Role of cold rolled followed by annealing on improvement of hydrogen induced cracking resistance in pipeline steel

被引:31
|
作者
Mohtadi-Bonab, M. A. [1 ]
Eskandari, M. [2 ]
Szpunar, J. A. [3 ]
机构
[1] Univ Bonab, Dept Mech Engn, Velayat Highway, Bonab, Iran
[2] Shahid Chamran Univ Ahvaz, Fac Engn, Dept Mat Sci & Engn, Ahvaz, Iran
[3] Univ Saskatchewan, Dept Mech Engn, 57 Campus Dr, Saskatoon, SK S7N5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen induced cracking; Crystallographic texture; X-ray diffraction; Pole figure; Electron backscatter diffraction; STRESS-CORROSION CRACKING; CRYSTALLOGRAPHIC TEXTURE; MICROSTRUCTURE; SUSCEPTIBILITY; PERMEATION; INCLUSIONS; FRACTURE; GROWTH;
D O I
10.1016/j.engfailanal.2018.04.044
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, we investigated the effect of cold rolled followed by annealing on hydrogen induced cracking susceptibility in an API X60 pipeline steel. To this, we carried out cold rolling on X60 steel up to 20%, 50% and 90% in thickness reduction to change the microstructure and texture of steel. Then, we annealed all specimens at 850 degrees C for 90 s. We studied all tested specimens by electron backscatter and X-ray diffraction techniques. EBSD results showed that the grain refinement process was properly done via cold rolling and annealing treatments in tested specimens. However, the dislocation density was high for all tested steels. Moreover, electrochemical hydrogen charging experiment on tested steels proved that all specimens were still highly susceptible to hydrogen induced cracking. Therefore, we increased the annealing temperature and its duration of the 90% cold rolled specimen (the specimen with finest grains) up to 950 degrees C for 5 min. Interestingly, there was no HIC crack on this steel after hydrogen charging experiment. EBSD measurements on this steel showed strong textures of {100}//ND and {111}//ND. As a result, such strong textures, low Kernel Average Misorientation data, a high proportion of recovered grains and coincidence site lattice boundaries were recognized as the most important reasons for the highest HIC resistance in the mentioned steel.
引用
收藏
页码:172 / 181
页数:10
相关论文
共 50 条
  • [1] Role of Ca treatment in hydrogen induced cracking of hot rolled API pipeline steel in acid sour media
    Moon, Joonoh
    Kim, Seong-Ju
    Lee, Changhee
    METALS AND MATERIALS INTERNATIONAL, 2013, 19 (01) : 45 - 48
  • [2] Role of Ca treatment in hydrogen induced cracking of hot rolled API pipeline steel in acid sour media
    Joonoh Moon
    Seong-Ju Kim
    Changhee Lee
    Metals and Materials International, 2013, 19 : 45 - 48
  • [3] The role of structural defects in hydrogen induced cold cracking of steel weldments
    Pokhodnya, IK
    Shvachko, VI
    Stepanyuk, SM
    ECF 12: FRACTURE FROM DEFECTS, VOLS. I-III, 1998, : 1241 - 1246
  • [4] Hydrogen induced cracking susceptibility in different layers of a hot rolled X70 pipeline steel
    Mohtadi-Bonab, M. A.
    Szpunar, J. A.
    Razavi-Tousi, S. S.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (31) : 13831 - 13841
  • [5] Effect of arisen dislocation density and texture components during cold rolling and annealing treatments on hydrogen induced cracking susceptibility in pipeline steel
    M. A. Mohtadi-Bonab
    M. Eskandari
    J. A. Szpunar
    Journal of Materials Research, 2016, 31 : 3390 - 3400
  • [6] Effect of arisen dislocation density and texture components during cold rolling and annealing treatments on hydrogen induced cracking susceptibility in pipeline steel
    Mohtadi-Bonab, M. A.
    Eskandari, M.
    Szpunar, J. A.
    JOURNAL OF MATERIALS RESEARCH, 2016, 31 (21) : 3390 - 3400
  • [7] A Review on the Role of Crystallographic Texture in Hydrogen-Induced Cracking Susceptibility in Pipeline Steel
    Mohtadi-Bonab, M. A.
    Masoumi, Mohammad
    Entezari, Ehsan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [8] Resistance to Hydrogen Cracking of Rolled Structural Steel after Heat Processing
    Naumenko V.V.
    Muntin A.V.
    Baranova O.A.
    Smetanin K.S.
    Steel in Translation, 2021, 51 (03) : 211 - 216
  • [9] Hydrogen induced cracking of X80 pipeline steel
    Dong, Chao-fang
    Xiao, Kui
    Liu, Zhi-yong
    Yang, Wen-jing
    Li, Xiao-gang
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2010, 17 (05) : 579 - 586
  • [10] CRYSTALLOGRAPHIC TEXTURE CONTROL HELPS IMPROVE PIPELINE STEEL RESISTANCE TO HYDROGEN-INDUCED CRACKING
    Venegas, V.
    Herrera, O.
    Caleyo, F.
    Hallen, J. M.
    Baudin, T.
    PROCEEDINGS OF THE ASME INTERNATIONAL PIPELINE CONFERENCE 2010, VOL 2, 2010, : 555 - 561