Joining of silicon nitride ceramic composites with Y2O3-Al2O3-SiO2 mixtures

被引:0
|
作者
Fei, Z [1 ]
机构
[1] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Peoples R China
关键词
silicon nitride; bonding; Y2O3-Al2O3-SiO2; joint strength; interface reaction;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot-pressure sintered silicon nitride ceramic composites were joined to themselves using Y2O3-Al2O3-SiO2 mixtures. Reaction behavior at interface between Si3N4 and Y2O3-Al2O3-SiO2 mixtures during silicon nitride composite joining was studied by means of SEM, EPMA and XRD. The joint strength under different bonding conditions was measured by four-point bending tests. The results of EPMA and XRD analyses show that the liquid glass solders react with silicon nitride at interface, forming the Si3N4/Si2N2O/Y-Si-Al-O-N glass/Y-Si-Al-O glass gradient interface. From the results of four-point bending tests, it is known that with increasing joining temperature and holding time, the joint strength first increased, reaching a peak, and then decreased. The maximum joining strength of 315 MPa measured by the four-point bending test is achieved for the Si3N4 composite-Si3N4 composite joint bonded at 1823 K for 15 min. Destructed part is considered to start at the diffusion layer, indicating that the joining strength will be much higher than that value. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:293 / 297
页数:5
相关论文
共 50 条
  • [21] Thermodynamic reassessment of the Y2O3-Al2O3-SiO2 system and its subsystems
    Mao, Huahai
    Selleby, Malin
    Fabrichnaya, Olga
    CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2008, 32 (02): : 399 - 412
  • [22] Phase equilibria and crystal chemistry in the Y2O3-Al2O3-SiO2 system
    Max-Planck-Inst. fur Metallforschung, Universität Stuttgart, Pulvermetallurgisches Laboratorium, Heisenbergstr. 5, D-70569 Stuttgart, Germany
    J Mater Res, 2 (447-455):
  • [23] Preparation of glass-ceramic composites containing Ce:YAG microcrystals from Y2O3-Al2O3-SiO2 ternary system
    Asahi, Taro
    Miyata, Tsuyoshi
    Nakayama, Susumu
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2015, 123 (1439) : S1 - S4
  • [24] Viscosity of nitrogen containing Y2O3-Al2O3-SiO2 melts and hardness of glasses
    Saito, N
    Kai, K
    Furusho, S
    Shimizu, F
    Nakashima, K
    Mori, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (01) : 40 - 46
  • [25] Interfacial reaction and joint strength of silicon nitride ceramic composites bonded with Y2O3-Al2O3-SiO2-Si3N4 mixture
    Zhou, F
    Suh, CM
    Kim, SS
    MATERIALS LETTERS, 2002, 55 (1-2) : 55 - 60
  • [26] SI3N4 WETTABILITY BY Y2O3-AL2O3-SIO2 LIQUIDS
    GILBERT, DW
    MILLER, AD
    AMERICAN CERAMIC SOCIETY BULLETIN, 1983, 62 (08): : 869 - 869
  • [27] Liquid-phase bonding of silicon nitride ceramics using Y2O3-Al2O3-SiO2-TiO2 mixtures
    Zhou, F
    Pan, JY
    Chen, KM
    MATERIALS LETTERS, 2004, 58 (7-8) : 1383 - 1386
  • [28] Bonding of silicon nitride ceramic composite with RE2O3-Al2O3-SiO2 glass solders
    Jiangsu Univ of Science and, Technology, Zhenjiang, China
    J Rare Earth, 3 (194-199):
  • [29] Bonding of silicon nitride ceramic composite with RE2O3-Al2O3-SiO2 glass solders
    Zhou, F
    Li, ZZ
    Luo, QF
    JOURNAL OF RARE EARTHS, 1999, 17 (03) : 194 - 199
  • [30] Preparation of P+-implanted Y2O3-Al2O3-SiO2 glass for radiotherapy of cancer
    Kawashita, M
    Miyaji, F
    Kokubo, T
    Takaoka, GH
    Yamada, I
    Suzuki, Y
    Inoue, M
    BIOCERAMICS, VOL 10, 1997, : 531 - 534