Structure-Property Correlation of Al-Mg-Si Alloys Micro-alloyed with Sn

被引:3
|
作者
Baruah, Monoj [1 ]
Borah, Anil [1 ]
机构
[1] Assam Engn Coll, Dept Mech Engn, Gauhati 13, Assam, India
关键词
Microstructure; mechanical properties; fractography; vacuum die-cast; hot rolling; micro-alloying Sn; Al-Mg-Si alloy; MICROSTRUCTURE; PRECIPITATION;
D O I
10.1007/s40962-021-00652-1
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Microstructure and mechanical properties of the cast and wrought Al-Mg-Si alloy micro-alloyed with 0.04 wt% and 0.08 wt% Sn were investigated at various processing conditions, viz. as-cast, solutionised, homogenised, hot rolled and peak-aged. Additionally, fracture surfaces of the alloys were also examined in the as-cast, peak-aged cast and peak-aged rolled conditions. It was observed that 0.04 wt% Sn favours the formation of a lamella-like eutectic Al + Mg2Si, whereas 0.08 wt% Sn favours the formation of plate/rod-like Mg2Si. The formation of the former deteriorated the hardness and tensile strength, but improves the ductility, whereas the formation of the later was found to contribute to the hardness, tensile strength as well as ductility of the Al-Mg-Si alloy. Homogenisation treatment had reduced the hardness of all the alloys to the lowest value due to the dissolution and spheroidisation of the intermetallic phases. However, hot rolling had significantly increased the hardness, tensile strength and ductility of the alloys. Thus, the increase in hardness, tensile strength and ductility were more prominent in the peak-aged rolled alloys relative to the peak-aged cast alloys. At the studied processing stages, the hardness and tensile strength of Al-Mg-Si alloy were found to decrease with the addition of 0.04 wt% Sn and increase with the addition of 0.08 wt% Sn. However, the ductility increased with Sn addition, and the increment was more prominent when micro-alloyed with 0.04 wt% Sn. Improvement in ductility in 0.04 wt% Sn alloy could be attributed to the formation of script-like Al(Fe, Mn)Si phase, whereas in 0.08 wt% Sn alloy could be attributed to the formation of ductile Mg-2(Si, Sn) phase. Furthermore, the fractography study had revealed that the fracture in the alloys was mainly developed by the cracking of Al(Fe, Mn)Si intermetallic particles. The fractures mode in the as-cast and peak-aged cast alloys was mainly by transgranular brittle with a cleavage fracture surface, whereas in the peak-aged rolled alloys was mainly by transgranular ductile with a dimpled fracture surface.
引用
收藏
页码:924 / 944
页数:21
相关论文
共 50 条
  • [41] Structure formation and multistep nucleation in CASTING Al-Mg-Si alloys
    Trudonoshyn, Oleksandr
    Prach, Olena
    Slyudova, Anna
    Lisovskii, Vitaliy
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2020, 33 (4-5) : 184 - 193
  • [42] Structure-dynamics relationship in Al-Mg-Si liquid alloys
    Fahs, Alaa
    Jarry, Philippe
    Jakse, Noel
    PHYSICAL REVIEW B, 2023, 108 (22)
  • [43] Effect of dynamic precipitation and twinning on dynamic recrystallization of micro-alloyed Mg-Al-Ca alloys
    Su, Jing
    Kaboli, Shirin
    Kabir, Abu Syed Humaun
    Jung, In-Ho
    Yue, Steve
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 587 : 27 - 35
  • [44] Influence of Sn on the age hardening behavior of Al-Mg-Si alloys at different temperatures
    Zhang, Xingpu
    Liu, Meng
    Sun, Haiming
    Banhart, John
    MATERIALIA, 2019, 8
  • [45] Effect of Sn contents on natural aging and precipitation hardening in Al-Mg-Si alloys
    Weng, Yaoyao
    Xu, Yaqi
    Ding, Lipeng
    Jia, Zhihong
    Zhang, Zongqing
    Chen, Jiahao
    Xie, Maoxuan
    Liu, Qing
    MATERIALS CHARACTERIZATION, 2021, 179
  • [46] Structure-property correlation of eutectic Al-12.4 Si alloys with and without Zirconium (Zr) addition
    Biswas, Prosanta
    Patra, Surajit
    Kumar Mondal, Manas
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2020, 33 (2-3) : 134 - 145
  • [47] Effect of Mg and Si Content on Microstructure and Property of Al-Mg-Si Alloy
    Ren Z.
    Luo B.
    Zheng Y.
    Gao Y.
    He C.
    Cailiao Daobao/Materials Reports, 2019, 33 (09): : 3072 - 3076
  • [48] Fabrication of Al-Si/graphite composites and their structure-property correlation
    Rajaram, G.
    Kumaran, S.
    Rao, T. Srinivasa
    JOURNAL OF COMPOSITE MATERIALS, 2011, 45 (26) : 2743 - 2750
  • [49] Influence of Mg/Si ratio on the clustering kinetics in Al-Mg-Si alloys
    Chang, Cynthia Sin Ting
    Liang, Zeqin
    Schmidt, Eric
    Banhart, John
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2012, 103 (08) : 955 - 961
  • [50] OBSERVATIONS ON THE ROLE OF MG AND SI IN THE DIRECTED OXIDATION OF AL-MG-SI ALLOYS
    NAGELBERG, AS
    JOURNAL OF MATERIALS RESEARCH, 1992, 7 (02) : 265 - 268