Effects of rapid quenching on structure and electrochemical characteristics of La0.5Ce0.2Mg0.3Co0.4Ni2.6-xMnx (x=0-0.4) electrode alloys

被引:9
|
作者
Zhang Yang-huan [1 ,2 ]
Zhao Dong-liang [1 ]
Dong Xiao-ping [1 ,3 ]
Qi Yan [1 ]
Guo Shi-hai [1 ]
Wang Xin-lin [1 ]
机构
[1] Cent Iron & Steel Res Inst, Dept Funct Mat Res, Beijing 100081, Peoples R China
[2] Inner Mongolia Univ Sci & Technol, Sch Mat, Baotou 014010, Peoples R China
[3] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
La-Mg-Ni system electrode alloy; rapid quenching; structure; electrochemical performance; HYDROGEN STORAGE ALLOYS; MICROSTRUCTURE; SUBSTITUTION; CAPACITY; COBALT; PHASE; LA; CO;
D O I
10.1016/S1003-6326(08)60279-4
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The La-Mg-Ni system PuNi3-type La0.5Ce0.2Mg0.3CO0.4Ni2.6-xMnx (x=0, 0.1, 0.2, 0.3, 0.4) hydrogen storage alloys were prepared by casting and rapid quenching. The effects of the rapid quenching on the structure and electrochemical characteristics of the alloys were studied. The results obtained by XRD, SEM and TEM indicate that the as-cast and quenched alloys mainly consist of two major phases, (La,Mg)Ni-3 and LaNi5, as well as a residual phase LaNi. The rapid quenching does not exert an obvious influence on the phase composition of the alloys, but it leads to an increase of the LaNi5 phase and a decrease of the (La, Mg)Ni-3 phase. The as-quenched alloys have a nano-crystal line structure, and the grain sizes of the alloys are in the range of 20-30 nm. The results by the electrochemical measurements indicate that both the discharge capacity and the high rate discharge(HRD) ability of the alloy first increase and then decrease with the variety of quenching rate and obtain the maximum values at the special quenching rate which is changeable with the variety of Mn content. The rapid quenching significantly improves the cycle stabilities of the alloys, but it slightly impairs the activation capabilities of the alloys.
引用
收藏
页码:364 / 371
页数:8
相关论文
共 50 条
  • [21] Effects of rapid quenching on the microstructures and electrochemical performances of La0.7Mg0.3Ni2.55-xCo0.45Alx (x=0∼0.4) alloys for electrodes
    Zhang Yanghuan
    Ren Huiping
    Wu Zhongwang
    Dong Xiaoping
    Guo Shihai
    Wang Xinlin
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (08) : 1431 - 1435
  • [22] Microstructure and electrochemical performances of La0.7Mg0.3Ni2.55-xCo 0.45Cux (x = 0-0.4) hydrogen storage alloys prepared by casting and rapid quenching
    Zhang, Yang-Huan
    Dong, Xiao-Ping
    Wang, Guo-Qing
    Guo, Shi-Hai
    Ren, Jiang-Yuan
    Wang, Xin-Lin
    Journal of Alloys and Compounds, 2006, 417 (1-2): : 224 - 229
  • [23] Effects of substituting Ni with Cu on the microstructures and electrochemical characteristics of the as-cast and quenchedLa0.7Mg0.3Ni2.55-xCo0.45Cux(x=0-0.4)electrode alloys
    Zhang, Yang-huan
    Li, Bao-wei
    Ren, Hui-ping
    Cai, Ying
    Dong, Xiao-ping
    Wang, Xin-lin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (15) : 3420 - 3426
  • [24] Influences of the substitution of Fe for Ni on structures and electrochemical performances of the as-cast and quenched La0.7Mg0.3Co0.45Ni2.55-xFex (x = 0-0.4) electrode alloys
    Zhang, Yang-Huan
    Li, Bao-Wei
    Ren, Hui-Ping
    Wu, Zhong-Wang
    Dong, Xiao-Ping
    Wang, Xin-Lin
    Journal of Alloys and Compounds, 2008, 460 (1-2): : 414 - 420
  • [25] Influences of the substitution of Fe for Ni on structures and electrochemical performances of the as-cast and quenched La0.7Mg0.3Co0.45Ni2.55-xFex (x=0-0.4) electrode alloys
    Zhang, Yang-Huan
    Li, Bao-Wei
    Ren, Hui-Ping
    Wu, Zhong-Wang
    Dong, Xiao-Ping
    Wang, Xin-Lin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 460 (1-2) : 414 - 420
  • [26] An electrochemical study of La0.4Ce0.3Mg0.3Ni2.975-xMnxCO0.525 (x=0.1-0.4) hydrogen storage alloys
    Pan, HG
    Jin, QW
    Gao, MX
    Liu, YF
    Li, R
    Lei, YQ
    Wang, QD
    JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 376 (1-2) : 196 - 204
  • [27] Structure and electrochemical hydrogen storage characteristics of the as-cast and annealed La0.8-xSmxMg0.2Ni3.15Co0.2Al0.1Si0.05 (x=0-0.4) alloys
    Li Ping
    Hou Zhonghui
    Yang Tai
    Shang Hongwei
    Qu Xuanhui
    Zhang Yanghuan
    JOURNAL OF RARE EARTHS, 2012, 30 (07) : 696 - 704
  • [28] Microstructure and electrochemical characteristics of Mm(Ni,Co,Mn,Al)5Bx (x=0-0.4) hydrogen storage alloys prepared by cast and rapid quenching
    Zhang, YH
    Chen, MY
    Wang, XL
    Wang, GQ
    Dong, XP
    Qi, Y
    ELECTROCHIMICA ACTA, 2004, 49 (07) : 1161 - 1168
  • [29] Structure and electrochemical hydrogen storage characteristics of the as-cast and annealed La0.8-xSmxMg0.2Ni3.15Co0.2Al0.1Si0.05 (x=0-0.4) alloys
    李平
    候忠辉
    杨泰
    尚宏伟
    曲选辉
    张羊换
    JournalofRareEarths, 2012, 30 (07) : 696 - 704
  • [30] Effects of the substitution of Al for Ni on the structure and electrochemical performance of La0.7Mg0.3Ni2.55 − xCo0.45Alx (x = 0–0.4) electrode alloys
    Yanghuan Zhang
    Dongliang Zhao
    Baowei Li
    Huiping Ren
    Shihai Guo
    Xinlin Wang
    Journal of Materials Science, 2007, 42 : 8172 - 8177