Structural Origin of Suppressed Voltage Decay in Single-Crystalline Li-Rich Layered Li[Li0.2Ni0.2Mn0.6]O2 Cathodes

被引:29
|
作者
Yang, Xiaoxia [1 ]
Wang, Suning [1 ,2 ]
Han, Duzhao [1 ]
Wang, Kai [3 ]
Tayal, Akhil [4 ]
Baran, Volodymyr [4 ]
Missyul, Alexander [5 ]
Fu, Qiang [2 ]
Song, Jiangxuan [6 ]
Ehrenberg, Helmut [2 ]
Indris, Sylvio [2 ]
Hua, Weibo [1 ,2 ]
机构
[1] Xi An Jiao Tong Univ, Sch Chem Engn & Technol, 28 West Xianning Rd, Xian 710049, Peoples R China
[2] Karlsruhe Inst Technol KIT, Inst Appl Mat IAM, Hermann von Helmholtz Pl 1, D-76344 Eggenstein Leopoldshafen, Germany
[3] Karlsruhe Inst Technol KIT, Inst Nanotechnol INT, D-76344 Eggenstein Leopoldshafen, Germany
[4] Deutsch Elekt Synchrotron DESY, Notkestr 85, D-22607 Hamburg, Germany
[5] CELLS ALBA Synchrotron, E-08290 Barcelona, Spain
[6] Xi An Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Mech Behav Mat, 28 Xianning West Rd, Xian 710049, Peoples R China
基金
美国国家科学基金会;
关键词
in situ synchrotron-based techniques; Li- and Mn-rich cathode materials; single crystals; structural stability; voltage decay; ANIONIC REDOX; HIGH-CAPACITY; OXYGEN-REDOX; ION-EXCHANGE; HIGH-POWER; GROWTH;
D O I
10.1002/smll.202201522
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Lithium- and manganese-rich layered oxides (LMLOs, >= 250 mAh g(-1)) with polycrystalline morphology always suffer from severe voltage decay upon cycling because of the anisotropic lattice strain and oxygen release induced chemo-mechanical breakdown. Herein, a Co-free single-crystalline LMLO, that is, Li[Li0.2Ni0.2Mn0.6]O-2 (LLNMO-SC), is prepared via a Li+/Na+ ion-exchange reaction. In situ synchrotron-based X-ray diffraction (sXRD) results demonstrate that relatively small changes in lattice parameters and reduced average micro-strain are observed in LLNMO-SC compared to its polycrystalline counterpart (LLNMO-PC) during the charge-discharge process. Specifically, the as-synthesized LLNMO-SC exhibits a unit cell volume change as low as 1.1% during electrochemical cycling. Such low strain characteristics ensure a stable framework for Li-ion insertion/extraction, which considerably enhances the structural stability of LLNMO during long-term cycling. Due to these peculiar benefits, the average discharge voltage of LLNMO-SC decreases by only approximate to 0.2 V after 100 cycles at 28 mA g(-1) between 2.0 and 4.8 V, which is much lower than that of LLNMO-PC (approximate to 0.5 V). Such a single-crystalline strategy offers a promising solution to constructing stable high-energy lithium-ion batteries (LIBs).
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Enhanced high-voltage properties of LiCoO2 coated with Li[Li0.2Mn0.6Ni0.2]O2
    Hu, Guo-rong
    Cao, Jing-chao
    Peng, Zhong-dong
    Cao, Yan-bing
    Du, Ke
    ELECTROCHIMICA ACTA, 2014, 149 : 49 - 55
  • [42] Fabrication and electrochemical performance of Li[Li0.2Ni0.2Mn0.6]O2 coated with Li2ZrO3 as cathode material for lithium-ion batteries
    Lin Jia-ming
    Zhao Tao-lin
    Wang Yu-hua
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2020, 48 (03): : 112 - 120
  • [43] 锂离子电池富锂材料Li[Li0.2Ni0.2Mn0.6]O2的制备及掺杂改性
    朱伟雄
    李新海
    王志兴
    郭华军
    中国有色金属学报, 2013, 23 (04) : 1047 - 1052
  • [44] Hybrid annealing method synthesis of Li [Li0.2Ni0.2Mn0.6]O2 composites with enhanced electrochemical performance for lithium-ion batteries
    Liu, Jin-Bei
    Kong, Ling-Bin
    Xing, Man
    Shi, Ming
    Luo, Yong-Chun
    Kang, Long
    RSC ADVANCES, 2015, 5 (05) : 3352 - 3357
  • [45] 高容量正极材料Li[Li0.2Ni0.2Mn0.6]O2的合成及电化学性能
    杜柯
    黄霞
    胡国荣
    彭忠东
    中国有色金属学报, 2012, 22 (04) : 1201 - 1208
  • [46] Cyclic deterioration and its improvement for Li-rich layered cathode material Li[Ni0.17Li0.2Co0.07Mn0.56]O2
    Ito, Atsushi
    Li, Decheng
    Sato, Yuichi
    Arao, Masazumi
    Watanabe, Manabu
    Hatano, Masaharu
    Horie, Hideaki
    Ohsawa, Yasuhiko
    JOURNAL OF POWER SOURCES, 2010, 195 (02) : 567 - 573
  • [47] Hierarchical Mesoporous Lithium-Rich Li[Li0.2Ni0.2Mn0.6]O2 Cathode Material Synthesized via Ice Templating for Lithium-Ion Battery
    Li, Yu
    Wu, Chuan
    Bai, Ying
    Liu, Lu
    Wang, Hui
    Wu, Feng
    Zhang, Na
    Zou, Yufeng
    ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (29) : 18832 - 18840
  • [48] 富锂锰基正极材料Li[Li0.2Ni0.2Mn0.6]O2的纳米TiO2掺杂改性
    王伟刚
    胡国荣
    周兴华
    彭忠东
    杜柯
    华南理工大学学报(自然科学版), 2017, 45 (10) : 39 - 45
  • [49] Preparation and characterization of spinel-layered mixed structural 0.2LiNi0.5Mn1.5O4•0.8Li[Li0.2Ni0.2Mn0.6]O2 as cathode materials for lithium-ion batteries
    Ge, Tao
    Guo, Zhaoxin
    Wu, Minfang
    Sun, Rui
    Li, Weili
    Yang, Gang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 801 : 254 - 261
  • [50] Lithium-Rich Li[Li0.2Ni0.2Mn0.6]O2/Hierarchical Porous Graphitic Carbon Composites Promoters for Polysulfides Regulation in Lithium-Sulfur Batteries
    Zhong, Haoxiang
    Hu, Qianqian
    Zhang, Lingzhi
    ENERGY TECHNOLOGY, 2022, 10 (12)