Role of cold rolled followed by annealing on improvement of hydrogen induced cracking resistance in pipeline steel

被引:31
|
作者
Mohtadi-Bonab, M. A. [1 ]
Eskandari, M. [2 ]
Szpunar, J. A. [3 ]
机构
[1] Univ Bonab, Dept Mech Engn, Velayat Highway, Bonab, Iran
[2] Shahid Chamran Univ Ahvaz, Fac Engn, Dept Mat Sci & Engn, Ahvaz, Iran
[3] Univ Saskatchewan, Dept Mech Engn, 57 Campus Dr, Saskatoon, SK S7N5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen induced cracking; Crystallographic texture; X-ray diffraction; Pole figure; Electron backscatter diffraction; STRESS-CORROSION CRACKING; CRYSTALLOGRAPHIC TEXTURE; MICROSTRUCTURE; SUSCEPTIBILITY; PERMEATION; INCLUSIONS; FRACTURE; GROWTH;
D O I
10.1016/j.engfailanal.2018.04.044
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, we investigated the effect of cold rolled followed by annealing on hydrogen induced cracking susceptibility in an API X60 pipeline steel. To this, we carried out cold rolling on X60 steel up to 20%, 50% and 90% in thickness reduction to change the microstructure and texture of steel. Then, we annealed all specimens at 850 degrees C for 90 s. We studied all tested specimens by electron backscatter and X-ray diffraction techniques. EBSD results showed that the grain refinement process was properly done via cold rolling and annealing treatments in tested specimens. However, the dislocation density was high for all tested steels. Moreover, electrochemical hydrogen charging experiment on tested steels proved that all specimens were still highly susceptible to hydrogen induced cracking. Therefore, we increased the annealing temperature and its duration of the 90% cold rolled specimen (the specimen with finest grains) up to 950 degrees C for 5 min. Interestingly, there was no HIC crack on this steel after hydrogen charging experiment. EBSD measurements on this steel showed strong textures of {100}//ND and {111}//ND. As a result, such strong textures, low Kernel Average Misorientation data, a high proportion of recovered grains and coincidence site lattice boundaries were recognized as the most important reasons for the highest HIC resistance in the mentioned steel.
引用
收藏
页码:172 / 181
页数:10
相关论文
共 50 条
  • [31] Development of continuous annealing technology for cold rolled steel sheet
    Song, Jia
    Shanghai Jinshu/Shanghai Metals, 21 (04): : 47 - 51
  • [32] Transformation of cold rolled austenitic stainless steel during annealing
    Jinshu Rechuli Xuebao/Transactions of Metal Heat Treatment, 18 (04): : 5 - 9
  • [33] A study on the annealing characteristics of BAF for cold rolled steel strip
    Kim, SK
    Kim, MK
    Jeon, EC
    KSME INTERNATIONAL JOURNAL, 1998, 12 (02): : 330 - 337
  • [34] Contribution of the microtexture evolution induced by plastic deformation on the resistance of a hot-rolled pipeline steel to flat cleavage fracture and to brittle delamination cracking
    Tankoua, F.
    Crepin, J.
    Thibaux, P.
    Cooreman, S.
    Gourgues-Lorenzon, A-F
    INTERNATIONAL JOURNAL OF FRACTURE, 2022, 233 (02) : 211 - 237
  • [35] Contribution of the microtexture evolution induced by plastic deformation on the resistance of a hot-rolled pipeline steel to flat cleavage fracture and to brittle delamination cracking
    F. Tankoua
    J. Crépin
    P. Thibaux
    S. Cooreman
    A.-F. Gourgues-Lorenzon
    International Journal of Fracture, 2022, 233 : 211 - 237
  • [36] Relationship between microstructure and hydrogen induced cracking behavior in a low alloy pipeline steel
    Jing Li
    Xiuhua Gao
    Linxiu Du
    Zhenguang Liu
    Journal of Materials Science & Technology, 2017, 33 (12) : 1504 - 1512
  • [37] The role of niobium in cold rolled trip steel
    Hulka, K
    MATERIALS SCIENCE, TESTING AND INFORMATICS II, 2005, 473-474 : 91 - 102
  • [38] Relationship between microstructure and hydrogen induced cracking behavior in a low alloy pipeline steel
    Li, Jing
    Gao, Xiuhua
    Du, Linxiu
    Liu, Zhenguang
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (12) : 1504 - 1512
  • [39] Effect of Ce content on the hydrogen induced cracking of X80 pipeline steel
    Cheng, Wensen
    Song, Bo
    Mao, Jinghong
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2023, 48 (40) : 15303 - 15316
  • [40] Role of crystallographic texture on the improvement of hydrogen-induced crack resistance in API 5L X70 pipeline steel
    Masoumi, Mohammad
    Silva, Cleiton Carvalho
    Beres, Miloslav
    Ladino, Duberney Hincapie
    Gomes de Abreu, Hamilton Ferreira
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (02) : 1318 - 1326