We report on our preliminary work on shock consolidation of pre-alloyed Ti3SiC2 powder as well as reaction synthesis of shock-densified powder precursors to form the titanium-silicon ternary carbide phase. The shock-compression experiments were performed using an 80-mm diameter single-stage gas gun at velocities of 500-900 mis, with the compaction pressures calculated using AUTODYN-2D numerical simulation. The consolidated pre-alloyed Ti3SiC2 samples revealed retention of the ternary phase with a microstructure showing extensive plastic strain, corresponding to a dislocation density of cold-rolled metals. Samples of the shock-densified Ti, SIG, and graphite powder precursors showed formation of the Ti3SiC2 phase under conditions of defect-enhanced solid-state diffusion upon heating at 1600 degrees C for 4 hours. The Ti3SiC2 phase appears to have been formed from a solid solution of TiC + Si. In this paper we will describe the experimental approach, microstructural characteristics, and deformation behavior of shock-consolidated as well as reaction synthesized Ti3SiC2 ternary carbide.
引用
收藏
页码:101 / 111
页数:11
相关论文
共 50 条
  • [21] Modelling the chemical transformations in system of titanium-silicon during shock-wave loading
    Zelepugin, S.A.
    Nikulichev, V.B.
    Ivanova, O.V.
    Zelepugin, A.S.
    Khimicheskaya Fizika, 2005, 24 (10): : 76 - 83
  • [22] Modeling the shock response of silicon carbide, boron carbide and titanium diboride
    Rajendran, AM
    Grove, DJ
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 1996, 18 (06) : 611 - 631
  • [23] Structural characterisation of titanium silicon carbide reaction
    Makhtari, A
    La Via, F
    Raineri, V
    Calcagno, L
    Frisina, F
    MICROELECTRONIC ENGINEERING, 2001, 55 (1-4) : 375 - 381
  • [24] Effect on addition of titanium diboride to titanium carbide produced by the SHS shock consolidation method
    Tomoshige, R
    Kakoki, Y
    Imamura, K
    Chiba, A
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1999, 85 (1-3) : 105 - 108
  • [25] Structure and mechanical properties of porous titanium-silicon carbide Tl3SiC2
    Brodnikovskij, N.P.
    Burka, M.P.
    Verbilo, D.G.
    Demydyk, A.Y.
    Ivanova, I.I.
    Koval, A.Yu.
    Pechkovskij, E.P.
    Polushko, G.P.
    Firstov, S.A.
    Poroshkovaya Metallurgiya, 2003, (7-8): : 109 - 120
  • [26] Creep of titanium-silicon carbide Ti3SiC in conditions of microindentation at a room temperature
    Gorban, VF
    Pechkovs'ky, EP
    Samelyuk, AV
    Firstov, SO
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2005, 27 (03): : 331 - 348
  • [28] HEATCONTENT AND HEAT CAPACITIES IN THE SYSTEM TITANIUM-SILICON
    GOLUTVIN, YM
    ZHURNAL FIZICHESKOI KHIMII, 1959, 33 (08): : 1798 - 1805
  • [29] SOME PRINCIPLES OF COMBUSTION OF TITANIUM-SILICON MIXTURES
    AZATYAN, TS
    MALTSEV, VM
    MERZHANOV, AG
    SELEZNEV, VA
    COMBUSTION EXPLOSION AND SHOCK WAVES, 1979, 15 (01) : 35 - 40
  • [30] Chlorination of Carburized Titanium-Silicon Concentrate.
    Levin, M.I.
    Masterova, A.P.
    Avdzhiev, G.R.
    Gens, M.A.
    Tsvetnye Metally, 1980, (09): : 63 - 66