Interfacial Reaction and Microstructure Evolution of Sn-9Zn/Ni(Cu) Solder Joints

被引:2
|
作者
Zhu, Xuewei [1 ]
Peng, Jian [2 ]
Wei, Xiaofeng [1 ]
Yan, Pengpeng [1 ]
Wang, Fu [1 ]
机构
[1] Northwest A&F Univ, Coll Mech & Elect Engn, Yangling 712100, Shaanxi, Peoples R China
[2] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
关键词
interfacial reaction; intermetallic compound; Sn-9Zn solder; Ni(Cu) substrates; PHASE-EQUILIBRIA; INTERMETALLIC COMPOUNDS; NI; CU; ALLOY;
D O I
10.3390/met9050604
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Sn-9Zn solder is a promising Pb-free solder, but it tends to form bulky intermetallic compounds (IMC) grains at the interface when soldered with common simple metal Cu or Ni substrates. Interfacial reaction between Sn-9Zn solder and Ni(Cu) solid solution substrates at 250 degrees C and 350 degrees C were systematically probed in this study. Results showed that when soldered at 250 degrees C, a Ni5Zn21 layer is formed at Sn-Zn/Ni-20Cu and Sn-Zn/Ni-40Cu joints; and Ni2Sn2Zn + Cu5Zn8 and Cu5Zn8 phases are formed in Sn-Zn/Ni-60Cu and Sn-Zn/Ni-80Cu joints, respectively. Fine-grained IMCs formed at the interface are formed even when the soldered time is prolonged to 16 h. This result indicates that Ni(Cu) solid solution substrates inhibit the rapid growth of IMC at the Sn-Zn/Ni-Cu interface. Ni(Cu) solid solution substrate can also provide various combinations of reaction products at the Sn-Zn/Ni-Cu joints. The Ni5Zn21 transfers to Ni2Sn2Zn + Cu5Zn8 phases when the Cu content increased to 60%, and a bi-layered structure Ni2Sn2Zn + Cu5Zn8 IMCs was formed in Sn-Zn/Ni(Cu) joints at 350 degrees C regardless of the Cu content in Ni(Cu) substrate (20-80%). These results would provide an effective support in designing Sn-Zn soldering system with optimized IMC layer to improve mechanical performance.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Influence of Zn additions on the interfacial reaction and microstructure of Sn37Pb/Cu solder joints
    Yu Qiu
    Xiaowu Hu
    Yulong Li
    Xiongxin Jiang
    Applied Physics A, 2017, 123
  • [22] Influence of Zn additions on the interfacial reaction and microstructure of Sn37Pb/Cu solder joints
    Qiu, Yu
    Hu, Xiaowu
    Li, Yulong
    Jiang, Xiongxin
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2017, 123 (10):
  • [23] Effects of Ce and La Additions on the Microstructure and Mechanical Properties of Sn-9Zn Solder Joints
    Hsiu-Jen Lin
    Tung-Han Chuang
    Journal of Electronic Materials, 2010, 39 : 200 - 208
  • [24] Influence of rapid solidification on microstructure, thermodynamic characteristic and the mechanical properties of solder/Cu joints of Sn-9Zn alloy
    Jing, Yanxia
    Sheng, Guangmin
    Zhao, Guoji
    MATERIALS & DESIGN, 2013, 52 : 92 - 97
  • [25] Effect of the Soldering Process on the Microstructure and Mechanical Properties of Sn-9Zn/Al Solder Joints
    Yao Yao
    Xue Feng
    Zhou Jian
    Feng Zhanying
    Chen Xu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (08) : 2908 - 2916
  • [26] Effect of the Soldering Process on the Microstructure and Mechanical Properties of Sn-9Zn/Al Solder Joints
    Yao Yao
    Xue Feng
    Zhou Jian
    Feng Zhanying
    Chen Xu
    Journal of Materials Engineering and Performance, 2015, 24 : 2908 - 2916
  • [27] Effect of Cu addition on interfacial reactions between Sn-9Zn lead-free solder and Ni substrate
    Yen, Yee-wen
    Liou, Wei-kai
    JOURNAL OF MATERIALS RESEARCH, 2007, 22 (10) : 2663 - 2667
  • [28] Effects of Ce and La Additions on the Microstructure and Mechanical Properties of Sn-9Zn Solder Joints
    Lin, Hsiu-Jen
    Chuang, Tung-Han
    JOURNAL OF ELECTRONIC MATERIALS, 2010, 39 (02) : 200 - 208
  • [29] Effect of Cu addition on interfacial reactions between Sn-9Zn lead-free solder and Ni substrate
    Yee-wen Yen
    Wei-kai Liou
    Journal of Materials Research, 2007, 22 : 2663 - 2667
  • [30] Interfacial growth behavior of Sn-9Zn/additive Cu-particles and Sn-9Zn/Cu-substrate
    College of Mechanical Engineering, South China University of Technology, Guangzhou 510641, China
    不详
    Zhongguo Youse Jinshu Xuebao, 2007, 7 (1083-1089):