On critical hydrogen concentration for hydrogen embrittlement of Fe3Al

被引:2
|
作者
Priyadarshi, A [1 ]
Balasubramaniam, R [1 ]
机构
[1] Indian Inst Technol, Dept Met & Mat Engn, Kanpur 208016, Uttar Pradesh, India
关键词
iron aluminides; hydrogen embrittlement; critical hydrogen concentration; decohesion; mechanism;
D O I
10.1007/BF02706731
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The critical hydrogen concentration for hydrogen embrittlement in iron aluminide, Fe3Al has been estimated (0.42 wppm). The estimated critical hydrogen content has been correlated to structural aspects of the decohesion mechanism of hydrogen embrittlement.
引用
收藏
页码:559 / 562
页数:4
相关论文
共 50 条
  • [41] Metal dusting of Fe3Al and (Fe,Ni)(3)Al
    Strauss, S
    Krajak, R
    Palm, M
    Grabke, HJ
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1996, 47 (12): : 701 - 702
  • [42] IMPURITY SEGREGATION AND HYDROGEN EMBRITTLEMENT OF FE AND NI
    JONES, RH
    BRUEMMER, SM
    THOMAS, MT
    BAER, DR
    JOURNAL OF METALS, 1982, 34 (08): : 40 - 40
  • [43] HYDROGEN EMBRITTLEMENT OF FE-NI MARTENSITES
    WAYMAN, ML
    SMITH, GC
    METALLURGICAL TRANSACTIONS, 1970, 1 (05): : 1189 - &
  • [44] The effects of boron and hydrogen on the embrittlement of polycrystalline Ni3AL
    Wang, FH
    Shang, JX
    Li, JM
    Wang, CY
    INTERMETALLICS, 2000, 8 (5-6) : 589 - 593
  • [45] HYDROGEN EMBRITTLEMENT OF Ni3Al plus B.
    Kuruvilla, A.K.
    Stoloff, N.S.
    1986, : 711 - 715
  • [46] HYDROGEN EMBRITTLEMENT IN A MG-AL ALLOY
    CHAKRAPANI, DG
    PUGH, EN
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (02): : 173 - 178
  • [47] The characteristics of hydrogen diffusion and concentration around a crack tip concerned with hydrogen embrittlement
    Yokobori, AT
    Chinda, Y
    Nemoto, T
    Satoh, K
    Yamada, T
    CORROSION SCIENCE, 2002, 44 (03) : 407 - 424
  • [48] DRIFT-DIFFUSION MODEL OF HYDROGEN-ATOMS FOR HYDROGEN EMBRITTLEMENT IN POLYCRYSTALLINE NI(3)AL
    HAN, GW
    FENG, D
    YE, WJ
    SCRIPTA METALLURGICA ET MATERIALIA, 1994, 31 (05): : 559 - 564
  • [49] Effects of dislocations and hydrogen concentration on hydrogen embrittlement of austenitic 316 stainless steels
    Ye, Fengjiao
    Zhu, Te
    Mori, Kazuhiro
    Xu, Qiu
    Song, Yamin
    Wang, Qianqian
    Yu, Runsheng
    Wang, Baoyi
    Cao, Xingzhong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 876
  • [50] Hot corrosion of Fe3Al
    D. Das
    R. Balasubramaniam
    M. N. Mungole
    Journal of Materials Science, 2002, 37 : 1135 - 1142