Methodology for measuring fracture toughness of ceramic materials by instrumented indentation test with vickers indenter

被引:17
|
作者
Ma, Dejun [1 ]
Wang, Jialiang [2 ]
Sun, Liang [1 ]
机构
[1] Acad Armored Forces Engn, Dept Mech Engn, Beijing, Peoples R China
[2] Engn Univ Chinese Armed Police Force, Coll Equipment Engn, Xian, Peoples R China
关键词
ceramic material; fracture toughness; instrumented indentation; vickers impression; BRITTLE MATERIALS; PALMQVIST CRACK; RADIAL CRACK;
D O I
10.1111/jace.14650
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Virtual crack closure technique and elastoplastic finite element method were employed to calculate the stress intensity factors (SIF) of ceramic materials on the tip of both half-penny crack (HPC) and radial crack (RC) induced by Vickers indenter and the value of fracture toughness (K-IC) was extracted by the design of equi-SIF contour of HPC and RC crack front. Through dimensional theorem and regressive analysis, a functional relationship between instrumented indentation parameters, crack length of Vickers impression and fracture toughness of ceramic materials was established, thus a novel methodology has been presented for measuring fracture toughness of ceramic materials by instrumented Vickers indentation. Both numerical analysis and experiments have indicated that this methodology enjoys higher measurement precision compared with other available indentation methods. The methodology is universally suitable for HPC, RC as well as transition cracks and capable of determining fracture toughness and elastic modulus in a single indentation test. In addition, it saves the effort of measuring the diagonal length of Vickers impression in case that the impression remains unclear.
引用
收藏
页码:2296 / 2308
页数:13
相关论文
共 50 条
  • [41] Estimation of Fracture Toughness for ε Zirconium Hydride by Vickers Microhardness Indentation Method
    Changxing Cui
    Feng Wang
    Zhongwu Hu
    Yanchao Li
    Benqi Jiao
    Jianrong Xue
    Mingming Wu
    Lian Zhou
    Wen Zhang
    JOM, 2021, 73 : 3468 - 3475
  • [42] Measurement of fracture toughness in AISI 1018 borided steels by vickers indentation
    Instituto Politécnico Nacional, SEPI-ESIME U.P. Adolfo López Mateos, Zacatenco. México D.F. 07738, Mexico
    不详
    Diffus Defect Data Pt A Diffus Forum, 2008, (675-680): : 675 - 680
  • [43] Estimation of Fracture Toughness for ε Zirconium Hydride by Vickers Microhardness Indentation Method
    Cui, Changxing
    Wang, Feng
    Hu, Zhongwu
    Li, Yanchao
    Jiao, Benqi
    Xue, Jianrong
    Wu, Mingming
    Zhou, Lian
    Zhang, Wen
    JOM, 2021, 73 (11) : 3468 - 3475
  • [44] Measurement of Fracture Toughness in AISI 1018 Borided Steels by Vickers Indentation
    Campos-Silva, I.
    Lopez-Perrusquia, N.
    Ortiz-Dominguez, M.
    Figueroa-Lopez, U.
    Hernandez-Sanchez, E.
    DIFFUSION IN SOLIDS AND LIQUIDS IV, 2009, 283-286 : 675 - +
  • [45] Determination of Vickers indentation fracture toughness of boronised alloyed ductile iron
    Toktas, A.
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2019, 97 (05): : 271 - 276
  • [46] Fracture Toughness of HVOF Sprayed Cermet Coatings Measured by Vickers Indentation
    Houdkova, Sarka
    Zahalka, Frantisek
    Kasparova, Michaele
    MATERIALS STRUCTURE & MICROMECHANICS OF FRACTURE, 2011, 465 : 475 - 478
  • [47] DEPENDENCE OF THE VICKERS INDENTATION FRACTURE-TOUGHNESS ON THE SURFACE CRACK LENGTH
    PONTON, CB
    RAWLINGS, RD
    BRITISH CERAMIC TRANSACTIONS AND JOURNAL, 1989, 88 (03): : 83 - 90
  • [48] COMPARATIVE MEASUREMENT OF INDENTATION FRACTURE-TOUGHNESS WITH BERKOVICH AND VICKERS INDENTERS
    DUKINO, RD
    SWAIN, MV
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (12) : 3299 - 3304
  • [49] Vickers indentation fracture toughness of Y-TZP dental ceramics
    Coric, Danko
    Renjo, Marijana Majic
    Curkovic, Lidija
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2017, 64 : 14 - 19
  • [50] Validating a facile approach to measuring fracture toughness by instrumented indentation without imaging crack-lengths
    Hempel, Jacob L.
    Meyer, Andrew
    Hill, Ryan
    Cheng, Yang-Tse
    MRS COMMUNICATIONS, 2022, 12 (02) : 279 - 282