical Properties for Laser Tailor Welded Blanks of DP590 and Low Carbon Steels
    Wei Chunhua
    Zhang Jing
    Yang Shanglu
    Tao Wu
    Wu Fengshun
    Xia Weisheng
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 : 68 - 73
  • [47] Mechanical Properties of Laser-Welded Multi-Material Tailor-Welded Blanks
    Nam, Ki Woo
    Park, Sang Hyun
    Lee, Kyu Hyun
    Lee, Mun Yong
    TRANSACTIONS OF THE KOREAN SOCIETY OF MECHANICAL ENGINEERS A, 2012, 36 (08) : 857 - 863
  • [48] Stress corrosion cracking of laser-welded stainless steels
    Kwok, C. T.
    Lo, K. H.
    Chan, W. K.
    PROCEEDINGS OF THE 1ST INTERNATIONAL JOINT SYMPOSIUM ON JOINING AND WELDING, 2013, : 547 - 552
  • [49] Microstructure and Mechanical Properties of Adding Adhesive-Layer Laser-Welded Joints of DP590 Dual-Phase Steel and 6061 Aluminum Alloy
    Zhou, Dianwu
    Li, Tian
    Xu, Shaohua
    Liu, Jinshui
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (12) : 3295 - 3304
  • [50] Fatigue resistance and influence of cutting technology on the mechanical properties of modern steels used in the automotive industry
    Ulewicz, Robert
    Novy, Frantisek
    12TH INTERNATIONAL SCIENTIFIC CONFERENCE OF YOUNG SCIENTISTS ON SUSTAINABLE, MODERN AND SAFE TRANSPORT, 2017, 192 : 899 - 904