Microstructure, Hardness, and Tensile Properties of Vacuum Carburizing Gear Steel

被引:11
|
作者
Chen, Wu [1 ,2 ]
He, Xiaofei [3 ]
Yu, Wenchao [3 ]
Wang, Maoqiu [3 ]
Yao, Kefu [1 ]
机构
[1] Tsinghua Univ, Sch Mat Sci & Engn, Beijing 100084, Peoples R China
[2] NCS Testing Technol Co Ltd, Beijing 100081, Peoples R China
[3] Cent Iron & Steel Res Inst, Inst Special Steel, Beijing 100081, Peoples R China
关键词
gear steel; vacuum carburizing; retained austenite; tensile test; fracture;
D O I
10.3390/met11020300
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We investigated the effects of the austenitizing temperature on the microstructure, hardness, and tensile properties of case-carburized steel after vacuum carburization at 930 degrees C and then re-austenitization at 820-900 degrees C followed by oil quenching and tempering. The results show that fractures occurred early with the increase in the austenitizing temperature, although all the carburized specimens showed a similar case hardness of 800 HV0.2 and case depth of 1.2 mm. The highest fracture stress of 1919 MPa was obtained for the experimental steel when the austenitizing temperature was 840 degrees C due to its fine microstructure and relatively high percentage of retained austenite transformed into martensite during the tensile tests. We also found that the stress-strain behavior of case-carburized specimens could be described by the area-weighted curves of the carburized case and the core in combination. The strain hardening exponent was about 0.4 and did not vary with the increase in the austenitizing temperature. We concluded that the optimum austenitizing temperature was around 840 degrees C for the experimental steel.
引用
收藏
页码:1 / 15
页数:15
相关论文
共 50 条
  • [41] The effect of hot rolling on hardness properties and microstructure of laterite steel
    Siahaan, E.
    Riza, A.
    TARUMANAGARA INTERNATIONAL CONFERENCE ON THE APPLICATIONS OF TECHNOLOGY AND ENGINEERING, 2019, 508
  • [42] NEW CARBURIZING STEEL WITH IMPROVED HOT HARDNESS AND TEMPER RESISTANCE
    KRIEBLE, RW
    PHILIP, TV
    CIM BULLETIN, 1977, 70 (784): : 148 - 148
  • [43] VACUUM CARBURIZING OF LOW-CARBON STEEL WITH METHANE
    TSUJI, S
    ISHIGAMI, I
    YAMANAKA, K
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1987, 28 (01): : 48 - 56
  • [44] Carburizing Behavior of AISI 4115 Steel According to the Flow Rates of Acetylene in Vacuum Carburizing
    Kwon, Gi-hoon
    Moon, Kyoungil
    Lee, Young-Kook
    Jung, Minsu
    KOREAN JOURNAL OF METALS AND MATERIALS, 2020, 58 (09): : 617 - 625
  • [45] SELECTION OF EQUIPMENT FOR VACUUM CARBURIZING OF CONSTRUCTIONAL STEEL PARTS
    USATYI, YP
    EMELINA, ZS
    ISTOMIN, NN
    METAL SCIENCE AND HEAT TREATMENT, 1982, 24 (1-2) : 40 - 44
  • [46] Effect of thermal aging on microstructure, hardness, tensile and impact properties of Alloy 617
    Singh, Aditya Narayan
    Moitra, A.
    Bhaskar, Pragna
    Sasikala, G.
    Dasgupta, Arup
    Bhaduri, A. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 710 : 47 - 56
  • [47] Effects of Be additions on microstructure, hardness and tensile properties of A380 aluminum alloy
    Rejaeian, Morteza
    Karamouz, Mostafa
    Emamy, Masoud
    Hajizamani, Mohsen
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (11) : 3539 - 3545
  • [48] Effect of Minor Carburizing on Microstructure and Mechanical Properties of M50 Bearing Steel
    Yu, Xingfu
    Shen, Xiangyang
    Wei, Yinghua
    Zhao, Wenzeng
    Li, Yanbin
    Xing, Fei
    Su, Yong
    STEEL RESEARCH INTERNATIONAL, 2022, 93 (08)
  • [49] Microstructure Characteristics and Wear Performance of a Carburizing Bainitic Ferrite plus Martensite Si/Al-Rich Gear Steel
    Wang, Yanhui
    He, Qingsong
    Yang, Qian
    Xu, Dong
    Yang, Zhinan
    Zhang, Fucheng
    METALS, 2022, 12 (05)
  • [50] THE EFFECT OF THE QUENCHING METHOD ON THE DEFORMATIONS SIZE OF GEAR WHEELS AFTER VACUUM CARBURIZING
    Dybowski, K.
    Sawicki, J.
    Kula, P.
    Januszewicz, B.
    Atraszkiewicz, R.
    Lipa, S.
    ARCHIVES OF METALLURGY AND MATERIALS, 2016, 61 (02) : 1057 - 1062