- [31] Surface characteristics comparison between additively manufactured Ti6Al4V and wrought Ti6Al4V turned samples MATERIAL FORMING, ESAFORM 2024, 2024, 41 : 2050 - 2056
- [33] Deformation Behavior and Microstructure Evolution of Powder Metallurgy Ti6Al4V Alloy During Hot Compression Journal of Materials Engineering and Performance, 2019, 28 : 4454 - 4466
- [34] An in situ study on the role of heterogeneous microstructure on anisotropic tensile deformation behaviour in an additive manufactured Ti6Al4V alloy MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 924
- [37] Influence of processing parameters of selective laser melting (SLM) on additive manufactured titanium alloy (Ti6Al4V) PROCEEDINGS OF MECHANICAL ENGINEERING RESEARCH DAY 2020 (MERD'20), 2020, : 55 - 57
- [39] Deformation behavior and microstructure evolutions in Ti-6Al-4V extrusion THERMEC'2003, PTS 1-5, 2003, 426-4 : 719 - 724