The effect of copper on the cyclic oxidation of Ti-48Al-2Cr-2Nb

被引:0
|
作者
Fergus, JW [1 ]
Harris, NL [1 ]
Long, CJ [1 ]
Salazar, VL [1 ]
Zhou, T [1 ]
Gale, WF [1 ]
机构
[1] Auburn Univ, Mat Res & Educ Ctr, Auburn, AL 36849 USA
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
One of the challenges in the application of gamma titanium aluminide alloys is the development of suitable joining techniques for fabrication and repair. Transient Liquid Phase (TLP) bonding with a copper-containing composite interlayer has been used successfully to join titanium aluminide alloys. The TLP bonding process introduces a small amount of copper into the alloy. Although the oxidation resistance of titanium aluminide alloys can be strongly affected by alloying additions, the amount of copper present in the TLP bond has been shown to be neutral or beneficial to the isothermal oxidation resistance of the alloy. The results presented in this paper similarly show that a small amount of copper (1 at%) does not significantly affect the cyclic oxidation of Ti-48 at% Al2 at% Cr-2 at% Nb, but that 2 at% Cu is detrimental to the cyclic oxidation resistance.
引用
收藏
页码:575 / 577
页数:3
相关论文
共 50 条
  • [31] Mechanical property and fracture behavior of the TiNb/Ti-48Al-2Cr-2Nb composite
    Zhang, QC
    He, GY
    Wu, JS
    Zhang, TX
    Cai, XZ
    RARE METAL MATERIALS AND ENGINEERING, 2001, 30 (05) : 372 - 375
  • [32] Grain-size control in Ti-48Al-2Cr-2Nb with yttrium additions
    P. B. Trivedi
    S. N. Patankar
    F. H. (Sam) Froes
    E. G. Baburaj
    A. Genç
    L. Ovecoglu
    Metallurgical and Materials Transactions A, 2002, 33 : 2729 - 2736
  • [33] Creep properties of a fully-lamellar Ti-48Al-2Cr-2Nb alloy
    Viswanathan, GB
    Kartikeyan, S
    Mills, MJ
    Vasudevan, VK
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 : 833 - 837
  • [34] Grain-size control in Ti-48Al-2Cr-2Nb with yttrium additions
    Trivedi, PB
    Baburaj, EG
    Genç, A
    Ovecoglu, L
    Patankar, SN
    Froes, FH
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (08): : 2729 - 2736
  • [35] Corrosion evaluation of Ti-48Al-2Cr-2Nb (at.%) in Ringer's solution
    Delgado-Alvarado, C.
    Sundaram, P. A.
    ACTA BIOMATERIALIA, 2006, 2 (06) : 701 - 708
  • [36] Microstructure stability of Ti2AlN/Ti-48Al-2Cr-2Nb composite at 900 °C
    Liu, Yi-wen
    Hu, Rui
    Zhang, Tie-bang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (02) : 423 - 430
  • [37] Influence of an oxidation protective coating upon hot corrosion and mechanical behaviour of Ti-48Al-2Cr-2Nb alloy
    Bacos, M-P
    Thomas, M.
    Raviart, J-L
    Morel, A.
    Mercier, S.
    Josso, P.
    INTERMETALLICS, 2011, 19 (08) : 1120 - 1129
  • [38] Influence of oxidation protective SiAl coatings on the tensile and fatigue behavior of Ti-48Al-2Cr-2Nb at elevated temperatures
    Guth, Stefan
    Swadzba, Radoslaw
    Breuner, Christoph
    Bauer, Peter-Philipp
    Nizamoglu, Sarper
    Mendala, Boguslaw
    Radwanski, Krzysztof
    Laska, Nadine
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 858
  • [39] Thermal Shock and Oxidation Behavior of HiPIMS TiAlN Coatings Grown on Ti-48Al-2Cr-2Nb Intermetallic Alloy
    Badini, Claudio
    Deambrosis, Silvia M.
    Padovano, Elisa
    Fabrizio, Monica
    Ostrovskaya, Oxana
    Miorin, Enrico
    D'Amico, Giuseppe C.
    Montagner, Francesco
    Biamino, Sara
    Zin, Valentina
    MATERIALS, 2016, 9 (12)
  • [40] Tensile deformation of Ti-48Al-2Cr-2Nb alloy experienced the high temperature oxidation in a simulated combustion gas
    Beijing Normal University, Beijing 100875, China
    不详
    Xiyou Jinshu Cailiao Yu Gongcheng, 2006, 3 (357-362):