Damage accumulation caused by cyclic indentation in zirconia ceramics

被引:8
|
作者
Matsuzawa, M [1 ]
Yajima, N [1 ]
Horibe, S [1 ]
机构
[1] Waseda Univ, Dept Mat Sci & Engn, Shinjyuku Ku, Tokyo 1698555, Japan
关键词
D O I
10.1023/A:1004759829255
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Indentation fatigue testing is carried out for four kinds of zirconia ceramics; 6Y-FSZ, 3Y-TZP, Mg-PSZ and Ce-TZP; which have different strengthening-toughening mechanisms one another. Each material shows different indentation fatigue behavior. Large sized surface chipping is produced easily in early cycles for non-toughened 6Y-FSZ, while 3Y-TZP toughened by anelasticity has high resistance against chipping. There is a possibility that anelastic characteristic works as resistance against indentation fatigue damage. Stress induced phase transformation also improves fatigue damage, but this effect depends on the extent of transformation and/or occurrence of microcracking. (C) 1999 Kluwer Academic Publishers.
引用
收藏
页码:5199 / 5204
页数:6
相关论文
共 50 条
  • [21] Indentation damage zone in calcium and lead titanate ceramics
    Calderon-Moreno, JM
    Guiu, F
    Meredith, M
    Reece, MJ
    Sohn, KS
    BRITISH CERAMIC TRANSACTIONS, 1999, 98 (06): : 296 - 298
  • [22] Subsurface indentation damage and mechanical characterization of α-sialon ceramics
    Xie, Z.-H., 1600, American Ceramic Society (87):
  • [23] Indentation damage zone in calcium and lead titanate ceramics
    Queen Mary and Westfield Coll, London, United Kingdom
    Br Ceram Trans, 6 (296-298):
  • [24] FATIGUE DAMAGE IN CERAMIC MATERIALS CAUSED BY REPEATED INDENTATION
    TAKAKURA, E
    HORIBE, S
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (22) : 6151 - 6158
  • [25] Micromechanical characterization of zirconia and silicon nitride ceramics using indentation and scratch methods
    Liu, Ming
    Chen, Shuai
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 19982 - 20010
  • [26] ELASTIC PLASTIC INDENTATION DAMAGE IN CERAMICS - THE LATERAL CRACK SYSTEM
    MARSHALL, DB
    LAWN, BR
    EVANS, AG
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1982, 65 (11) : 561 - 566
  • [27] Grain-size effect on cracking accumulation in yttria-doped zirconia ceramics during cyclic martensitic transformations
    Crystal, Isabel R.
    Schuh, Christopher A.
    ACTA MATERIALIA, 2021, 209
  • [28] Cavity damage accumulation in alumina doped with zirconia or magnesia
    Hiraga, K
    Nakano, K
    Suzuki, TS
    Sakka, Y
    TOWARDS INNOVATION IN SUPERPLASTICITY II, 1999, 304-3 : 431 - 436
  • [29] Anelastic behaviour of zirconia ceramics under monotonic and cyclic loadings
    Pan, LS
    Horibe, S
    ACTA MATERIALIA, 1997, 45 (02) : 463 - 469
  • [30] Research on the cyclic fatigue behavior of zirconia ceramics at the room temperature
    Li Chunguang
    Si Wenjie
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 : 344 - 347