Investigation on effects of traverse speed and number of passes on mechanical and abrasive properties of AA7075-T6/ZrO2 surface nanocomposite produced using friction stir processing

被引:13
|
作者
Jamali, Amir [1 ]
Mirsalehi, Seyyed Ehsan [1 ]
机构
[1] Amirkabir Univ Technol, Dept Mat & Met Engn, Tehran Polytech, Tehran 158754413, Iran
关键词
Friction stir processing; ZrO2; nanoparticles; Surface composite; Traverse speed and Number of passes; Mechanical properties; Surface abrasive behavior; ALUMINUM-MAGNESIUM ALLOY; WELDED-JOINTS; MICROSTRUCTURE; FABRICATION; COMPOSITE; WEAR; NANOPARTICLES; SIZE; FSP;
D O I
10.1007/s40194-022-01331-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this study, a AA7075-T6/ZrO2 nanocomposite was successfully fabricated. The effects of the traverse speed and the number of passes on mechanical properties were evaluated. For this purpose, after examining the external surfaces of the samples, various test samples were extracted. Metallographic samples were first investigated with a stereomicroscope and an optical microscope. Then for more details, such as observing grains with higher resolution and distribution of nanoparticles in the matrix, the samples were studied with an electron microscope. XRD and EDS analyses were also performed to evaluate the formed phases. For a more detailed study, metallographic samples were used for the microhardness test. Tensile tests were performed to assess nanocomposites' yield and tensile strengths and to compare them with those of the base metal. Then, the fracture surfaces were examined under an electron microscope to observe and evaluate different aspects of fracture surfaces. Finally, an abrasion test was performed to assess the wear rate of nanocomposite samples and compare them with the base metal. Two main factors of grain and agglomeration sizes play important roles in the mechanical and wear properties. The Mean and max microhardness of the base metal was increased by 31.3% and 44% by nanocomposite production, respectively. Even though the tensile properties such as yield and tensile strength decreased compared to the base metal, they are better with a long-distance than annealed condition. Also, the wear rate in sample 30-1, which had minimum grain and agglomeration size, decreased up to 67% compared to the base metal.
引用
收藏
页码:2297 / 2313
页数:17
相关论文
共 50 条
  • [21] The role of stirring time on the metallurgical and mechanical properties during modified friction stir clinching of AA6061-T6 and AA7075-T6 sheets
    Memon, Shabbir
    Paidar, Moslem
    Ojo, Olatunji O.
    Cooke, Kavian
    Babaei, Behzad
    Masoumnezhad, Mojtaba
    RESULTS IN PHYSICS, 2020, 19
  • [22] Optimization of Operational Parameters in Friction Stir Welding of AA7075-T6 Aluminum Alloy Using Response Surface Method
    Farzadi, A.
    Bahmani, M.
    Haghshenas, D. F.
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2017, 42 (11) : 4905 - 4916
  • [23] Optimization of Operational Parameters in Friction Stir Welding of AA7075-T6 Aluminum Alloy Using Response Surface Method
    A. Farzadi
    M. Bahmani
    D. F. Haghshenas
    Arabian Journal for Science and Engineering, 2017, 42 : 4905 - 4916
  • [24] Influence of Traverse speed on Microstructure and Mechanical Properties of AA6082-TiC Surface Composite Fabricated by Friction Stir Processing
    Thangarasu, A.
    Murugan, N.
    Dinaharan, I.
    Vijay, S. J.
    INTERNATIONAL CONFERENCE ON ADVANCES IN MANUFACTURING AND MATERIALS ENGINEERING (ICAMME 2014), 2014, 5 : 2115 - 2121
  • [25] Research on the formation mechanism and mechanical properties of refill friction stir riveting (RFSR) joints of aluminium alloy AA7075-T6
    Zhao, Huan
    Liu, Yunpeng
    Ma, Yunwu
    Ping, Xuecheng
    Zhang, Dongzhe
    Li, Yongbing
    THIN-WALLED STRUCTURES, 2024, 198
  • [26] Experimental investigation on microstructure and mechanical properties of functionally graded AA7075 using friction stir processing
    Veeramallu K.
    Sunkari S.
    Mishikari N.
    Materials Today: Proceedings, 2022, 56 : 1551 - 1557
  • [27] Influence of tool rotational speed on the properties of friction stir spot welded AA7075-T6/Al 2 O 3 composite joint
    Suresh, S.
    Venkatesan, K.
    Natarajan, Elango
    Rajesh, S.
    MATERIALS TODAY-PROCEEDINGS, 2020, 27 : 62 - 67
  • [28] Correlation of microstructure, texture, and mechanical properties of friction stir welded Joints of AA7075-T6 plates using a flat tool pin profile
    Kesharwani, Rahul
    Jha, Kishor Kumar
    Imam, Murshid
    Sarkar, Chiranjit
    Barsoum, Imad
    HELIYON, 2024, 10 (03)
  • [29] Effect of Friction Stir Welding Process Parameters on Microstructure and Mechanical Properties of Dissimilar AA6061-T6 and AA7075-T6 Aluminum Alloy Joints
    Saravanan V.
    Rajakumar S.
    Muruganandam A.
    Metallography, Microstructure, and Analysis, 2016, 5 (6) : 476 - 485
  • [30] Investigation of the Effects of Tool Positioning Factors on Peak Temperature in Dissimilar Friction Stir Welding of AA6061-T6 and AA7075-T6 Aluminum Alloys
    Ghiasvand, Amir
    Suksatan, Wanich
    Tomkow, Jacek
    Rogalski, Grzegorz
    Derazkola, Hesamoddin Aghajani
    MATERIALS, 2022, 15 (03)