Recovery of Iron from Copper Slag Using Coal-Based Direct Reduction: Reduction Characteristics and Kinetics

被引:26
|
作者
Zhang, Hanquan [1 ]
Hu, Chaojie [1 ]
Gao, Wangjie [1 ]
Lu, Manman [2 ]
机构
[1] Wuhan Inst Technol, Sch Resources & Safety Engn, Wuhan 430205, Peoples R China
[2] Cent South Univ, Sch Minerals Proc & Bioengn, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
copper slag; direct reduction; reduction kinetics; pellet; MAGNETIC SEPARATION; MECHANISM; HEMATITE; CONCRETE; CARBON; FINES;
D O I
10.3390/min10110973
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
The Fe3O4 and Fe2SiO4 in copper slag were successfully reduced to metallic iron by coal-based direct reduction. Under the best reduction conditions of 1300 degrees C reduction temperature, 30 min reduction time, 35 wt.% coal dosage, and 20 wt.% CaO dosage (0.75 binary basicity), the Fe grade of obtained iron concentration achieved 91.55%, and the Fe recovery was 98.13%. The kinetic studies on reduction indicated that the reduction of copper slag was controlled by the interfacial reaction and carbon gasification at 1050 degrees C. When at a higher reduction temperature, the copper slag reduction was controlled by the diffusion of the gas. The integral kinetics model research illustrated that the reaction activation energy increased as the reduction of copper slag proceeded. The early reduction of Fe3O4 needed a low reaction activation energy. The subsequent reduction of Fe2SiO4 needed higher reaction activation energy compared with that of Fe3O4 reduction.
引用
收藏
页码:1 / 17
页数:18
相关论文
共 50 条
  • [31] Iron recovery from flotation middling produced in carbonates-bearing hematite ore using coal-based reduction
    Gao, Peng
    Ji, Xin
    Ren, Duo-Zhen
    Han, Yue-Xin
    Zhongguo Kuangye Daxue Xuebao/Journal of China University of Mining and Technology, 2013, 42 (05): : 812 - 816
  • [32] Research on the coal-based direct reduction of vanadium titanomagenetite
    Jiang, Tao
    Guan, Shanfei
    Xia, Yi
    Yu, Shaowu
    Xue, Xiangxin
    Bai, Ruiguo
    Chen, Donghui
    Chang, Fuzeng
    MATERIALS PROCESSING AND MANUFACTURING III, PTS 1-4, 2013, 753-755 : 16 - +
  • [33] Development of coal-based direct reduction ironmaking process
    Kobe Steel, Ltd., Kobe, Japan
    1600, 26-33 (2005):
  • [34] BEHAVIOR OF COAL-BASED DIRECT REDUCTION REACTION OF IRON OXIDE PELLETS BY MICROWAVE HEATING
    Huang Zhu-cheng
    Wang Hua
    Hu Bing
    Peng Hu
    Xia Guang-bin
    2ND INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING, 2011, : 15 - 24
  • [35] Iron Recovery from Discarded Copper Slag in a RHF Direct Reduction and Subsequent Grinding/Magnetic Separation Process
    Cao, Zhicheng
    Sun, Tichang
    Xue, Xun
    Liu, Zhanhua
    MINERALS, 2016, 6 (04):
  • [36] Kinetics of reduction of copper oxide from liquid slag using carbon
    Reddy, RG
    Prabhu, VL
    Mantha, D
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2003, 22 (01) : 25 - 33
  • [37] Kinetics and mechanism of coal-based direct reduction of high-chromium vanadium–titanium magnetite
    Jian Yang
    Tao Jiang
    Shi-hong Ma
    Song-tao Yang
    Mi Zhou
    Journal of Iron and Steel Research International, 2022, 29 : 1723 - 1733
  • [38] Reaction Mechanism of Siderite Lump in Coal-Based Direct Reduction
    Zhu, Deqing
    Luo, Yanhong
    Pan, Jian
    Zhou, Xianlin
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2016, 35 (02) : 185 - 194
  • [39] Effect of roasting temperature on the coal-based direct reduction of high-iron vanadium tailings
    Yang, Hui-Fen
    Wang, Jing-Jing
    Jing, Li-Li
    Dang, Chun-Ge
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2010, 32 (10): : 1258 - 1263
  • [40] Thermogravimetric study of the reduction of copper slag by biomassReduction characteristics and kinetics
    Zongliang Zuo
    Qingbo Yu
    Mengqi Wei
    Huaqing Xie
    Wenjun Duan
    Kun Wang
    Qin Qin
    Journal of Thermal Analysis and Calorimetry, 2016, 126 : 481 - 491