Fracture toughness of a ceramic-resin interface

被引:23
|
作者
Moharamzadeh, Keyvan [1 ]
Hooshmand, Tabassom [2 ]
Keshuad, Alireza [3 ]
Van Noort, Richard [1 ]
机构
[1] Univ Sheffield, Sch Clin Dent, Sheffield S10 2TA, S Yorkshire, England
[2] Univ Tehran Med Sci, Res Ctr Sci & Technol Med, Dent Res Ctr, Dept Dent Mat, Tehran, Iran
[3] Shahed Univ, Sch Clin Dent, Dept Prosthodont, Tehran, Iran
关键词
dental ceramics; luting resin; silane; fracture toughness; interface;
D O I
10.1016/j.dental.2007.04.002
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The purpose of this study was to compare the interfacial fracture toughness of smooth and roughened ceramic surfaces bonded with a luting resin using an optimized method of silane treatment. Methods. Ceramic discs were prepared with four different surface preparations (n = 20) consisting of (1) polished, (2) gritblasted, (3) hydrofluoric acid etched and (4) gritblasted and etched. The ceramic discs were then covered by a PTFE tape with a chevron shaped circular hole. The exposed surfaces were treated by an optimized silane treatment followed by an unfilled resin and then a luting resin. Specimens were then stored in distilled water at 37 degrees C for (A) 24h and (B) 30 days. The interfacial fracture toughness was measured, the mode of failure and fracture surfaces were also examined under a stereo-zoom microscope and a scanning electron microscope. Results. One-way ANOVA showed that there was no statistically significant difference in the mean interfacial fracture toughness for groups A1-A4 (P > 0.05). However, the mean interfacial fracture toughness for group B1 was significantly different from that for groups B2, B3 and B4 (P < 0.05). Independent-samples t-test results showed that there was a significant increase in the G(IC) mean value for groups B2 and B3 after 30 days water storage (P < 0.05). The modes of failure were predominantly interfacial or cohesive within the resin. Significance. it can be concluded that micro-mechanical retention by gritblasting the ceramic surfaces could be sufficient with no need for HF acid etching the ceramic surfaces when an appropriate silane application procedure is used. (c) 2007 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:172 / 177
页数:6
相关论文
共 50 条
  • [21] Fracture toughness of eutectic ceramic composite
    Ni, Xinhua
    Liu, Xiequan
    Han, Baohong
    Cheng, Zhaogang
    Zhong, Guohui
    Zhao, Lei
    Lixue Xuebao/Chinese Journal of Theoretical and Applied Mechanics, 2010, 42 (04): : 682 - 690
  • [22] Fracture toughness of ceramics and ceramic composites
    Gogotsi, GA
    CERAMICS INTERNATIONAL, 2003, 29 (07) : 777 - 784
  • [23] On the fracture toughness of ceramic matrix composites
    Kostopoulos, V
    Markopoulos, YP
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 250 (02): : 303 - 312
  • [24] On the fracture toughness of ceramic matrix composites
    Kostopoulos, V.
    Markopoulos, Y.P.
    Materials Science and Engineering: A, 1998, 250 (02): : 303 - 312
  • [25] FRACTURE-TOUGHNESS OF POROUS-MACHINABLE-CERAMIC RESIN COMPOSITES PREPARED FOR DENTAL APPLICATIONS
    LIAO, WM
    TANAKA, N
    SHINTANI, H
    TAIRA, M
    WAKASA, K
    YAMAKI, M
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1993, 12 (07) : 457 - 458
  • [26] TOUGHNESS, MICROSTRUCTURE AND INTERFACE CHARACTERISTICS FOR CERAMIC CERAMIC COMPOSITES
    OSMANI, H
    ROUBY, D
    FANTOZZI, G
    LEQUERTIER, JM
    COMPOSITES SCIENCE AND TECHNOLOGY, 1990, 37 (1-3) : 191 - 206
  • [27] SEVNB Method on Fracture Toughness of Ceramic
    Hu Yiwen
    Si Wenjie
    Gong Jianghong
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 155 - 158
  • [28] Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding
    Rona, Nergiz
    Yenisey, Murat
    Kucukturk, Gokhan
    Gurun, Hakan
    Cogun, Can
    Esen, Ziya
    JOURNAL OF PROSTHODONTIC RESEARCH, 2017, 61 (02) : 158 - 167
  • [29] Effect of Bleaching on Fracture Toughness of Resin Composites
    Cho, S. D.
    Bulpakdi, P.
    Matis, B. A.
    Platt, J. A.
    OPERATIVE DENTISTRY, 2009, 34 (06) : 703 - 708
  • [30] Fracture toughness of nine flowable resin composites
    Bonilla, ED
    Yashar, M
    Caputo, AA
    JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (03): : 261 - 267