Sliding wear of chromium carbide based cermets under different wear conditions

被引:0
|
作者
Juhani, K. [1 ]
Pirso, J. [1 ]
Viljus, M. [1 ]
Letunovits, S. [1 ]
机构
[1] Tallinn Univ Technol, EE-19086 Tallinn, Estonia
关键词
chromium carbide; cermets; sliding wear; wear coefficient; wear mechanism;
D O I
暂无
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Present paper considers the sliding wear properties of chromium carbide based cermets, produced by different methods and with different chemical compositions (10-30% of Ni), under different wear conditions. Sliding wear properties depend on the chemical composition and microstructure Of cermets and although on wear conditions. Sliding wear under normal load 40 N is surprising, sliding wear coefficient decreases in increase of binder content. Under higher normal loads wear coefficient increases in increase of binder content. Wear coefficient is highest for pure water conditions; wear coefficient in case of artificial seawater is lower than for dry and pure water conditions. Better wear resistance exhibited cermets produced by reactive sintering. Wear mechanism of chromium carbide based cermets is mainly dependent on thermal cracking and fatigue related crushing of large carbide grains and carbide framework and also adhesion.
引用
收藏
页码:455 / 459
页数:5
相关论文
共 50 条
  • [21] Effect of linear velocity on sliding wear behavior of TiCN based cermets
    Yadav, Prabhat Chand
    Sharma, Sandan Kumar
    Kumar, B. Venkata Manoj
    Kang, Sinhoo
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (09) : 17342 - 17349
  • [22] Optimization of dry sliding wear behavior of epoxy nanocomposites under different conditions
    Namdev, Anurag
    Purohit, Rajesh
    Telang, Amit
    Kumar, Ashish
    Saxena, Kuldeep K.
    Mabuwa, Sipokazi
    Msomi, Velaphi
    Mohammed, Kahtan A.
    MATERIALS RESEARCH EXPRESS, 2022, 9 (06)
  • [23] Friction and wear of HNBR with different fillers under dry rolling and sliding conditions
    Xu, D.
    Karger-Kocsis, J.
    Schlarb, A. K.
    EXPRESS POLYMER LETTERS, 2009, 3 (02): : 126 - 136
  • [24] Wear and wear transition in silicon carbide ceramics during sliding
    Cho, SJ
    Um, CD
    Kim, SS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (05) : 1247 - 1251
  • [25] Wear and wear transition mechanism in silicon carbide during sliding
    Korea Research Inst of Standards and, Science, Taejon, Korea, Republic of
    J Am Ceram Soc, 4 (1076-1078):
  • [26] DYNAMIC SEM WEAR STUDIES OF TUNGSTEN CARBIDE CERMETS
    BRAINARD, WA
    BUCKLEY, DH
    ASLE TRANSACTIONS, 1976, 19 (04): : 309 - 318
  • [27] TITANIUM CARBIDE (MO) CERMETS RESIST HEAT AND WEAR
    PECKNER, D
    MATERIALS ENGINEERING, 1968, 67 (05): : 37 - &
  • [28] PARTICULATE DENTAL COMPOSITES UNDER SLIDING WEAR CONDITIONS
    FRIEDRICH, K
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1993, 4 (03) : 266 - 272
  • [29] SLIDING WEAR OF NICKEL UNDER SOME ATMOSPHERIC CONDITIONS
    SASADA, T
    KANDO, H
    JOURNAL OF JAPAN SOCIETY OF LUBRICATION ENGINEERS, 1972, 17 (02): : 90 - &
  • [30] Characterization of wear particles generated from CoCrMo alloy under sliding wear conditions
    Pourzal, R.
    Catelas, I.
    Theissmann, R.
    Kaddick, C.
    Fischer, A.
    WEAR, 2011, 271 (9-10) : 1658 - 1666