Blistering in semi-solid die casting of aluminium alloys and its avoidance

被引:57
|
作者
Hu, X. G. [1 ,2 ,3 ]
Zhu, Q. [1 ,4 ]
Midson, S. P. [1 ,5 ]
Atkinson, H. V. [3 ]
Dong, H. B. [3 ]
Zhang, F. [1 ]
Kang, Y. L. [2 ]
机构
[1] Gen Res Inst Nonferrous Met, Beijing 100088, Peoples R China
[2] Univ Sci & Technol Beijing, Beijing 100083, Peoples R China
[3] Univ Leicester, Dept Engn, Leicester LE1 7RH, Leics, England
[4] Southern Univ Sci & Technol, Shenzhen 518055, Peoples R China
[5] Colorado Sch Mines, Golden, CO 80401 USA
关键词
Blistering; Semi-solid die casting; Process window; Heat treatment; Aluminium alloy 319s; AL-SI-CU; MICROSTRUCTURAL EVOLUTION; BEHAVIOR; THIXOFORMABILITY; SLURRIES;
D O I
10.1016/j.actamat.2016.11.032
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Semi-solid die casting of relatively high solid-fraction aluminum alloys (0.5-0.7 fraction solid) can be used for the production of high quality industrial components. However, surface blistering during solution heat treatment can still be a problem and is associated with the entrapment of gas whether from air or from burned lubricant. Here the mechanism for formation of blisters is presented. The Reynolds number in the surface layer of the semi-solid flow is then analysed to obtain the relationships with hydraulic diameter and flow velocity for different slurry temperatures. The hypothesis is that it is some flow instability at the flow front, even where the overall nature of the flow is essentially laminar, which is leading to the entrapment. The crucial finding is that if the Reynolds number is plotted against temperature there is a decrease followed by an increase. The position of this minimum is dependent on the ratio of fill velocity to the hydraulic diameter, v/D. Thus there is a 'sweet spot' in terms of temperature (i.e. fraction liquid), flow velocity and hydraulic diameter (i.e. die design) where the flow front has the maximum stability, giving maximum resistance to blister formation. This is in contrast with conventional wisdom which would suggest that low fractions liquid would give the most stable flow front. A rationale for this is presented in terms of the particle crowding at the relatively low fraction of liquid. Experimental results with aluminium alloy 319s as an exemplar, and a die which has varying cross sectional dimensions, are presented and validate the hypothesis. (c) 2016 Acta Materialia Inc. Published by Elsevier Ltd.
引用
收藏
页码:446 / 455
页数:10
相关论文
共 50 条
  • [31] Mechanical properties in the semi-solid state and hot tearing of aluminium alloys
    Eskin, DG
    Suyitno
    Katgerman, L
    PROGRESS IN MATERIALS SCIENCE, 2004, 49 (05) : 629 - 711
  • [32] Microstructure Comparison for AlSn20Cu Antifriction Alloys Prepared by Semi-Continuous Casting, Semi-Solid Die Casting, and Spray Forming
    Huang, Shuhui
    Zhu, Baohong
    Zhang, Yongan
    Liu, Hongwei
    Wu, Shuaishuai
    Xie, Haofeng
    METALS, 2022, 12 (10)
  • [33] Assessment of Mechanisms for Particle Migration in Semi-Solid High Pressure Die Cast Aluminium-Silicon Alloys
    Law, Madeleine
    Hulme-Smith, Christopher Neil
    Matsushita, Taishi
    Jonsson, Par G.
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2020, 4 (02):
  • [34] CASTING SEMI-SOLID METALS.
    Flemings, M.C.
    Mehrabian, R.
    Modern Casting, 1973, 63 (12) : 31 - 33
  • [35] Modelling and simulation of die casting process for A356 semi-solid alloy
    Fu, Jinlong
    Wang, Kaikun
    11TH INTERNATIONAL CONFERENCE ON TECHNOLOGY OF PLASTICITY, ICTP 2014, 2014, 81 : 1565 - 1570
  • [36] In-line ultrasonic monitoring of semi-solid magnesium die casting process
    Jen, CK
    Moisan, JF
    Zheng, CQ
    Loong, CA
    Kruger, SE
    Shehata, MT
    Essadiqi, E
    ULTRASONICS, 2004, 41 (10) : 777 - 784
  • [37] Feasibility of semi-solid die casting of ADC12 aluminum alloy
    Janudom, S.
    Rattanochaikul, T.
    Burapa, R.
    Wisutmethangoon, S.
    Wannasin, J.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (09) : 1756 - 1762
  • [38] THE INVESTIGATION ON THE RHEOLOGICAL BEHAVIOR OF SEMI-SOLID ALUMINUM ALLOY DURING DIE CASTING
    X.J. Yang and J.Liu School of Mechanic & Electronic Engineering
    ActaMetallurgicaSinica(EnglishLetters), 2002, (06) : 511 - 516
  • [39] Pressurized solidification of semi-solid aluminum die casting alloy A356
    Guo, Hong-Min
    Yang, Xiang-Jie
    Wang, Jia-Xuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 485 (1-2) : 812 - 816
  • [40] Pressurized solidification of semi-solid aluminum die casting alloy A356
    Guo, Hong-Min
    Yang, Xiang-Jie
    Wang, Jia-Xuan
    Journal of Alloys and Compounds, 2009, 485 (1-2): : 812 - 816