Characterization of the residual stresses introduced by a new joining method in diamond and tungsten carbide composites

被引:5
|
作者
Lavigne, Olivier [1 ]
Luzin, Vladimir [2 ]
Mendez, Marco [1 ]
Malik, Abds-Sami [3 ]
Carrasco, Oscar [1 ]
Salvemini, Floriana [2 ]
机构
[1] Hyper Mat & Technol, Pol Ind Roca, C Verneda S-N, Barcelona 08107, Spain
[2] ANSTO, Lucas Heights, NSW 2234, Australia
[3] Hyper Mat & Technol, 6325 Huntley Rd, Worthington, OH 43085 USA
关键词
Diamond composite; Cemented carbide composite; Co-sintering; Bond strength; Neutron diffraction; Residual stresses; Neutron tomography;
D O I
10.1016/j.ijrmhm.2019.105051
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, a co-sintering method was used to attach diamond to cemented carbide composites. The joining method consists of sintering a green part (ring) of cemented carbide (CC) around a thermally stable diamond composite (TSDC) part (plug) to radially contain it. During the sintering step, the green body shrinks to a controlled level and therefore forms interference fit between the two parts (mismatch between the inner diameter (ID) of the CC ring and the outer diameter (OD) of the TSDC cylinder). The residual stresses induced by this process as well as the bond strength between the CC and the TSDC parts were quantitatively evaluated. It is shown that the interface pressure between the two parts, and the level of residual stresses, increased with increase in the designed interference fit, as well as with the increase of the ID/OD ratios of the CC ring. For the chosen material combination (cemented carbide ring comprised 90 vol% WC and 10 vol% Co with medium coarse WC grains; diamond composite plug comprised 84 vol% diamond and 16 vol% SiC), the values of the hoop stresses at the interface in the CC ring measured by neutron diffraction was determined to be between 150 MPa and 550 MPa, depending on the ID/OD ratio. It was also found that for a given ID/OD ratio, the increase of the designed interference fit had little effect on that attained due to the plastic deformation of the cemented carbide material at the interface during the sintering (dynamic) process. A mechanical bond around 60 MPa was nevertheless achieved.
引用
收藏
页数:6
相关论文
共 50 条
  • [21] Measurement of residual stresses in layered composites by compliance method
    Ersoy, N
    Vardar, O
    JOURNAL OF COMPOSITE MATERIALS, 2000, 34 (07) : 575 - 598
  • [22] A novel method to measure residual stresses in laminated composites
    Ifju, PG
    Kilday, BC
    Niu, XK
    Liu, SC
    JOURNAL OF COMPOSITE MATERIALS, 1999, 33 (16) : 1511 - 1524
  • [23] RESIDUAL-STRESSES IN SILICON-CARBIDE PARTICULATE REINFORCED ALUMINUM COMPOSITES
    SUN, ZM
    LI, JB
    WANG, ZG
    LI, WJ
    ACTA METALLURGICA ET MATERIALIA, 1992, 40 (11): : 2961 - 2966
  • [24] Surface properties of graphene and graphene/diamond composites located at a substrate with tungsten carbide doped by metals composites
    Terpilowski, Konrad
    Szaniawska, Magdalena
    ADSORPTION-JOURNAL OF THE INTERNATIONAL ADSORPTION SOCIETY, 2019, 25 (03): : 513 - 520
  • [25] Surface properties of graphene and graphene/diamond composites located at a substrate with tungsten carbide doped by metals composites
    Konrad Terpiłowski
    Magdalena Szaniawska
    Adsorption, 2019, 25 : 513 - 520
  • [26] Semi-quantitative Characterization of Residual Stresses of Polycrystalline Diamond Compacts
    Liu, Fang
    Fan, Wenjie
    Zhou, Chuanxun
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 665 - +
  • [27] Characterization of residual stresses near interfaces in SiCfAl model composites
    Liu, C.
    Qin, J.N.
    Zhang, G.D.
    Naka, M.
    Shanghai Jiaotong Daxue Xuebao/Journal of Shanghai Jiaotong University, 2001, 35 (03): : 368 - 370
  • [28] Effect of rare earth on diamond-tungsten carbide super-hard composites
    Man, CH
    Zhao, HY
    Ning, GF
    JOURNAL OF RARE EARTHS, 2003, 21 : 159 - 161
  • [29] Effect of Rare Earth on Diamond-Tungsten Carbide Super-Hard Composites
    满翠华
    赵会友
    宁桂峰
    Journal of Rare Earths, 2003, (S1) : 159 - 161
  • [30] RADIATION ANALYTICAL MATERIAL CHARACTERIZATION OF DIAMOND LAYERS DEPOSITED ONTO TUNGSTEN CARBIDE
    ULLRICH, HJ
    SCHLAUBITZ, M
    HAUBNER, R
    LUX, B
    MIKROCHIMICA ACTA, 1992, 107 (3-6) : 257 - 263