Estimation of Schottky contacts to porous Si by photoacoustic spectroscopy

被引:5
|
作者
Kawahara, T
Funaki, S
Okamoto, M
Inoue, Y
Tahira, K
Okamoto, Y
Morimoto, J
机构
[1] Natl Def Acad, Dept Mat Sci & Engn, Yokosuka, Kanagawa 2398686, Japan
[2] Natl Def Acad, Dept Elect & Elect Engn, Yokosuka, Kanagawa 2398686, Japan
关键词
PAS; photoacoustic spectroscopy; porous Si; Schottky contacts; I-V characteristics;
D O I
10.1143/JJAP.43.2932
中图分类号
O59 [应用物理学];
学科分类号
摘要
The photoacoustic (PA) spectra of porous Si (PS) were measured using a microphone under various surface treatments such as vibration during anodisation, vibration during rinsing, and acid surface treatment before contact deposition. The Fourier transform infrared (FTIR) spectra were also compared for the estimation of surface conditions. To obtain good contacts for electroluminescence (EL) devices, where a large injection current during operation is required, the vibration during rinsing in distilled (DI) water and hydrochloric (HCl) acid surface treatment are important. The PA signals increase with such vibration because of the enhancement of the pressure effects in pores of PS. Moreover, the decrease in PA signals caused by the surface change of pores can be also observed with the surface treatments. As the good contacts are obtained both by the vibration and surface treatments, the surface states in the pores seem to be important for the contacts to PS. This process can be monitored by PA spectroscopy in a noncontact manner because the PA signals from the PS are enhanced in the pores by the pressure effects, and PA spectroscopy can be sensitive to the change in surface of pores of PS.
引用
收藏
页码:2932 / 2935
页数:4
相关论文
共 50 条
  • [41] FT-IR photoacoustic spectroscopy of porous SiC layer
    Du, YL
    Li, K
    Wu, BM
    Lee, T
    Kim, Y
    PROGRESS IN NATURAL SCIENCE, 2001, 11 : S205 - S209
  • [42] ELECTRICAL CHARACTERISTICS OF ION BOMBARDED NI/N-SI SCHOTTKY CONTACTS
    MYBURG, G
    MALHERBE, JB
    FRIEDLAND, E
    APPLIED SURFACE SCIENCE, 1989, 43 : 242 - 247
  • [43] Schottky and ohmic contacts to doped Si1-x-yGexCy layers
    Peterson, JJ
    Hunt, CE
    Robinson, M
    SOLID-STATE ELECTRONICS, 1999, 43 (09) : 1725 - 1734
  • [44] Electrical characterization of inhomogeneous Ni2Si/SiC Schottky contacts
    Roccaforte, F
    La Via, F
    Raineri, V
    Pierobon, R
    Zanoni, E
    SILICON CARBIDE AND RELATED MATERIALS 2003, PRTS 1 AND 2, 2004, 457-460 : 869 - 872
  • [45] MODELING OF CRSI2-SI AND MOSI2-SI SCHOTTKY-BARRIER CONTACTS
    DONOVAL, D
    SNOWDEN, CM
    NAGL, V
    RACKO, J
    BARUS, M
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1995, 42 (06) : 1187 - 1189
  • [46] FORMATION OF SHALLOW SCHOTTKY CONTACTS TO SI USING PT-SI AND PD-SI ALLOY-FILMS
    EIZENBERG, M
    FOELL, H
    TU, KN
    JOURNAL OF APPLIED PHYSICS, 1981, 52 (02) : 861 - 868
  • [47] THE APPLICATION OF AUGER-ELECTRON SPECTROSCOPY IN CHARACTERIZING SCHOTTKY AND OHMIC CONTACTS TO GAAS
    KULKARNI, AK
    SURFACE AND INTERFACE ANALYSIS, 1988, 11 (6-7) : 400 - 400
  • [48] Porous alloyed W/Si contacts for light emitting devices
    Ichinohe, T
    Masaki, S
    Nozaki, S
    Morisaki, H
    PROCEEDINGS OF THE INTERNATIONAL SYMPOSIUM ON PITS AND PORES: FORMATION, PROPERTIES, AND SIGNIFICANCE FOR ADVANCED LUMINESCENT MATERIALS, 1997, 97 (07): : 517 - 523
  • [49] A transport analysis of the BEEM spectroscopy of Au/Si Schottky barriers
    Hohenester, U
    Kocevar, P
    deAndres, P
    Flores, F
    PHYSICA STATUS SOLIDI B-BASIC RESEARCH, 1997, 204 (01): : 397 - 399
  • [50] Effects of the annealing temperature on Ni silicide/n-Si(100) Schottky contacts
    Zhu, SY
    Van Meirhaeghe, RL
    Forment, S
    Ru, GP
    Li, BZ
    SOLID-STATE ELECTRONICS, 2004, 48 (01) : 29 - 35