Investigation of intermetallic compound and voids growth in fine-pitch Sn-3.5Ag/Ni/Cu microbumps

被引:14
|
作者
Wang, Dongfan [1 ]
Ling, Huiqin [1 ]
Sun, Menglong [1 ]
Miao, Xiaoying [1 ]
Hu, Anmin [1 ]
Li, Ming [1 ]
Dai, Fengwei [2 ]
Zhang, Wenqi [2 ]
Cao, Liqiang [2 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Met Matrix Composites, 800 Dongchuan Rd, Shanghai 200240, Peoples R China
[2] Chinese Acad Sci, Inst Microelect, Beijing 100029, Peoples R China
基金
中国国家自然科学基金;
关键词
CU/SN-3.5AG SOLDER JOINTS; MU-M DIAMETER; MULTIPLE REFLOW; SHEAR-STRENGTH; CU; PILLAR; NI; INTERCONNECTS; TEMPERATURE; RELIABILITY;
D O I
10.1007/s10854-017-8096-7
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Micron level Cu-pillar microbumps, which appear as the size of three-dimensional packaging shrinks down, have to introduce many unexpected reliability problems. The fast growth of intermetallic compounds (IMC) and voids tend to be a serious one. In this paper, the growth behaviors of IMC and voids were investigated in Sn-3.5Ag/Ni/Cu bumps, which were in the diameter ranging from 6 to 11 mu m and fabricated under same reflow process. The consequence manifested that the growth rate of interfacial IMC increased from 0.448 to 0.578 mu m/min as the bump diameter decreased from 11 to 6 mu m and the acquired IMC could be divided into two layers: the (Cu, Ni)(6)Sn-5 layer and Ni3Sn4 layer. As a result of the migration of Ni atoms, many voids were left in the interface between (Cu, Ni)(6)Sn-5 and Ni3Sn4. In the edge of Cu pillar, side wall wetting reaction was detected, which was confirmed by the formation of voids and (Cu, Ni)(6)Sn-5 phase. Further, as the bump diameter decreased, the side wall wetting reaction aggravated, which partly contributed to the acceleration of IMC growth.
引用
收藏
页码:1861 / 1867
页数:7
相关论文
共 50 条
  • [21] Investigation of the intermetallic compounds growth in 10μm Cu/Sn and Cu/Ni/Sn microbumps under isothermal temperature aging
    Yin, Yihao
    Ling, Huiqin
    Guo, Fayao
    Hu, Anmin
    Li, Ming
    2020 21ST INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2020,
  • [22] Effects of Current Stressing on Formation and Evolution of Kirkendall Voids at Sn-3.5Ag/Cu Interface
    Yu, C.
    Yang, Y.
    Lu, H.
    Chen, J. M.
    JOURNAL OF ELECTRONIC MATERIALS, 2010, 39 (08) : 1309 - 1314
  • [23] The formation and growth of intermetallic compounds between Sn-3.5Ag lead-free solder and Cu substrate
    Yu, DQ
    Duan, LL
    Zhao, J
    Lai, W
    FIFTH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY, PROCEEDINGS, 2003, : 327 - 329
  • [24] Intermetallic Compound Growth between Electroless Nickel/Electroless Palladium/Immersion Gold Surface Finish and Sn-3.5Ag or Sn-3.0Ag-0.5Cu Solder
    Oda, Yukinori
    Fukumuro, Naoki
    Yae, Shinji
    JOURNAL OF ELECTRONIC MATERIALS, 2018, 47 (04) : 2507 - 2511
  • [25] Intermetallic Compound Growth between Electroless Nickel/Electroless Palladium/Immersion Gold Surface Finish and Sn-3.5Ag or Sn-3.0Ag-0.5Cu Solder
    Yukinori Oda
    Naoki Fukumuro
    Shinji Yae
    Journal of Electronic Materials, 2018, 47 : 2507 - 2511
  • [26] Effects of Temperature and Current Stressing on the Intermetallic Compounds Growth Characteristics of Cu Pillar/Sn-3.5Ag Microbump
    Kwak, Byoung-Hyun
    Jeong, Myeong-Hyeok
    Park, Young-Bae
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2012, 51 (05)
  • [27] Effect of Cu content on the mechanical reliability of Ni/Sn-3.5Ag system
    Kim J.Y.
    Sohn Y.C.
    Yu J.
    Journal of Materials Research, 2007, 22 (3) : 770 - 776
  • [28] Effect of Cu content on the mechanical reliability of Ni/Sn-3.5Ag system
    Kim, J. Y.
    Sohn, Y. C.
    Yu, Jin
    JOURNAL OF MATERIALS RESEARCH, 2007, 22 (03) : 770 - 776
  • [29] Intermetallic growth activation energy improvement in graphene doped Sn-3.5Ag solder
    Mayappan, Ramani
    Salleh, Amirah
    MATERIALS LETTERS, 2022, 310
  • [30] Reaction diffusions of Cu6Sn5 and Cu3Sn intermetallic compound in the couple of Sn-3.5Ag eutectic solder and copper substrate
    Yoon, JW
    Lee, CB
    Kim, DU
    Jung, SB
    METALS AND MATERIALS INTERNATIONAL, 2003, 9 (02): : 193 - 199