摘要
Tritium breeding ceramic materials are placed at high temperatures for a long period in a fusion DEMO reactor. Therefore, the understanding of Li mass loss phenomena and its influence on tritium behavior are important. In this study, the pebbles of Li2TiO3 with excess Li were heated at 900 degrees C for 30 days in a 1000 Pa H-2/Ar flow and tritium sorption and recovery experiments were carried out. Li mass loss by the heating was evaluated to be 0.7 wt%. The value of Li mass loss was almost same as that for 3 days heating at the same condition. Tritium sorption capacity for the heated pebbles at 600 degrees C and 900 degrees C were almost same as that for the pebbles as received. Tritium sorbed in the pebbles could not be recovered effectively by the 1000 Pa H-2/Ar purge at room temperature and 300 degrees C but it could be recovered at 600 degrees C and 900 degrees C. The influence of the long-time heating on the behavior of tritium sorbed in the pebbles was not large.
引用
收藏
页数:6
相关论文
共 50 条
  • [41] Effect of surface water on tritium release behavior from Li2TiO3
    Hanada, T.
    Nishikawa, M.
    Kanazawa, T.
    Yamasaki, H.
    Yamashita, N.
    Fukada, S.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 735 - 738
  • [42] First results of the investigation of Li2ZrO3 and Li2TiO3 pebbles
    Lulewicz, JD
    Roux, N
    FUSION ENGINEERING AND DESIGN, 1998, 39-40 : 745 - 750
  • [43] Effects of pre-treatments of Li2TiO3 pebbles on the release of tritium generated during short irradiations
    Alvani, C
    Carconi, PL
    Casadio, S
    Roux, N
    FUSION ENGINEERING AND DESIGN, 2001, 58-59 : 701 - 705
  • [44] Kinetics of tritium release from irradiated Li2TiO3 pebbles in out-of-pile TPD tests
    Alvani, C
    Casadio, S
    Casadio, S
    FUSION ENGINEERING AND DESIGN, 2003, 69 (1-4) : 275 - 280
  • [45] Enhancing the density and crush load of Li2TiO3 tritium breeding ceramic pebbles by adding LiNO3-Li2CO3
    Gong, Yichao
    Na, Qingze
    Dang, Chao
    Yang, Yijiang
    Tang, Mingxiang
    Liu, Zhanwen
    Zhang, Guojun
    ANNALS OF NUCLEAR ENERGY, 2024, 196
  • [46] A novel preparation of porous Li2TiO3 pebbles with a distinctive structure
    Gong, Yichao
    Li, Zhaokun
    Li, Junjie
    Qi, Jianqi
    Zhuo, Longchao
    Zhang, Guojun
    Lu, Tiecheng
    JOURNAL OF NUCLEAR MATERIALS, 2025, 603
  • [47] Fabrication tests of Li2TiO3 pebbles by direct wet process
    Tsuchiya, K
    Uchida, M
    Kawamura, H
    Casadio, S
    Alvani, C
    CBBI-10: PROCEEDINGS OF THE 10TH INTERNATIONAL WORKSHOP ON CERAMIC BREEDER BLANKET INTERACTIONS, 2002, 6720 : 93 - 100
  • [48] Evaluation of contact strength of Li2TiO3 pebbles with different diameters
    Tsuchiya, K
    Kawamura, H
    Tanaka, S
    FUSION ENGINEERING AND DESIGN, 2006, 81 (8-14) : 1065 - 1069
  • [49] Helium as a temperature moderator in batch irradiation of Li2TiO3 pebbles
    Avila, RE
    Peña, LA
    Padilla-Campos, L
    Jiménez, JC
    CBBI-10: PROCEEDINGS OF THE 10TH INTERNATIONAL WORKSHOP ON CERAMIC BREEDER BLANKET INTERACTIONS, 2002, 6720 : 79 - 84
  • [50] Fabrication of Li2TiO3 pebbles by a selective laser sintering process
    Zhou, Qilai
    Gao, Yue
    Liu, Kai
    Xue, Lihong
    Yan, Youwei
    FUSION ENGINEERING AND DESIGN, 2015, 100 : 166 - 170