Improvement of Interlaminar Fracture Toughness in Glass Fiber Reinforced Plastic Laminates with Inorganic Nanofiber Sheet Interleaf

被引:3
|
作者
Wu, Ning [1 ]
Yang, Jie [1 ]
Zheng, Shanshan [1 ]
Wang, Jing [1 ]
Chen, Li [1 ]
机构
[1] Tianjin Polytech Univ, Inst Composite Mat, Minist Educ, Lab Adv Text Composites, Tianjin 300387, Peoples R China
基金
中国国家自然科学基金;
关键词
TiO2 nanofiber sheet; Laminates; Fracture toughness; Fracture surface analysis; Interlayer toughing mechanism; MODE-I; SURFACE-PROPERTY; HMPBO FIBERS; COMPOSITES; DELAMINATION; ENHANCEMENT; THICKNESS;
D O I
10.1007/s12221-019-1226-5
中图分类号
TB3 [工程材料学]; TS1 [纺织工业、染整工业];
学科分类号
0805 ; 080502 ; 0821 ;
摘要
The present study developed a new type of nanofibrous structure-TiO2 nanofiber sheets (TNFS) to increase the interlaminar fracture toughness of glass fiber reinforced polymer (GFRP) laminates. SEM was employed to characterize the nanofibers before and after calcination. In order to quantify TNFS, the thickness and the crevice area of TNFS were analyzed, the results showed that the thickness and the proportion of crevice area were increased with the increase of TNFS contents. Mode I and Mode II interlaminar fracture toughness were investigated for GFRP laminates toughened by different mass fraction of TNFS. The highest Mode I fracture toughness value achieved by inserting 5 wt.% TNFS in the interleaf. G(Ic) value was 74.35 % higher than those of base GFRP laminates. Meanwhile, with 6 wt.% addition of TNFS, the GFRP laminates showed the highest Mode II fracture toughness, which is 60.76 % higher than those of base GFRP laminates. The improvement mechanism of toughness was illustrated by the fracture surface analysis of TNFS interlayered laminates.
引用
收藏
页码:2175 / 2183
页数:9
相关论文
共 50 条
  • [41] Mode III interlaminar fracture behavior of glass fiber reinforced polymer woven laminates at 293 to 4 k
    Rizov, Victor
    Shindo, Yasuhide
    Horiguchi, Katsumi
    Narita, Fumio
    APPLIED COMPOSITE MATERIALS, 2006, 13 (05) : 287 - 304
  • [42] INFLUENCE OF SILANE COUPLING AGENTS ON INTERLAMINAR FRACTURE IN GLASS-FIBER FABRIC REINFORCED UNSATURATED POLYESTER LAMINATES
    SUZUKI, Y
    MAEKAWA, Z
    HAMADA, H
    YOKOYAMA, A
    SUGIHARA, T
    HOJO, M
    JOURNAL OF MATERIALS SCIENCE, 1993, 28 (07) : 1725 - 1732
  • [43] Fracture and interlaminar properties of clay-modified epoxies and their glass reinforced laminates
    Quaresimin, Marino
    Salviato, Marco
    Zappalorto, Michele
    ENGINEERING FRACTURE MECHANICS, 2012, 81 : 80 - 93
  • [44] Mode III Interlaminar Fracture Behavior of Glass Fiber Reinforced Polymer Woven Laminates at 293 to 4 K
    Victor Rizov
    Yasuhide Shindo
    Katsumi Horiguchi
    Fumio Narita
    Applied Composite Materials, 2006, 13 : 287 - 304
  • [45] Fracture toughness of fiber-reinforced glass concrete
    Meyer, C
    Monawar, TM
    HIGH PERFORMANCE FIBER REINFORCED CEMENT COMPOSITES (HPFRCC3), 1999, 6 : 261 - 269
  • [46] Interlaminar fracture toughness of carbon/epoxy composites laminates toughened by short carbon fiber
    Wang, Yongan
    Shen, Wei
    Chen, Lifeng
    Zhu, Lvtao
    Natsuki, Toshiaki
    POLYMER COMPOSITES, 2023, 44 (08) : 5261 - 5271
  • [47] Experimental determination of fracture toughness of woven/chopped glass fiber hybrid reinforced thermoplastic composite laminates
    Ozdemir, A. O.
    Karatas, C.
    SCIENTIA IRANICA, 2021, 28 (04) : 2202 - 2212
  • [48] Influence of interlaminar fracture toughness on impact resistance of glass fibre reinforced polymers
    Kuboki, T
    Jar, PYB
    Forest, TW
    COMPOSITES SCIENCE AND TECHNOLOGY, 2003, 63 (07) : 943 - 953
  • [49] Mode I and mode II interlaminar fracture toughness of CFRP laminates toughened by carbon nanofiber interlayer
    Arai, Masahiro
    Noro, Yukihiro
    Sugimoto, Koh-Ichi
    Endo, Morinobu
    COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (02) : 516 - 525
  • [50] Improvement of mode I interlaminar fracture toughness of composites reinforced by ultrathin fibers
    School of Aeronautics, Astronautics and Mechanics, Tongji University, Shanghai 200092, China
    Fuhe Cailiao Xuebao, 2007, 4 (166-171):