Isothermal diffusion in uranium-plutonium-zirconium alloys

被引:19
|
作者
Petri, MC [1 ]
Dayananda, MA [1 ]
机构
[1] PURDUE UNIV,SCH MAT ENGN,W LAFAYETTE,IN 47907
关键词
D O I
10.1016/S0022-3115(96)00669-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Isothermal diffusion couple experiments were performed at 1023 K to investigate diffusion phenomena in body-centered cubic U-Pu-Zr alloys. The U-Pu-Zr alloys covered the uranium-rich comer of the ternary phase diagram with plutonium concentrations up to 27 at.% and zirconium concentrations up to 20 at.%, Ternary interdiffusion coefficients were calculated at the common composition between two couples with intersecting diffusion paths. The cross interdiffusion coefficient for zirconium ((D) over tilde(ZrPu)(U)) is negative and has a magnitude twice that of the main coefficient ((D) over tilde(ZrZr)(U)). In contrast, (D) over tilde(PuZr)(U) is negligible compared with (D) over tilde(PuPu)(U). (D) over tilde(PuPu)(U) is an order of magnitude greater than (D) over tilde(ZrZr)(U). Average effective interdiffusion coefficients were determined for all components over concentration ranges on the two sides of the Matano plane as well as for the entire diffusion zone of the couples. In general, these coefficients increase with increasing plutonium concentration and decrease with increasing zirconium concentration.
引用
收藏
页码:131 / 143
页数:13
相关论文
共 50 条