Shear Bond Strength of Cement to Zirconia

被引:8
|
作者
Rosentritt, M. [1 ]
Behr, M. [1 ]
van der Zel, J. M. [2 ,3 ]
Feilzer, A. J. [2 ,3 ]
机构
[1] Univ Regensburg, Med Ctr, Dept Prosthet Dent, D-93042 Regensburg, Germany
[2] Univ Amsterdam, Acad Ctr Dent Amsterdam, Dept Dent Mat Sci, NL-1066 EA Amsterdam, Netherlands
[3] Vrije Univ Amsterdam, NL-1066 EA Amsterdam, Netherlands
关键词
Zirconia; bonding; self-adhesive; resin; OXIDE CERAMIC CROWNS; DENTAL CERAMICS; LUTING CEMENTS; RESIN; DURABILITY; RETENTION; ADHESION; SURFACES;
D O I
10.1163/156856109X432758
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
This study investigated the shear bond strength (SBS) of various cements to zirconia ceramic. CoCr-cylinders were bonded to zirconia plates (20 mm x 10 mm x 2 mm; n = 8 per group) using four self-adhesive resin cements (one capsule, three hand-mixed) and four resin cements, partly in combination with a tribochemical/ silane treatment. All cements were auto-polymerizing. The bonding areas were sandblasted using 110 mu m Al(2)O(3). The shear bond strength was determined after 24 h, 30 days, 90 days of water storage (37 degrees C) and after 12 000 thermal cycles. Statistical analysis was performed using one-way analysis of variance (ANOVA) and Bonferroni post hoc test (alpha = 0.05). After 24 h and after thermal cycling (TC) the lowest value of shear bond strength was found for the control Variolink without bonding pre-treatment (9.5 MPa/3.1 MPa) and the highest results were determined for Calibra with bonding pre-treatment (37.3 MPa/31.9 MPa). After 30 days and 90 days of storage in water the highest SBS values were found for RelyX (33.3 MPa/28.6 MPa), and again lowest values were determined for Variolink (8.8 MPa/9.1 MPa). After 90 days storage all samples of Maxcem failed. The groupwise comparison revealed significantly different SBS results between 90 days storage and the initial results after 24 h (p = 0.003). No significant differences were found between the other storage conditions (p > 0.057). The systems without bonding pre-treatment provided significantly lower SBS in comparison to the self-adhesive systems and the systems with bonding pre-treatment (p = 0.000). Within the limitations of this study, three of four self-adhesive bonding systems provided bond strengths to zirconia, comparable to systems with additional bonding pre-treatment. The durability of the bonding resin and zirconia can only be judged after long-term water storage. (C) Koninklijke Brill NV, Leiden, 2009
引用
收藏
页码:1125 / 1132
页数:8
相关论文
共 50 条
  • [41] Effectiveness of different surface cleaning methods on the shear bond strength of resin cement to contaminated zirconia: an in vitro study
    Tunc, Elif Pak
    Chebib, Najla
    Sen, Deniz
    Zandparsa, Roya
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2016, 30 (05) : 554 - 565
  • [42] Effects of Surface-Etching Systems on the Shear Bond Strength of Dual-Polymerized Resin Cement and Zirconia
    Kim, Sang-Hyun
    Oh, Kyung Chul
    Moon, Hong-Seok
    MATERIALS, 2024, 17 (13)
  • [43] Effect of different energy densities of CO2 laser on shear bond strength of resin cement to zirconia
    Ghoveizi R.
    Bayati E.
    Beyabanaki E.
    Hejazi S.
    Tavakolizadeh S.
    Lasers in Dental Science, 2023, 7 (2) : 61 - 66
  • [44] Shear Bond Strength of Resin Cement to Zirconia Ceramic After Aluminum Oxide Sandblasting and Various Laser Treatments
    Akin, Hakan
    Ozkurt, Zeynep
    Kirmali, Omer
    Kazazoglu, Ender
    Ozdemir, Ali Kemal
    PHOTOMEDICINE AND LASER SURGERY, 2011, 29 (12) : 797 - 802
  • [45] Effectiveness of different surface cleaning methods on the shear bond strength of resin cement to contaminated zirconia: An in vitro study
    Tunc, Elif Pak
    Chebib, Najla
    Sen, Deniz
    Zandparsa, Roya
    Journal of Adhesion Science and Technology, 2016, 30 (05): : 554 - 565
  • [46] Effect of different surface shapes formed by femtosecond laser on zirconia-resin cement shear bond strength
    Akpinar, Yusuf Ziya
    Yavuz, Tevfik
    Aslan, Muhammed Ali
    Kepceoglu, Abdullah
    Kilic, Hamdi Sukur
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2015, 29 (03) : 149 - 157
  • [47] Shear bond strength of composite cement to alumina-coated versus tribochemical silica-treated zirconia
    Thammajaruk, Putsadeeporn
    Blatz, Markus B.
    Buranadham, Supanee
    Guazzato, Massimiliano
    Wang, Yu
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 105 (105)
  • [48] Evaluation of shear bond strength between dual cure resin cement and zirconia ceramic after thermocycling treatment
    Lee, Jung-Jin
    Kang, Cheol-Kyun
    Oh, Ju-Won
    Seo, Jae-Min
    Park, Ju-Mi
    JOURNAL OF ADVANCED PROSTHODONTICS, 2015, 7 (01): : 1 - 7
  • [49] Effect of combining different 10-MDP-containing primers and cement systems on shear bond strength between resin cement and zirconia
    Wongkamhaeng, Kan
    Poomparnich, Kopchai
    Chitkraisorn, Top
    Boonpitak, Kwanwong
    Tosiriwatanapong, Terawat
    BMC ORAL HEALTH, 2025, 25 (01):
  • [50] Shear bond strength of indirect composite material to monolithic zirconia
    Sari, Fatih
    Secilmis, Asli
    Simsek, Irfan
    Ozsevik, Semih
    JOURNAL OF ADVANCED PROSTHODONTICS, 2016, 8 (04): : 267 - 274