Cracking and residual stress in hybrid coatings on float glass

被引:49
|
作者
Malzbender, J [1 ]
de With, G [1 ]
机构
[1] Eindhoven Univ Technol, Lab Solid State & Mat Chem, NL-5600 MB Eindhoven, Netherlands
关键词
cracking; hybrid organic-inorganic coatings; spin coating technique; residual stress; fracture toughness;
D O I
10.1016/S0040-6090(99)00885-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Observations with respect to the cracking of hybrid organic-inorganic coatings applied on float glass are reported. The coatings were deposited using a spin coating technique. The films showed cracks above a critical thickness and delaminated largely from the substrate. A relationship between the crack spacing and the film thickness is reported, and described by a model relating multiple cracking and crack spacing to the coating thickness for elastic relaxation. Thicker films had a higher initial stress associated with a higher number of cracks. The residual stress was calculated using the bending of the delaminated coating fragments and was proportional to the squared coating thickness. The results on the residual stress and the critical thickness allowed the fracture toughness of the coatings to be determined. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:210 / 214
页数:5
相关论文
共 50 条
  • [21] Residual stress effects in stress-corrosion cracking
    J. Toribio
    Journal of Materials Engineering and Performance, 1998, 7 : 173 - 182
  • [22] Acid interleave coatings inhibit float-glass weathering, corrosion
    Schaut, RA
    Pantano, CG
    AMERICAN CERAMIC SOCIETY BULLETIN, 2005, 84 (10): : 44 - 49
  • [23] Special features of functional coatings preparation upon float glass production
    Gorin, A.E.
    Bondareva, L.N.
    Martynenko, V.B.
    Steklo i Keramika, 2004, (04): : 11 - 12
  • [24] 'GLASS FLOAT'
    MCNEIL, M
    LITERARY REVIEW, 1988, 31 (02) : 190 - 190
  • [25] Float glass
    McKee, Bradford
    ARCHITECT, 2007, 96 (08): : 68 - 75
  • [26] Influence of residual compressive stress on nanoindentation response of ion-exchanged aluminosilicate float glass on air and tin sides
    Li, Xiaoyu
    Jiang, Liangbao
    Zhang, Xiaowen
    Yan, Yue
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2014, 385 : 1 - 8
  • [27] STRESS RELAXATION OF GLASS FOR COATINGS
    MILLS, JJ
    LARSEN, DC
    AMERICAN CERAMIC SOCIETY BULLETIN, 1972, 51 (04): : 352 - &
  • [28] Residual stress and cracking in expanded austenite layers
    Hoeft, D
    Latella, BA
    Short, KT
    JOURNAL OF PHYSICS-CONDENSED MATTER, 2005, 17 (23) : 3547 - 3558
  • [29] Residual stress driven cracking in superalloy weldments
    Tung, David C.
    Lippold, John C.
    MATERIALS AT HIGH TEMPERATURES, 2017, 34 (03) : 186 - 193
  • [30] THE INFLUENCE OF RESIDUAL-STRESS ON FATIGUE CRACKING
    OKAMOTO, A
    NAKAMURA, H
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1990, 112 (03): : 199 - 203