In Situ Observation of Oxidation of Liquid Droplets of Tin and Melting Behavior of a Tin Particle Covered With a Tin Oxide Layer

被引:3
|
作者
Mima, Takayuki [2 ]
Takeuchi, Hironori [2 ]
Arai, Shigeo [1 ]
Kishita, Keisuke [3 ]
Kuroda, Kotaro [2 ]
Saka, Hiroyasu [1 ]
机构
[1] Nagoya Univ, Ecotopia Sci Inst, 1MV Electron Microscopy Lab, Nagoya, Aichi 4648603, Japan
[2] Nagoya Univ, Grad Sch Engn, Nagoya, Aichi 4648603, Japan
[3] Toyota Motor Co Ltd, Mat Anal Dept, Toyota 4718542, Japan
关键词
liquid metal; solid-liquid interface; oxidation; TRANSMISSION ELECTRON-MICROSCOPY; GROWTH-PROCESS; INSITU OBSERVATION; INTERFACE; CRYSTAL; BI;
D O I
10.1002/jemt.20675
中图分类号
R602 [外科病理学、解剖学]; R32 [人体形态学];
学科分类号
100101 ;
摘要
Oxidation of a liquid droplet of tin (Sn) was observed using an in situ specimen heating holder in an oxygen environment. The surface of the Sn liquid droplet was covered with a tin oxide layer, Sn3O4, the thickness of which depended on the oxygen pressure and temperature. Subsequent cooling of the droplet resulted in the formation of a solid Sn particle covered with a Sn3O4 layer. The solid Sn particle was then heated above the melting temperature of Sn, and the melting behavior of Sn was observed. Microsc. Res. Tech. 72:223-231, 2009. (C) 2009 Wiley-Liss, Inc.
引用
收藏
页码:223 / 231
页数:9
相关论文
共 50 条
  • [1] Kinetically limited de-lithiation behavior of nanoscale tin-covered tin oxide nanowires
    Meduri, Praveen
    Clark, Ezra
    Dayalan, Ethirajulu
    Sumanasekera, Gamini U.
    Sunkara, Mahendra K.
    ENERGY & ENVIRONMENTAL SCIENCE, 2011, 4 (05) : 1695 - 1699
  • [2] OXIDATION BEHAVIOR OF MONOLITHIC TIN AND TIN DISPERSED IN CERAMIC MATRICES
    GOGOTSI, YG
    PORZ, F
    DRANSFIELD, G
    OXIDATION OF METALS, 1993, 39 (1-2): : 69 - 91
  • [3] Atomic layer deposition of tin oxide and zinc tin oxide using tetraethyltin and ozone
    Warner, Ellis J.
    Johnson, Forrest
    Campbell, Stephen A.
    Gladfelter, Wayne L.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2015, 33 (02):
  • [4] Tin antimony oxide oxidation catalysts
    Berry, FJ
    HYPERFINE INTERACTIONS, 1998, 111 (1-4): : 35 - 37
  • [5] Oxidation of liquid alloys of tin with silver
    Denisov V.M.
    Antonova L.T.
    Talashmanova Y.S.
    Russian Journal of Non-Ferrous Metals, 2007, 48 (6) : 430 - 432
  • [6] Tin oxide atomic layer deposition from tetrakis(dimethylamino)tin and water
    Mullings, Marja N.
    Haegglund, Carl
    Bent, Stacey F.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2013, 31 (06):
  • [7] Atomic layer deposition of tin oxide films using tetrakis(dimethylamino) tin
    Elam, Jeffrey W.
    Baker, David A.
    Hryn, Alexander J.
    Martinson, Alex B. F.
    Pellin, Michael J.
    Hupp, Joseph T.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2008, 26 (02): : 244 - 252
  • [8] Effect of TiN particle size on wear behavior of SiAlON-TiN composites
    Bilecik, Nurcan Calis Acikbas
    Islak, Bilge Yaman
    Bilecik, Gokhan Acikbas
    MATERIALS TESTING, 2020, 62 (12) : 1251 - 1258
  • [9] THE OXIDATION BEHAVIOR OF MONOLITHIC TIN CERAMIC
    TAMPIERI, A
    LANDI, E
    BELLOSI, A
    BRITISH CERAMIC TRANSACTIONS AND JOURNAL, 1991, 90 (06): : 194 - 196
  • [10] Re-melting behavior of tin coatings
    Kurtz, Olaf
    Barthelmes, Jürgen
    Rüther, Robert
    Kühlkamp, Peter
    Moniak, Alexander
    Galvanotechnik, 2013, 104 (02): : 276 - 287