Effect of Fe and Mn additions on microstructure and wear properties of spray-deposited Al-20Si alloy

被引:33
|
作者
Wang, F
Zhang, ZY
Ma, YJ
Jin, YS
机构
关键词
microstructure; dry sliding wear behavior; spray deposition; wear mechanism;
D O I
10.1016/j.matlet.2004.02.027
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the hypereutectic AI-Si alloys were synthesized by spray atomization and deposition technique. The microstructures of spray-deposited alloys were studied using scanning electron microscopy (SEM) and X-ray diffraction (XRD). The dry sliding wear behavior of the alloys was investigated under the applied load of 8.9-35.6 N. The wear behavior of the alloys was dependent on the morphology of the intermetallics in microstructure and applied load. At lower load (8.9 and 17.8N), the Fe-containing alloy showed higher wear rate compared with the binary alloy due to the tendency for embrittlement brought about by needle-like intermetallics. At higher load (35.6 N), Fe- and Mn-containing alloy exhibited inferior wear resistance than the binary alloy due to the fragmentation of the intermetallics, thus leading to easier crack nucleation and propagation. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:2442 / 2446
页数:5
相关论文
共 50 条
  • [31] Microstructure and mechanical properties of spray deposited Al-Si-Fe-Cu-Mg alloy
    Harbin Institute of Technology, Harbin 150001, China
    不详
    Jinshu Xuebao, 3 (252):
  • [32] THE EFFECT OF FE ADDITIONS ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A Ti-Al-Mn ALLOY
    Bettles, C. J.
    Puehringer, T.
    Morton, A. J.
    Tomus, D.
    Gibson, M. A.
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2009, 23 (6-7): : 783 - 789
  • [33] Effect of spraying rate on microstructure of spray deposited Al-Fe-V-Si alloy
    Kalkanli, A
    Oren, EE
    POWDER METALLURGY, 2003, 46 (04) : 324 - 328
  • [34] Effect of HCPEB treatment on microstructure and microhardness of hypereutectic Al-20Si alloy
    Hao, Yi
    Gao, Bo
    Tu, Gan-Feng
    Shi, Wei-Xi
    Li, Shi-Wei
    Hao, Sheng-Zhi
    Dong, Chuang
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (09): : 142 - 145
  • [35] Effects of melt superheat treatment on microstructure and wear behaviours of hypereutectic Al-20Si alloy
    Li, Q. L.
    Xia, T. D.
    Lan, Y. F.
    Li, P. F.
    MATERIALS SCIENCE AND TECHNOLOGY, 2014, 30 (07) : 835 - 841
  • [36] Microstructure and mechanical properties of spray-deposited Al-17Si-4.5Cu-0.6Mg wrought alloy
    Wu, Yue
    Cassada, William A.
    Lavernia, Enrique J.
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1995, 26 A (05): : 1235 - 1247
  • [37] Microstructure of rapidly solidified Al-20Si alloy powders
    Kim, TS
    Lee, BT
    Lee, CR
    Chun, BS
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 304 (1-2): : 617 - 620
  • [38] Microstructure and phase formation in spray-deposited Al-18%Si-5%Fe-1.5%Cu alloy
    Srivastava, VC
    Ghosal, P
    Ojha, SN
    MATERIALS LETTERS, 2002, 56 (05) : 797 - 801
  • [39] Effect of Cu Additions on the Microstructure and Mechanical Properties of Spray Deposited Zn-30Al Alloy
    Liu, Hong-Wei
    Wang, Feng
    Huang, Shu-Hui
    Yan, Hong-Wei
    Li, Xi-Wu
    Li, Zhi-Hui
    Zhang, Yong-An
    Xiong, Bai-Qing
    PROCEEDINGS OF THE 2ND ANNUAL INTERNATIONAL CONFERENCE ON ADVANCED MATERIAL ENGINEERING (AME 2016), 2016, 85 : 361 - 365
  • [40] The Effect of Heat Aging on the Microstructure and Properties of Spray-Deposited AlZnMgCu Alloy Extruded Plates
    Chen, Chen
    Feng, Di
    He, Zhiping
    Zhu, Yichao
    Tao, Zhiyuan
    Xu, Yinhui
    Wang, Haoran
    Wang, Jingtao
    Liu, Ying
    MATERIALS, 2024, 17 (15)