In the steam generators of nuclear power plants, the flow of cooling water can cause the tubes to vibrate, resulting in fretting wear damage due to contacts between these tubes and their supports. The tubes are made of Inconel 690 and Inconel 600 and the supports are made of STS 304. In this paper, fretting wear tests in water were performed using the materials Inconel 690 and Inconel 600 in contact with STS 304. Fretting tests using a cross-cylinder type set up were conducted under various vibrating amplitudes and applied normal loads in order to measure friction forces and wear volumes. Also, conventional sliding tests using a pin-on-disk type set up were carried out to compare these test results. In the fretting tests, friction force was found to be strongly dependent on normal load and vibrating amplitude. Coefficients of friction decreased with an increase in the normal load and a decrease in the vibrating amplitude applied. Also, the wear of Inconel 600 and Inconel 690 was predicted using a work rate model. Depending on the normal load and vibrating amplitude applied, distinctively different wear mechanisms and often drastically different wear rates occurred. It was found that the fretting wear coefficients for Inconel 600 and Inconel 690 were 9.3 x 10(-15) and 16.2 x 10(-15) Pa-1, respectively. This study shows that Inconel 690 can result in lesser friction forces and exhibits less wear resistance than Inconel 600 in room temperature water. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:97 / 105
页数:9
相关论文
共 50 条
  • [31] The synergy of corrosion and fretting wear process on Inconel 690 in the high temperature high pressure water environment
    Wang, Zihao
    Xu, Jian
    Li, Jie
    Xin, Long
    Lu, Yonghao
    Shoji, Tetsuo
    Takeda, Yoichi
    Otsuka, Yuichi
    Mutoh, Yoshiharu
    JOURNAL OF NUCLEAR MATERIALS, 2018, 502 : 255 - 262
  • [32] CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER
    Wang Jianqiu
    Huang Fa
    Ke Wei
    ACTA METALLURGICA SINICA, 2016, 52 (10) : 1333 - 1344
  • [33] The subsurface damage mechanism of Inconel 690 during fretting wear in pure water
    Li, J.
    Lu, Y. H.
    Xin, L.
    Shoji, T.
    TRIBOLOGY INTERNATIONAL, 2018, 117 : 152 - 161
  • [34] Fretting wear behavior of Inconel 690 in hydrazine environments
    Zhang, Xiao-yu
    Ren, Ping-di
    Peng, Jin-fang
    Zhu, Min-hao
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (02) : 360 - 367
  • [35] Wear Behavior of Plasma Nitrided Inconel 690 Alloy
    Kumar, Ravindra
    Sharma, Yogesh Chandra
    Vidyasagar, Vajja
    Bhardwaj, Dheeraj
    DAE SOLID STATE PHYSICS SYMPOSIUM 2018, 2019, 2115
  • [36] A STRESS-CORROSION CRACKING EVALUATION OF INCONEL 690 FOR STEAM-GENERATOR TUBING APPLICATIONS
    AIREY, GP
    VAIA, AR
    ASPDEN, RG
    NUCLEAR TECHNOLOGY, 1981, 55 (02) : 436 - 448
  • [37] Fretting wear properties of Inconel600 alloy at high temperature
    Xin, Long
    Ma, Miao
    Lu, Yong-Hao
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2015, 37 (07): : 928 - 935
  • [38] DEGRADATION OF INCONEL 600 MA STEAM-GENERATOR TUBES AND POTENTIAL REPLACEMENT MATERIALS
    BRICENO, DG
    HERNANDEZ, AML
    MARIN, MLC
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 1994, 21 (01) : 59 - 71
  • [39] Friction stir welding of Inconel alloy 600
    Fuxing Ye
    Hidetoshi Fujii
    Takuya Tsumura
    Kazuhiro Nakata
    Journal of Materials Science, 2006, 41 : 5376 - 5379
  • [40] Friction stir welding of Inconel alloy 600
    Ye, Fuxing
    Fujii, Hidetoshi
    Tsumura, Takuya
    Nakata, Kazuhiro
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (16) : 5376 - 5379