Critical ageing of hydroxyapatite sol-gel solutions

被引:98
|
作者
Chai, CS [1 ]
Gross, KA [1 ]
Ben-Nissan, B [1 ]
机构
[1] Univ Technol Sydney, Dept Chem Mat & Forens Sci, Sydney, NSW 2007, Australia
关键词
hydroxyapatite; ageing; sol-gel; coating;
D O I
10.1016/S0142-9612(98)90138-7
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
It has been established that hydroxyapatite coatings can be produced using an alkoxide based sol-gel technique. Previous work showed that in addition to hydroxyapatite other phases including CaO were observed. A critical factor in determining the composition of the final coating is the period between solution preparation and coating deposition. The current study addresses how the ageing time affects the composition of the coating and the time required before a solution can be used to deposit monophasic coatings. Powders and coatings were produced with ageing times up to one week and examined with X-ray diffraction, thermal gravimetric analysis and differential thermal analysis. By depositing coatings after various ageing times, it was found that a solution ageing time of at least 1 day was required before monophasic hydroxyapatite coatings could be deposited. Thermogravimetric analysis showed that heating of the gel in air or in nitrogen both produced hydroxyapatite. Thermogravimetric analysis could be used as a simple and effective tool for identifying the critical ageing time required to produce high-purity hydroxyapatite coatings. (C) 1998 Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2291 / 2296
页数:6
相关论文
共 50 条
  • [41] Size Control of Electrospun Hydroxyapatite Nanofibers by Sol-Gel System
    Zhou Yuanyuan
    Li Yike
    Liu Qian
    Li Zhongjun
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2013, 13 (10) : 6581 - 6587
  • [42] Sol-gel derived hydroxyapatite/titania biocoatings on titanium substrate
    Xu, W
    Hu, WY
    Li, MH
    Wen, C
    MATERIALS LETTERS, 2006, 60 (13-14) : 1575 - 1578
  • [43] Phospholipid bilayer formation on hydroxyapatite sol-gel synthesized films
    Nellis, Barbara A.
    Satcher, Joe H., Jr.
    Risbud, Subhash H.
    COLLOIDS AND SURFACES B-BIOINTERFACES, 2011, 82 (02) : 647 - 650
  • [44] A STUDY OF THE SOL-GEL TRANSFORMATION OF GELATIN SOLUTIONS
    TANAKA, N
    UTSUMI, I
    BULLETIN OF THE CHEMICAL SOCIETY OF JAPAN, 1963, 36 (01) : 63 - 66
  • [45] Crystal growth of hydroxyapatite microplates synthesised by Sol-Gel method
    Mendez-Lozano, Nestor
    Apatiga-Castro, Lui M.
    Rivera-Munoz, Eric M.
    Manzano-Ramirez, Alejandro
    Gonzalez-Gutierrez, Carlos A.
    Zamora-Antunano, Marco A.
    MICRO & NANO LETTERS, 2019, 14 (14) : 1414 - 1417
  • [46] Adhesion strength of sol-gel derived fluoridated hydroxyapatite coatings
    Sam Zhang
    Zeng Xianting
    Wang Yongsheng
    Cheng Kula
    Weng Wenjian
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (22-23): : 6350 - 6354
  • [47] Interaction of a glass substrate with sol-gel solutions
    Atkarskaya, AB
    Kiyan, VI
    Mashir, YI
    GLASS AND CERAMICS, 2001, 58 (5-6) : 161 - 163
  • [48] Rheology of gelatin solutions at the sol-gel transition
    Peyrelasse, J
    Lamarque, M
    Habas, JP
    ElBounia, N
    PHYSICAL REVIEW E, 1996, 53 (06): : 6126 - 6133
  • [49] Effect of Solution and Calcination Time on Sol-gel Synthesis of Hydroxyapatite
    Turk, Serbuelent
    Altinsoy, Ibrahim
    Efe, Gozde Celebi
    Ipek, Mediha
    Ozacar, Mahmut
    Bindal, Cuma
    JOURNAL OF BIONIC ENGINEERING, 2019, 16 (02) : 311 - 318
  • [50] Microwave-assisted sol-gel synthesis of hydroxyapatite nanoparticles
    CHEN ChunYu
    DING Xuan
    LI ShouChuan
    SUN BaoChang
    LV ShanShan
    北京化工大学学报(自然科学版), 2019, 46 (03) : 7 - 15