Effect of T6 Heat Treatment on Dry Sliding Frictional Wear Characteristics of Al-20Si-5Cu Alloy

被引:1
|
作者
Jin, Yunxue [1 ]
Tong, Qiangqiang [1 ]
Wang, Xiaoya [1 ]
Chen, Hongmei [1 ]
机构
[1] Jiangsu Univ Sci & Technol, Prov Key Lab Adv Welding Technol, Zhenjiang 212003, Peoples R China
来源
关键词
hypereutectic Al-Si alloy; brake disc; T6 heat treatment; frictional wear; wear mechanism;
D O I
10.4028/www.scientific.net/AMR.750-752.591
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of T6 heat treatment on dry sliding friction and wear characteristics of Al-20Si-5Cu under a fixed sliding speed of 200r/min and sliding time of 30mins was illustrated in this paper. The result reveals that T6 heat treatment can improve morphology of primary Si and Al2Cu particles, enhance the hardness of the matrix. Wear rate increased with increasing of applied load. T6 heat treated samples have high wear resistance which is related to the improvement of microstructure, particularly with their increased hardness of matrix. But friction coefficient varies with heat treatment processes and has no sensitivity to applied loads, which fluctuates in a small range, so the friction coefficient can be considered to be stable. The wear mechanisms of T6 heat treated samples are also changed with increasing of applied load, from oxidative wear to fatigue wear.
引用
收藏
页码:591 / 595
页数:5
相关论文
共 50 条
  • [41] Effect of hard anodizing and T6 heat treatment on the dry sliding wear behavior of AlSi10Mg fabricated by direct metal laser sintering
    Vishnu, Vineesh
    Prabhu, T. Ram
    Vineesh, K. P.
    WEAR, 2025, 564
  • [42] Wear of spray deposited Al-6Cu-Mn alloy under dry sliding conditions
    Gui, MC
    Kang, SB
    Lee, JM
    WEAR, 2000, 240 (1-2) : 186 - 198
  • [43] Influence of Sn content on the microstructure and dry sliding wear behaviour of hypereutectic Al-20Si alloy
    Wu, X. F.
    Zhang, G. A.
    MATERIALS AND MANUFACTURING, PTS 1 AND 2, 2011, 299-300 : 265 - +
  • [44] Dry sliding friction and wear properties of Al-25Zn-3Cu-3Si alloy
    Savaskan, Temel
    Bican, Osman
    TRIBOLOGY INTERNATIONAL, 2010, 43 (08) : 1346 - 1352
  • [45] Effects of Mn Content on Microstructure, Mechanical and Dry Sliding Wear Properties of Eutectic Al–Si–Cu Alloy
    Yasin Alemdag
    Murat Beder
    Metals and Materials International, 2020, 26 : 1811 - 1819
  • [46] Effect of Precipitation During Quenching on the Prediction of the Mechanical Properties of Al-5 Pct Cu Alloy After T6 Treatment
    Yisen Hu
    Gang Wang
    Wenguang Wang
    Yiming Rong
    Metallurgical and Materials Transactions A, 2017, 48 : 5667 - 5677
  • [47] Dry sliding wear behaviour of thixoformed hypoeutectic Al-Si-Cu alloy with different amounts of magnesium
    Alhawari, K. S.
    Omar, M. Z.
    Ghazali, M. J.
    Salleh, M. S.
    Mohammed, M. N.
    COMPOSITE INTERFACES, 2016, 23 (06) : 519 - 531
  • [48] Influence of Mg addition and T6 heat treatment on microstructure, mechanical and tribological properties of Al-12Si-3Cu based alloy
    Beder, M.
    Alemdag, Y.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2021, 31 (08) : 2208 - 2219
  • [49] Effect of Precipitation During Quenching on the Prediction of the Mechanical Properties of Al-5 Pct Cu Alloy After T6 Treatment
    Hu, Yisen
    Wang, Gang
    Wang, Wenguang
    Rong, Yiming
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (11): : 5667 - 5677
  • [50] The Effects of T5 and T6 Heat Treatments on Wear Behaviour of AA6063 Alloy
    Ozyurek, Dursun
    Tuncay, Tansel
    Kaya, Hasan
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2014, 33 (03) : 231 - 237