Stressed-oxidation behavior of 2D CVI SiC/BN/SiC at elevated temperature in air

被引:6
|
作者
Han, Xiao [1 ,3 ]
Pan, Rong [5 ]
Shi, Jian [5 ]
Yu, Guoqiang [1 ,3 ]
Song, Fangxiao [1 ,3 ]
Gao, Xiguang [1 ,3 ]
Song, Yingdong [1 ,3 ,4 ]
Wang, Fang [2 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Key Lab Aeroengine Thermal Environm & Struct, Minist Ind & Informat Technol, Coll Energy & Power Engn, Nanjing 210016, Peoples R China
[2] Nanjing Forestry Univ, Coll Chem Engn, Nanjing 210016, Peoples R China
[3] Nanjing Univ Aeronaut & Astronaut, Coll Energy & Power Engn, Jiangsu Prov Key Lab Aerosp Power Syst, Nanjing 210016, Peoples R China
[4] Nanjing Univ Aeronaut & Astronaut, State Key Lab Mech & Control Mech Struct, Nanjing 210016, Peoples R China
[5] AECC Sichuan Gas Turbine Estab, Chengdu 610500, Peoples R China
关键词
SiC; BN; SiC composites; Intermediate temperature; Stressed-oxidation behavior; Strain-time curve; Failure mechanism; MATRIX COMPOSITES; BORON-NITRIDE; RUPTURE; MECHANISMS; LIFETIME; FIBERS; CARBON; DAMAGE;
D O I
10.1016/j.ceramint.2021.06.082
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The stressed-oxidation behaviors of 2D woven SiCf/BN/SiC composites were investigated at 950 degrees C and 1100 degrees C in air. The different proportions (60%-90%) of the ultimate tensile strength (UTS) at corresponding temperatures were chosen as constant stress. The stressed-oxidation experiments were taken to failure or interrupted (240h). The UTS decreases by 20.75% at 950 degrees C and 30.71% at 1100 degrees C. The composites did not fail during stressed oxidation when subjected to constant stress corresponding to the initial linear and the beginning of nonlinear segments of the tensile curve, above which the composites failed with a maximum failure life of about 10h. Fiber degradation due to the thermal exposure and the fiber cracks caused by the oxidation of BN interface coating and SiC fiber could be responsible for the strength degradation and failure of the composites during stressed oxidation.
引用
收藏
页码:28158 / 28166
页数:9
相关论文
共 50 条
  • [41] Oxidation resistance of 2D C/SiC composites fabricated by FCVI
    Wang, Chunpeng
    Tang, Jie
    Chen, Yufeng
    HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 : 1056 - 1058
  • [42] Tensile and in situ fibre properties of 3-D SiC/SiC-based composite tested at elevated temperature in vacuum and air with and without an oxidation protection system
    Davies, IJ
    Ishikawa, T
    Suzuki, N
    Shibuya, M
    Hirokawa, T
    Gotoh, J
    22ND ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: A, 1998, 19 (03): : 275 - 282
  • [43] Oxidation behavior of C/SiC-Ti3SiC2 at 800-1300°C in air
    Fan, Xiaomeng
    Yin, Xiaowei
    Ma, Yuzhao
    Zhang, Litong
    Cheng, Laifei
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (10) : 2427 - 2433
  • [44] Fatigue behavior of sylramic-iBN/BN/CVI SiC ceramic matrix composite in combustion environment
    D. J. Bertrand
    V. Sabelkin
    L. Zawada
    S. Mall
    Journal of Materials Science, 2015, 50 : 7437 - 7447
  • [45] Tensile and in situ fibre properties of 3-D SiC/SiC-based composite tested at elevated temperature in vacuum and air with and without an oxidation protection system
    Davies, Ian J.
    Ishikawa, Takashi
    Suzuki, Naoto
    Shibuya, Masaki
    Hirokawa, Tetsuro
    Gotoh, Jun
    Ceramic Engineering and Science Proceedings, 1998, 19 (03): : 275 - 282
  • [46] Oxidation and corrosion behavior of 2D laminated SiC/SiC with Si/mullite/BSAS EBC in dry oxygen/water vapor at 1200 °C
    Cao, Xinxin
    Luan, Xingang
    Wang, Yulei
    Zhang, Ziqi
    Li, Jianzhang
    Han, Guifang
    Cheng, Laifei
    CORROSION SCIENCE, 2023, 219
  • [47] Oxidation Behavior of SiCf/SiC Minicomposites with Multilayered (BN/SiC)n Interfacial Coatings under Humid Environment
    Jianwei Dai
    Limin He
    Zhenhua Xu
    Zaoyu Shen
    Zhen Zhen
    Guanxi Liu
    Rende Mu
    Journal of Materials Engineering and Performance, 2022, 31 : 10343 - 10353
  • [48] Fatigue behavior of sylramic-iBN/BN/CVI SiC ceramic matrix composite in combustion environment
    Bertrand, D. J.
    Sabelkin, V.
    Zawada, L.
    Mall, S.
    JOURNAL OF MATERIALS SCIENCE, 2015, 50 (22) : 7437 - 7447
  • [49] Oxidation Behavior of SiCf/SiC Minicomposites with Multilayered (BN/SiC)n Interfacial Coatings under Humid Environment
    Dai, Jianwei
    He, Limin
    Xu, Zhenhua
    Shen, Zaoyu
    Zhen, Zhen
    Liu, Guanxi
    Mu, Rende
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 10343 - 10353
  • [50] Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere
    Liu, Yongsheng
    Wan, Jiajia
    Zuo, Xinzhang
    Cheng, Laifei
    Zhang, Litong
    APPLIED SURFACE SCIENCE, 2015, 353 : 214 - 223