Improvement of the Adhesive Fracture Toughness of Bonded Aluminum Joints Using E-Glass Fibers at Cryogenic Temperature

被引:23
|
作者
Yoon, Soon Ho [1 ]
Kim, Byung Chul [1 ]
Lee, Kwan Ho [1 ]
Lee, Dai Gil [1 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Mech Engn, Taejon 305701, South Korea
关键词
Adhesive joints; glass fibers; fracture toughness; crack propagation; fiber bridging; DCB test; COMPOSITE;
D O I
10.1163/016942409X12541266699635
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Fracture toughness and crack resistance of aluminum adhesive joints were measured at the cryogenic temperature of -150 degrees C, with respect to the orientation and volume fraction of the E-glass fibers in the epoxy adhesive. Cleavage tests on the DCB (Double Cantilever Beam) adhesive joints were performed using two different test rates of 1.67 x 10(-2) and 8.33 x 10(-4) mm/s to observe the crack propagation trends. From the experiments, it was found that the DCB joints bonded with the epoxy adhesive reinforced with E-glass fibers not only showed a stable crack propagation with a low crack propagation speed, but also higher fracture toughness and crack resistance than those of the DCB joints bonded with the unreinforced epoxy adhesive at a cryogenic temperature of -150 degrees C. (C) Koninklijke Brill NV, Leiden, 2010
引用
收藏
页码:429 / 444
页数:16
相关论文
共 50 条