Oxide microstructure and deuterium ingress in Zr-2.5Nb CANDU® pressure tubes

被引:5
|
作者
Woo, OT [1 ]
Lin, YP
Khatamian, D
机构
[1] Atom Energy Canada Ltd, Chalk River Labs, Chalk River, ON K0J 1J0, Canada
[2] Kinectrics, Toronto, ON M8Z 6C4, Canada
关键词
irradiated oxide microstructure; deuterium ingress; Zr-2.5; Nb;
D O I
10.3184/096034003782750178
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructures of oxides grown on the inside surface (water-side) of Zr-2.5Nb pressure tubes removed from CANDU(R)* reactors were characterised by TEM and correlated with deuterium ingress. Oxide cross-sections consisted of two structurally distinct regions: a columnar oxide region next to the metal/oxide interface, and an outer coarse equiaxed oxide region. Near the metal/oxide interface, the microstructure consisted of columnar grains without overt porosity. Away from the interface, the oxide consisted of coarsened equiaxed grains with (100)(m)-twins, grain-boundary cracks and nanopores. The oxide microstructures on various pressure tubes differ in the proportion of equiaxed grains. Electron micrographs suggest that a larger proportion of equiaxed grains is associated with higher deuterium uptake. The predominance of grain-boundary cracks in equiaxed oxides indicates that they are likely more permeable to water than columnar oxides. Energy dispersive X-ray analyses revealed substantial amounts of Fe-K-alpha (and Mn-K-alpha) in the equiaxed oxide grains at the outermost surface. Energy Dispersive X-ray mapping of Fe-K-alpha and detection of the Mn-K-alpha (produced by neutron activation of Fe-54 and subsequent decay of Fe-55) in the absence of external excitation, unequivocally demonstrated that the iron had accumulated in the oxide during reactor operation. The Fe concentration was highest near the outermost region, and decreased inwards towards the metal/oxide interface. These results are consistent with permeable equiaxed oxides picking up considerable amounts of Fe at the outermost region from the heavy water coolant.
引用
收藏
页码:593 / 600
页数:8
相关论文
共 50 条
  • [31] Effect of Irradiation Damage on the Deformation Properties of Zr-2.5Nb Pressure Tubes
    Griffiths, M.
    Wang, N.
    Buyers, A.
    Donohue, S. A.
    ZIRCONIUM IN THE NUCLEAR INDUSTRY: 15TH INTERNATIONAL SYMPOSIUM, 2009, 1505 : 541 - 549
  • [32] Overload fracture of flaw tip hydrides in Zr-2.5Nb pressure tubes
    Shek, Gordon K.
    Cui, Jun
    Perovic, Vuko
    Zirconium in the Nuclear Industry: 14th International Symposium, 2005, 1467 : 729 - 758
  • [33] Hydrogen ingress through EDM surfaces of Zr-2.5Nb pressure-tube material
    Chow, CK
    Brady, GR
    Urbanic, VF
    Coleman, CE
    JOURNAL OF NUCLEAR MATERIALS, 1998, 257 (01) : 35 - 43
  • [34] Determination of hydrogen and deuterium in Zr-2.5Nb by laser ablation
    Bickel, Grant A.
    Sopchyshyn, Fred C.
    McRae, Glenn A.
    Walker, Zane H.
    Green, Lawrence W.
    1998, Elsevier Sci B.V., Amsterdam, Netherlands (140) : 1 - 2
  • [35] Determination of hydrogen and deuterium in Zr-2.5Nb by laser ablation
    Bickel, GA
    Sopchyshyn, FC
    McRae, GA
    Walker, ZH
    Green, LW
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1998, 140 (1-2): : 217 - 228
  • [36] OXIDE THICKNESS MEASUREMENTS AND CHARACTERIZATION OF TWO Zr-2.5Nb PRESSURE TUBES OF EMBALSE NUCLEAR POWER PLANT
    Bordoni, R.
    Olmedo, A. M.
    ACTA MICROSCOPICA, 2011, 20 (01): : 10 - 20
  • [37] A study of the effect of extrusion parameters on the properties of extruded Zr-2.5Nb pressure tubes
    Keskar, Nachiket
    Raizada, Vikrant
    Kumar, Vaibhaw
    Jha, Sanjay K.
    Srivastava, Dinesh
    Dey, Gautam K.
    Saibaba, N.
    ADVANCES IN MATERIALS AND PROCESSING: CHALLENGES AND OPPORTUNITIES, 2012, 585 : 371 - +
  • [38] Mechanical Properties of Zr-2.5Nb Pressure Tubes Made from Electrolytic Powder
    Coleman, Christopher
    Griffiths, Malcolm
    Grigoriev, Viatcheslav
    Kiseliov, Vladimir
    Rodchenkov, Boris
    Markelov, Vladimir
    ZIRCONIUM IN THE NUCLEAR INDUSTRY: 15TH INTERNATIONAL SYMPOSIUM, 2009, 1505 : 699 - +
  • [39] Fe Distribution in Zr-2.5Nb Pressure Tubes having Variable Deformation Properties
    Trudeau, M. L.
    Serventi, A. M.
    Gauvin, R.
    MICROSCOPY AND MICROANALYSIS, 2009, 15 : 482 - 483
  • [40] In-reactor deformation of cold-worked Zr-2.5Nb pressure tubes
    Holt, R. A.
    JOURNAL OF NUCLEAR MATERIALS, 2008, 372 (2-3) : 182 - 214