Study of acetalization on poly(vinyl alcohol)/soybean protein fibers

被引:0
|
作者
Yan Dongyan [1 ]
Fu Changfei [1 ]
Gu Lixia [1 ]
机构
[1] Donghua Univ, State Key Lab Modificat Chem Fibres & Polymer Mat, Shanghai 201620, Peoples R China
关键词
PVA-SPF; acetalizing reaction; dialdehydes; cross-linking agent;
D O I
暂无
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Acetalizatioin of poly(vinyl alcohol)/soybean protein blend fibers(PVA-SPF) was studied. Dialdehydes were used as cross-linking agents to acetalize PVA-SPF. Latin square experiments were designed to determine the optimal acetalizing conditions: 41g/l dialdehyde A, 9min, 67 degrees C, where the tenacity of fiber was highest(3.76cN/dtex). FTIR spectra indicated the existence of cross-linking in acetalized PVA-SPF. Tensile test and boiling water shrinkage measurements showed that the physical properties of PVA-SPF crosslinked by dialdehydes were greatly improved comparing with those formalized PVA-SPF fibers.
引用
收藏
页码:768 / 770
页数:3
相关论文
共 50 条
  • [41] Preparation and characterization of alginate/poly(vinyl alcohol) blend fibers
    Fan, LH
    Du, YM
    Wang, XH
    Huang, RH
    Zhang, LN
    Hu, L
    JOURNAL OF MACROMOLECULAR SCIENCE-PURE AND APPLIED CHEMISTRY, 2005, A42 (01): : 41 - 50
  • [42] Structure and preparation of chitosan/poly(vinyl alcohol) blend fibers
    Zheng, Hua
    Du, Yu-min
    Yu, Jian-hui
    2000, Wuhan Univ, Wuhan, China (46):
  • [43] Electrospun poly(vinyl alcohol)/α-zirconium phosphate nanocomposite fibers
    Wei, Suying
    Lizu, Monira
    Zhang, Xi
    Sampathi, Jayanthi
    Sun, Luyi
    Milner, Matthew F.
    HIGH PERFORMANCE POLYMERS, 2013, 25 (01) : 25 - 32
  • [44] Properties of poly(vinyl alcohol)/montmorillonite nanocomposite fibers.
    Wang, YP
    Wang, YM
    Yan, DY
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2003, 225 : U547 - U547
  • [45] Electrospinning of poly(ethylene-co-vinyl alcohol) fibers
    Kenawy, ER
    Layman, JM
    Watkins, JR
    Bowlin, GL
    Matthews, JA
    Simpson, DG
    Wnek, GE
    BIOMATERIALS, 2003, 24 (06) : 907 - 913
  • [46] Electrospinning and stabilization of fully hydrolyzed poly(vinyl alcohol) fibers
    Yao, L
    Haas, TW
    Guiseppi-Elie, A
    Bowlin, GL
    Simpson, DG
    Wnek, GE
    CHEMISTRY OF MATERIALS, 2003, 15 (09) : 1860 - 1864
  • [47] Preparation and characterization of chitosan/poly(vinyl alcohol) blend fibers
    Zheng, H
    Du, YM
    Yu, JH
    Huang, RH
    Zhang, L
    JOURNAL OF APPLIED POLYMER SCIENCE, 2001, 80 (13) : 2558 - 2565
  • [48] MECHANICAL-PROPERTIES OF POLY(VINYL ALCOHOL) FIBERS AND COMPOSITES
    PEIJS, T
    VANVUGHT, RJM
    GOVAERT, LE
    COMPOSITES, 1995, 26 (02): : 83 - 90
  • [49] Enhanced tensile strength and initial modulus of poly(vinyl alcohol)/graphene oxide composite fibers via blending poly(vinyl alcohol) with poly(vinyl alcohol)-grafted graphene oxide
    Zhang, Shengchang
    Liu, Pengqing
    Zhao, Xiangsen
    Xu, Jianjun
    JOURNAL OF POLYMER RESEARCH, 2018, 25 (03)
  • [50] Enhanced tensile strength and initial modulus of poly(vinyl alcohol)/graphene oxide composite fibers via blending poly(vinyl alcohol) with poly(vinyl alcohol)-grafted graphene oxide
    Shengchang Zhang
    Pengqing Liu
    Xiangsen Zhao
    Jianjun Xu
    Journal of Polymer Research, 2018, 25