Roll-to-roll manufacturing method of aqueous-processed thick LiNi0.5Mn0.3Co0.2O2 electrodes for lithium-ion batteries

被引:10
|
作者
Demiryurek, Ridvan [1 ]
Gurbuz, Nergiz [1 ]
Hatipoglu, Gizem [1 ,2 ]
Er, Mesut [1 ]
Malkoc, Hasan [1 ]
Guleryuz, Ozkan [1 ]
Uyar, Gulsen [1 ]
Uzun, Davut [1 ]
Ates, Mehmet Nurullah [1 ]
机构
[1] Sci & Technol Res Council Turkey TUBITAK, Energy Storage Div, Rail Transport Technol Inst RTTI, TR-41470 Kocaeli, Turkey
[2] Fraunhofer Inst Mat Recycling & Resource Strategi, Hanau, Germany
关键词
aqueous processing; crack-free coating; electrode manufacturing; lithium-ion batteries; WATER-SOLUBLE BINDERS; ELECTROCHEMICAL PERFORMANCE; CARBOXYMETHYL CELLULOSE; NEGATIVE ELECTRODES; ACTIVE MATERIAL; CATHODE; CAPACITY; POLYMER; STABILITY; CELLS;
D O I
10.1002/er.7171
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Aqueous-based slurry media for cathode electrode production offers a cleaner and safer environment during the electrode manufacturing step compared with the conventional organic solvent-based method used in the lithium-ion battery industry. In this work, carboxymethyl cellulose (CMC), styrene-butadiene rubber (SBR), and poly(ethylene oxide) (PEO) water-based binders are used to prepare LiNi0.5Mn0.3Co0.2O2 (NMC) cathode electrode. Detail electrochemical analysis reveals that the optimum mass ratio of CMC:SBR mixture is 1:2 when preparing an aqueous slurry for the NMC electrode. To mitigate particle cracking phenomenon during electrode drying step and obtain higher mass loading, a multi-layer coating technique is implemented. CMC-PEO binder mixture in aqueous media is also studied as an alternative aqueous processing method for NMC electrodes. The electrodes prepared with CMC-PEO mixture are demonstrated to be all crack-free, and electrochemical results indicate that the optimum mass loading of NMC electrode is between 15 and 18 mg cm(-2). This method is further tested in pouch cell format using a roll-to-roll pilot-scale production line to show the feasibility for commercial applications. Remarkably, pouch cell results manifest that aqueous-processed NMC cathode against graphite anode maintains its 89% capacity at 1C even after 1000 cycles. Highlights Water-based binders of carboxymethyl cellulose-poly(ethylene oxide) provide excellent cycling stability for LiNi0.5Mn0.3Co0.2O2 electrode. Multilayer coating allows electrodes for higher loadings without any crack formation. The water-based electrode preparation method is validated by pilot scale roll-to-roll electrode production line.
引用
收藏
页码:21182 / 21194
页数:13
相关论文
共 50 条
  • [1] Synthesis of Single Crystal LiNi0.5Mn0.3Co0.2O2 for Lithium Ion Batteries
    Li, Jing
    Li, Hongyang
    Stone, Will
    Weber, Rochelle
    Hy, Sunny
    Dahn, J. R.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (14) : A3529 - A3537
  • [2] Performance and ageing behavior of water-processed LiNi0.5Mn0.3Co0.2O2/Graphite lithium-ion cells
    Bichon, Marie
    Sotta, Dane
    De Vito, Eric
    Porcher, Willy
    Lestriez, Bernard
    JOURNAL OF POWER SOURCES, 2021, 483
  • [3] Effect of overcharge on the electrochemical and thermal safety behaviors of LiNi0.5Mn0.3Co0.2O2/graphite lithium-ion batteries
    Xie, Song
    Gong, Yize
    Ping, Xianke
    Sun, Jian
    Chen, Xiantao
    He, Yuanhua
    JOURNAL OF ENERGY STORAGE, 2022, 46
  • [4] Aqueous Lithium Carboxymethyl Cellulose and Polyacrylic Acid/Acrylate Copolymer Composite Binder for the LiNi0.5Mn0.3Co0.2O2 Cathode of Lithium-Ion Batteries
    Cui, Yan
    Chen, Jiahui
    Zhao, Jingyang
    Ma, Zhen
    Tan, Yuming
    Xue, Jianjun
    Xu, Hanliang
    Nan, Junmin
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2022, 169 (01)
  • [5] Improved electrochemical performance of bagasse and starch-modified LiNi0.5Mn0.3Co0.2O2 materials for lithium-ion batteries
    Caijian Zhu
    Jun Chen
    Shanshan Liu
    Boming Cheng
    Yong Xu
    Pengwei Zhang
    Qian Zhang
    Yutao Li
    Shengwen Zhong
    Journal of Materials Science, 2018, 53 : 5242 - 5254
  • [6] Improved electrochemical performance of bagasse and starch-modified LiNi0.5Mn0.3Co0.2O2 materials for lithium-ion batteries
    Zhu, Caijian
    Chen, Jun
    Liu, Shanshan
    Cheng, Boming
    Xu, Yong
    Zhang, Pengwei
    Zhang, Qian
    Li, Yutao
    Zhong, Shengwen
    JOURNAL OF MATERIALS SCIENCE, 2018, 53 (07) : 5242 - 5254
  • [7] Investigating the Compatibility of TTMSP and FEC Electrolyte Additives for LiNi0.5Mn0.3Co0.2O2 (NMC)-Silicon Lithium-Ion Batteries
    Haridas, Anulekha K.
    Nguyen, Quan Anh
    Terlier, Tanguy
    Blaser, Rachel
    Biswal, Sibani Lisa
    ACS APPLIED MATERIALS & INTERFACES, 2021, 13 (02) : 2662 - 2673
  • [8] Unravelling the Mechanism of Pulse Current Charging for Enhancing the Stability of Commercial LiNi0.5Mn0.3Co0.2O2/Graphite Lithium-Ion Batteries
    Guo, Jia
    Xu, Yaolin
    Exner, Moritz
    Huang, Xinrong
    Li, Yongchun
    Liu, Yanchen
    Wang, Hui
    Kowal, Julia
    Zhang, Qi
    Kristensen, Peter Kjaer
    Wang, Deyong
    Pedersen, Kjeld
    Gurevich, Leonid
    Stroe, Daniel-Ioan
    Adelhelm, Philipp
    ADVANCED ENERGY MATERIALS, 2024, 14 (22)
  • [9] Surface modification with oxygen vacancy in LiNi0.5Co0.2Mn0.3O2 for lithium-ion batteries
    Feng, Liwei
    Liu, Yan
    Wu, Lei
    Qin, Wenchao
    Yang, Zihao
    Liu, Jinfeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 881
  • [10] Effect of Duty Cycle on the Lifetime of Single Crystal LiNi0.5Mn0.3Co0.2O2/Graphite Lithium-Ion Cells
    Cheng, J. H.
    Harlow, J. E.
    Johnson, M. B.
    Gauthier, Roby
    Dahn, J. R.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2020, 167 (13)