The differences between the corrosion process of the bath and the top side of float glass and the dependence on the corrosion process on the thickness of the glass could be demonstrated by ellipsometric measurements of defined corroded float glasses. The effectiveness of different cleaning procedures on corroded float glass surfaces is discussed. Ellipsometry can help determine suitable separating agent for the storage of float glass sheets. (C) 1997 Elsevier Science B.V.
引用
收藏
页码:205 / 209
页数:5
相关论文
共 50 条
  • [31] Studies on the initial stages of zinc atmospheric corrosion in the presence of chloride
    Chen, Y. Y.
    Chung, S. C.
    Shih, H. C.
    CORROSION SCIENCE, 2006, 48 (11) : 3547 - 3564
  • [32] Initial stages of the copper corrosion in sulfite-containing solutions
    Val'syunas, I.
    Mechinskas, P.
    Yasulajtene, V.
    Lejnartas, K.
    Zashchita Metallov, 2002, 38 (01): : 77 - 83
  • [33] Optical interference system for controlling float-glass ribbon thickness at hot stages of production
    Novikov, MA
    Tertyshnik, AD
    Ivanov, VV
    Markelov, VA
    Goryunov, AV
    Volkov, PV
    Morozov, AP
    Chuplygin, VN
    Granek, AI
    Knyazev, SY
    Mishulin, YA
    Peskov, VP
    GLASS AND CERAMICS, 2004, 61 (1-2) : 37 - 41
  • [34] INITIAL-STAGES OF ATMOSPHERIC CORROSION OF STEEL IN THE ARABIAN GULF
    ALLAM, IM
    ARLOW, JS
    SARICIMEN, H
    CORROSION SCIENCE, 1991, 32 (04) : 417 - &
  • [35] Optical Interference System for Controlling Float-Glass Ribbon Thickness at Hot Stages of Production
    M. A. Novikov
    A. D. Tertyshnik
    V. V. Ivanov
    V. A. Markelov
    A. V. Goryunov
    P. V. Volkov
    A. P. Morozov
    V. N. Chuplygin
    A. I. Granek
    S. Yu. Knyazev
    Yu. A. Mishulin
    V. P. Peskov
    Glass and Ceramics, 2004, 61 : 37 - 41
  • [36] Initial Stages of the Copper Corrosion in Sulfite-Containing Solutions
    I. Val'syunas
    P. Mechinskas
    V. Yasulaitene
    K. Leinartas
    Protection of Metals, 2002, 38 : 71 - 77
  • [37] INITIAL STAGES OF STRESS CORROSION CRACKING IN AUSTENITIC STAINLESS STEELS
    LOUTHAN, MR
    CORROSION, 1965, 21 (09) : 288 - &
  • [38] Exciton absorption at the initial stages of the formation of the CuCl phase in a glass
    P. M. Valov
    V. I. Leĭman
    Optics and Spectroscopy, 2007, 103 : 585 - 591
  • [39] Exciton absorption at the initial stages of the formation of the CuCl phase in a glass
    Valov, P. M.
    Leiman, V. I.
    OPTICS AND SPECTROSCOPY, 2007, 103 (04) : 585 - 591
  • [40] DYNAMIC FATIGUE OF FLOAT GLASS
    CHANDAN, HC
    BRADT, RC
    RINDONE, GE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1978, 61 (5-6) : 207 - 210