Development of Secondary-fuel Injection Technology for Energy Reduction in Iron Ore Sintering Process

被引:5
|
作者
Oyama, Nobuyuki [1 ]
Iwami, Yuji [1 ]
Yamamoto, Tetsuya [1 ]
Machida, Satoshi [1 ]
Higuchi, Takahide [1 ]
Sato, Hideaki [1 ]
Sato, Michitaka [1 ]
Takeda, Kanji [1 ]
Watanabe, Yoshinori [2 ]
Shimizu, Masakata [3 ]
Nishioka, Koki [3 ]
机构
[1] JFE Steel Corp, Steel Res Lab, Hiroshima 7218510, Japan
[2] JFE Steel Corp, E Japan Works Keihin, Hiroshima 7218510, Japan
[3] Kyushu Univ, Dept Mat Sci & Engn, Fukuoka 812, Japan
关键词
sinter; sintering; gaseous fuel; temperature distribution; pore structure; pressure drop; GAS RECIRCULATION SYSTEM; COMBUSTION-RATE; PORE STRUCTURE; REDUCIBILITY; PERMEABILITY; CARBON; AGGLOMERATION; STRENGTH; PLANT; MODEL;
D O I
10.2355/tetsutohagane.97.510
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
JFE Steel Corporation developed the hydrogen-based gas fuel injection technology for sintering machines to improve sinter quality without increasing coke breeze ratio. With the technology, it is possible to extend the temperature zone between 1200 degrees C and 1400 degrees C by injecting the gaseous fuel from the top surface of the sintering machine as a partial substitute for coke breeze. Theoretical and experimental studies were carried out to verify the effect of the gaseous-fuel injection technology on pore structure in the sinter cake with the X-ray CT scanner and sintering pot test. It is important to hold the temperature between 1200 degrees C and 1400 degrees C in order to produce high strength and high reducibility sinter. The liquid phase ratio can be increased with extending the proper temperature zone by applying the gaseous fuel injection technology. The increase in liquid phase ratio promotes the combination of pores (1-5 mm) and sinter strength is improved. At the same time, the pores over 5 mm growth are promoted and the permeability is improved in the sintering bed. Moreover, the low-temperature sintering process depresses the iron ore self-densification. Micro pores under 1 mu m remain in unmelted ores and improve sinter reducibility. As a result, the technology enables to improve the pore structure in the sinter cake and sinter quality. The technology was put into commercial operation at Keihin No. 1 sinter plant in January 2009 and stable operation has continued up to the present. As a result, the enemy efficiency in the sintering process is greatly improved, and it has been achieved to reduce CO2 emissions by a maximum of approximately 60000 t/year at Keihin No. 1 sinter plant.
引用
收藏
页码:510 / 518
页数:9
相关论文
共 50 条
  • [31] Development of Sinter Quality and the Technology with Corresponding to the Change of Iron Ore Resources: 100 years of Sintering Process and to the Future
    Kawaguchi, Takazo
    Matsumura, Masaru
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2014, 100 (02): : 148 - 159
  • [32] Lignite Semicoke as a Fuel in Iron-Ore Sintering
    Strakhov, V. M.
    Surovtseva, I. V.
    Dolinskii, V. A.
    Karpenko, M. I.
    Islamov, S. R.
    COKE AND CHEMISTRY, 2007, 50 (08) : 219 - 225
  • [33] Review on alternative fuel application in iron ore sintering
    Kojo Alex, Acquah
    Shijie, Wang
    Fang, Hongming
    Wu, Xiaoxiong
    Chen, Wangsheng
    Che, Peilin
    Xu, Zhen
    IRONMAKING & STEELMAKING, 2021, 48 (10) : 1211 - 1219
  • [34] DEVELOPMENT OF OXIDATION-REDUCTION PROCESSES IN SINTERING OF IRON-ORE MATERIALS
    KOROTICH, VI
    KLIMOVA, NS
    KAPLUN, LI
    STEEL IN THE USSR, 1975, 5 (06): : 291 - 292
  • [35] IRON-ORE SINTERING PROCESS OPTIMIZATION
    Froehlichova, M.
    Ivanisin, D.
    Maslejova, A.
    Findorak, R.
    Legemza, J.
    ARCHIVES OF METALLURGY AND MATERIALS, 2015, 60 (04) : 2895 - 2899
  • [36] Lignite semicoke as a fuel in iron-ore sintering
    V. M. Strakhov
    I. V. Surovtseva
    V. A. Dolinskii
    M. I. Karpenko
    S. R. Islamov
    Coke and Chemistry, 2007, 50 (8) : 219 - 225
  • [37] STRENGTHENING REFRACTORY IRON ORE SINTERING WITH BIOMASS FUEL
    Fan, Xiaohui
    Ji, Zhiyun
    Gan, Min
    Chen, Xuling
    Li, Wenqi
    Yu, Zhiyuan
    3RD INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING, 2012, : 357 - 364
  • [38] Reduction of carbon emission in iron sintering process based on hot air sintering technology
    Li, Chaoqun
    Qin, Shuai
    Wang, Xue
    Zhu, Tingyu
    Song, Jianfei
    Zhao, Ruizhuang
    Xu, Wenqing
    JOURNAL OF CLEANER PRODUCTION, 2024, 471
  • [39] Numerical Modeling of the Iron Ore Sintering Process
    Zhou, Hao
    Zhao, Jia Pei
    Loo, Chin Eng
    Ellis, Benjamin George
    Cen, Ke Fa
    ISIJ INTERNATIONAL, 2012, 52 (09) : 1550 - 1558
  • [40] Dynamic process modelling of iron ore sintering
    Nath, NK
    DaSilva, AJ
    Chakraborti, N
    STEEL RESEARCH, 1997, 68 (07): : 285 - 292