Laser micromachining of Al2O3-TiC ceramics

被引:25
|
作者
Oliveira, V
Vilar, R
Conde, O
Freitas, P
机构
[1] UNIV LISBON, DEPT PHYS, P-1700 LISBON, PORTUGAL
[2] INST SUPER TECN, DEPT PHYS, P-1096 LISBON, PORTUGAL
关键词
D O I
10.1557/JMR.1997.0418
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al2O3-34 wt.% TiC ceramics have been machined with a KrF (248 nm) excimer laser under normal atmosphere, In the initial steps of the irradiation process both the roughness and the removal rate present a strong variation with the number of pulses. After approximately 200 pulses the process reaches a stationary regime where the roughness and the removal rate become constant, Characterization of the machined areas by scanning electron microscopy showed that the variations in roughness and removal rate are related to the evolution of the surface topography of the samples, Also, as a consequence of laser irradiation, TiC and Al2O3 are partially transformed into TiO2 TiC0.7N0.3, and an Al-Ti solid solution.
引用
收藏
页码:3206 / 3209
页数:4
相关论文
共 50 条
  • [21] Excimer laser ablation of Al2O3-TiC ceramics:: laser induced modifications of surface topography and structure
    Oliveira, V
    Vilar, R
    Conde, O
    APPLIED SURFACE SCIENCE, 1998, 127 : 831 - 836
  • [22] STRENGTH OF AL2O3 AND AL2O3-TIC CERAMICS IN RELATION TO THEIR FRACTURE SOURCES
    WATANABE, M
    FUKUURA, I
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 394 - 394
  • [23] Characterization of columns grown during KrF laser micromachining of Al2O3–TiC ceramics
    V. Oliveira
    R. Vilar
    Journal of Materials Research, 2003, 18 : 1123 - 1130
  • [24] The Effect of TiC Content and Sintering Temperature on Mechanical Property of Al2O3-TiC Composite Ceramics
    柳军旺
    郭英奎
    石春艳
    哈尔滨理工大学学报, 2008, (06) : 114 - 116
  • [25] Effect of grain size on thermal shock resistance of Al2O3-TiC ceramics
    You, XQ
    Si, TZ
    Liu, N
    Ren, PP
    Xu, YD
    Feng, JP
    CERAMICS INTERNATIONAL, 2005, 31 (01) : 33 - 38
  • [26] Mechanism of structure formation and the presence of defects in ceramics of the Al2O3-TiC system
    Pilyankevich, A.N.
    Melnikova, V.A.
    Kulik, A.I.
    Soviet journal of superhard materials, 1988, 10 (05): : 22 - 27
  • [27] Column-growth mechanisms during KrF laser micromachining of Al2O3–TiC ceramics
    V. Oliveira
    F. Simões
    R. Vilar
    Applied Physics A, 2005, 81 : 1157 - 1162
  • [28] Synthesis of Al2O3-TiC by reactive milling
    Pallone, EMJA
    Tomasi, R
    Botta, WJ
    METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, PTS 1 AND 2, 2000, 343-3 : 393 - 398
  • [29] Influence of the processing parameters on the formation and deposition of particles in UV pulsed laser ablation of Al2O3-TiC ceramics
    Mendes, M
    Vilar, R
    APPLIED SURFACE SCIENCE, 2003, 217 (1-4) : 149 - 162
  • [30] Mechanochemically synthesized Al2O3-TiC nanocomposite
    Sharifi, E. Mohammad
    Karimzadeh, F.
    Enayati, M. H.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 491 (1-2) : 411 - 415