COMPARISON OF P92 STEEL FATIGUE TEST RESULTS IN RELATION TO SPECIMEN SIZE AND MANUFACTURING

被引:0
|
作者
Volak, Josef [1 ]
Bunda, Zbynek [1 ]
Mentl, Vaclav [1 ]
机构
[1] Res & Testing Inst Plzen Sro, Plzen, Czech Republic
关键词
Small Fatigue Test; correlation; material P92; energetic components; waterjet cutting;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper describes fatigue properties of steel P92. This material is used as a standard in the energy industry, especially for production of pipes and flange branches and distance pieces of supercritical steam turbines. This material contains (unlike material P91) up to 2% of tungsten which has positive influence on creep strength increase. Compared to the P91 material, it is possible to reduce wall thickness of the P92 pipe up to 20%. Fatigue tests were carried out on standard samples and compared with SFT samples (Small Fatigue Test). SFT samples can be gently withdrawn from energy component by SSam 2 device made by company Rolls Royce. There is no necessity for shutdown of power plant. Thanks to the existing correlations between SFT and Fatigue tests, it is possible to determine mechanical properties of material from a small amount of withdrawn material. At the same time a comparison between a traditional way of sample production and a sample production by means of waterjet cutting was carried out.
引用
收藏
页数:5
相关论文
共 50 条
  • [21] Fatigue crack growth behavior of heat affected zone in P92 steel weldment
    Kim, BJ
    Ryu, SH
    Lim, BS
    METALS AND MATERIALS INTERNATIONAL, 2004, 10 (01) : 19 - 25
  • [22] Quantifying the constraint effect induced by specimen geometry on creep crack growth behavior in P92 steel
    Zhao, Lei
    Xu, Lianyong
    Han, Yongdian
    Jing, Hongyang
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2015, 94-95 : 63 - 74
  • [23] EFFECT OF MULTI-AXIAL STRESS ON CREEP DAMAGE BEHAVIOR FOR NOTCHED SPECIMEN OF P92 STEEL
    Shigeyama, Haruhisa
    Sugiura, Ryuji
    Yokobori, A. Toshimitsu, Jr.
    Matsuzaki, Takashi
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2013, VOL 6A: MATERIALS AND FABRICATION, 2014,
  • [24] Influence of dislocation density and grain size on precipitation kinetics on P92 grade steel
    Gururaj, K.
    Pal, Snehanshu
    MATERIALS TODAY-PROCEEDINGS, 2019, 18 : 1364 - 1374
  • [25] LOCAL CREEP EVALUATION OF P92 STEEL WELDMENT BY SMALL PUNCH CREEP TEST
    Bumjoon Kim
    Byeongsoo Lim
    Acta Mechanica Solida Sinica, 2008, (04) : 312 - 317
  • [26] LOCAL CREEP EVALUATION OF P92 STEEL WELDMENT BY SMALL PUNCH CREEP TEST
    Kim, Bumjoon
    Lim, Byeongsoo
    ACTA MECHANICA SOLIDA SINICA, 2008, 21 (04) : 312 - 317
  • [27] Experimental and numerical characterization of low cycle fatigue and creep fatigue behaviour of P92 steel welded joint
    Wang, X.
    Zhang, W.
    Gong, J.
    Jiang, Y.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 41 (03) : 611 - 624
  • [28] Local Creep Evaluation of P92 Steel Weldment by Small Punch Creep Test
    Bumjoon Kim
    Byeongsoo Lim
    Acta Mechanica Solida Sinica, 2008, 21 : 312 - 317
  • [29] Crack growth behaviour of P92 steel under creep and creep-fatigue conditions
    Shi, K. X.
    Lin, F. S.
    Wan, H. B.
    Wang, Y. F.
    MATERIALS AT HIGH TEMPERATURES, 2014, 31 (04) : 343 - 347
  • [30] Low Cycle Fatigue and Relaxation Performance of Ferritic-Martensitic Grade P92 Steel
    Juergens, Maria
    Olbricht, Juergen
    Fedelich, Bernard
    Skrotzki, Birgit
    METALS, 2019, 9 (01)