Reduced-recoil-risk (RRR) rope is synthetic fiber rope which is designed to have a reduced tendency to completely break suddenly and to recoil catastrophically. The purpose is to reduce the risk of injuries and damage. The RRR rope usually breaks in a cascading manner which provides time to take corrective action or to "get out of the way" This feature also reduces the energy release at break and thus reduces the reach and impact of the broken rope. This paper discusses the new Cordage Institute (CI) RRR rope test method. It explains some of the physics of how such a rope reduces the risks of recoil. It demonstrates how to use the results of the CI test method to evaluate and compare the performance of different RRR rope designs. The additional stretch of the rope from its length at first break to its length at complete failure is an important RRR criteria. It can be used to calculate the time between first break and complete rope failure. Thus it is called warning-time stretch. Rope length is an important parameter. A short rope might not completely fail, but a longer rope of the same design will completely fail at first break. Rope size is another important parameter. For a given length, a small rope might break but a large rope might not. These principals apply to all ropes - fiber and wire, RRR design or not.
引用
收藏
页码:9 / 17
页数:9
相关论文
共 50 条
  • [31] Mooring lines with reduced recoil properties - Design, analysis and standardization
    Stenvers, D
    Wilke, W
    McCorkle, E
    Chou, R
    OCEANS '04 MTS/IEEE TECHNO-OCEAN '04, VOLS 1- 2, CONFERENCE PROCEEDINGS, VOLS. 1-4, 2004, : 1895 - 1899
  • [32] A novel TMR-based MFL sensor for steel wire rope inspection using the orthogonal test method
    Wu, B.
    Wang, Y. J.
    Liu, X. C.
    He, C. F.
    SMART MATERIALS AND STRUCTURES, 2015, 24 (07)
  • [33] Evaluation of seismic damage risk of elevator rope in high-rise building based on CCQC method
    Department of System Design Engineering, Keio University, Yokohama 223-8522, Japan
    不详
    US Natl. Can. Conf. Earthqu. Eng., Incl. Pap. Int. Tsunami Symp., 1600, (5865-5874):
  • [34] Research on Integrated Test System of Tank Recoil Mechanism
    Xu Zhenhui
    Song Wu
    Chen Tianli
    PROCEEDINGS OF THE THIRD INTERNATIONAL SYMPOSIUM ON TEST AUTOMATION & INSTRUMENTATION, VOLS 1 - 4, 2010, : 1509 - 1512
  • [35] Test method for determining the scuffing capacity of oils with reduced oil volume
    Gerges, Wassem
    Heipl, Oliver
    Pfeifer, Bernd
    Bartel, Dirk
    Wettlaufer, Marc
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2023, 237 (07) : 1568 - 1582
  • [36] A METHOD OF EXTENDING WIRE ROPE SERVICE LIFE
    WOOD, S
    CIM BULLETIN, 1982, 75 (842): : 61 - 64
  • [37] Method of designing hyperbolic rope couplings "MAMSar"
    Minasyan, Minas A.
    Minasyan, Armen M.
    MARINE INTELLECTUAL TECHNOLOGIES, 2024, (01): : 89 - 96
  • [38] A METHOD OF PREDICTING ROPE LIFE AND RESIDUAL STRENGTH
    FLORY, J
    PARSEY, M
    LEECH, C
    OCEANS 89, VOL 1-6: AN INTERNATIONAL CONFERENCE ADDRESSING METHODS FOR UNDERSTANDING THE GLOBAL OCEAN, 1989, : 1436 - 1441
  • [39] THE ROPE TRICK - ENERGY US MOMENTUM METHOD
    LITTLE, EM
    AMERICAN JOURNAL OF PHYSICS, 1950, 18 (09) : 579 - 579
  • [40] An efficient test pattern selection method for improving defect coverage with reduced test data volume and test application time
    Wang, Zhanglei
    Chakrabarty, Krishnendu
    PROCEEDINGS OF THE 15TH ASIAN TEST SYMPOSIUM, 2006, : 333 - +