Phase transition and negative thermal expansion properties of Sc2-xCrxMo3O12

被引:22
|
作者
Wu, M. M. [1 ]
Peng, J. [2 ]
Han, S. B. [1 ]
Hu, Z. B. [3 ]
Liu, Y. T. [1 ]
Chen, D. F. [1 ]
机构
[1] China Inst Atom Energy, Beijing 102413, Peoples R China
[2] Chinese Acad Sci, Expt Phys Ctr, Inst High Energy Phys, Beijing 100049, Peoples R China
[3] Chinese Acad Sci, Coll Mat & Photoelect Technol, Grad Univ, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
Thermal expansion; Molybdates; X-ray diffraction; SOLID-SOLUTIONS; MOLYBDATES; TUNGSTATE; Y2MO3O12;
D O I
10.1016/j.ceramint.2012.05.033
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The crystal structure, phase transition and thermal expansion behaviors of solid solutions Sc2-xCrxMo3O12 (0 <= x <= 2) were investigated using X-ray diffraction (XRD) and differential scanning calorimetry (DSC). At room temperature, samples with x <= 0.7 and x >= 0.8 crystallize in orthorhombic and monoclinic structures, respectively. DSC result indicates that the phase transition of Sc0.5Cr1.5Mo3O12 from monoclinic to orthorhombic structure occurs at 203.66 degrees C. The linear thermal expansion coefficient of orthorhombic phases varies from -2.334 x 10(-6) degrees C-1 to 0.993 x 10(-6) degrees C-1 when x increases from 0.0 to 1.5. The near-zero linear thermal expansion coefficients of -0.512 x 10(-6) degrees C-1 and 0.466 x 10(-6) degrees C-1 are observed for compounds with x = 0.5 and 0.7, respectively. (c) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:6525 / 6529
页数:5
相关论文
共 50 条
  • [31] Phase transition temperature and negative thermal expansion of Sc-substituted In2(MoO4)3 ceramics
    Zhiping Zhang
    Yuenan Wang
    Weikang Sun
    Xiuyun Zhang
    Hongfei Liu
    Xiaobing Chen
    Xianghua Zeng
    Journal of Materials Science, 2020, 55 : 5730 - 5740
  • [32] Thermal, vibrational, and thermoelastic properties of Y2Mo3O12 and their relations to negative thermal expansion
    Romao, Carl P.
    Miller, Kimberly J.
    Johnson, Michel B.
    Zwanziger, J. W.
    Marinkovic, Bojan A.
    White, Mary Anne
    PHYSICAL REVIEW B, 2014, 90 (02):
  • [33] Electrospinning synthesis and negative thermal expansion of one-dimensional Sc2Mo3O12 nanofibers
    Liu, Hongfei
    Huang, Feiyu
    Wang, Wei
    Meng, Xiangdong
    Zhang, Zhiping
    CERAMICS INTERNATIONAL, 2023, 49 (07) : 10714 - 10721
  • [34] Fluorescent probe effect of super-sensitive transition Dy3+ ions in the negative thermal expansion materials Sc2W3O12
    Han, Lili
    Li, Qiangtong
    Wang, Lijuan
    Zhou, Wenqain
    Miao, Yifan
    Tian, Siyuan
    Fan, Yuncan
    He, Ziqi
    Ci, Zhipeng
    OPTICAL MATERIALS, 2024, 149
  • [36] Preparation and Thermal Expansion of Cu/Sc2W3O12 Composite
    Gao, Shuai
    Yang, Juan
    Ju, Xiangwen
    Zhou, Yazhou
    Cheng, Xiaonong
    Liu, Qinqin
    MATERIALS, INFORMATION, MECHANICAL, ELECTRONIC AND COMPUTER ENGINEERING (MIMECE 2016), 2016, : 74 - 78
  • [37] Phase transition and thermal expansion in W-substituted In2Mo3O12 ceramics
    Zhang, Zhiping
    Zhang, Hang
    Wang, Wei
    Meng, Xiangdong
    Liu, Hongfei
    CERAMICS INTERNATIONAL, 2023, 49 (22) : 36825 - 36830
  • [38] Preparation and optical, nanomechanical, negative thermal expansion properties of Sc2W3O12 thin film grown by pulsed laser deposition
    Liu, Hongfei
    Yang, Lu
    Zhang, Zhiping
    Pan, Kunmin
    Zhang, Fang
    Cheng, Honghui
    Zeng, Xianghua
    Chen, Xiaobing
    CERAMICS INTERNATIONAL, 2016, 42 (07) : 8809 - 8814
  • [39] Investigating negative thermal expansion property of decahedral Sc2Mo3O12 prepared via hydrothermal method
    Liu, Hongfei
    Zhang, Nan
    Zhang, Zhiping
    SOLID STATE SCIENCES, 2022, 132
  • [40] Preparation and characterization of negative thermal expansion Sc2W3O12/Cu core-shell composite
    Liu, Qinqin
    Yang, Juan
    Cheng, Xiaonong
    Liang, Guoshan
    Sun, Xiujuan
    CERAMICS INTERNATIONAL, 2012, 38 (01) : 541 - 545