Synthesis and pyrolysis behavior of a soluble polymer precursor for ultra-fine zirconium carbide powders

被引:35
|
作者
Dong, Zhijun [1 ,2 ]
Zhang, Xian [1 ,2 ]
Huang, Qing [2 ]
Zhang, Jiang [2 ]
Zuo, Xiaohua [3 ]
Li, Wen [3 ]
Yuan, Guanming [2 ]
Li, Xuanke [1 ,2 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
[2] Wuhan Univ Sci & Technol, Hubei Prov Key Lab Coal Convers & New Carbon Mat, Wuhan 430081, Hubei, Peoples R China
[3] Hubei Polytech Univ, Sch Chem & Mat Engn, Huangshi 435003, Hubei, Peoples R China
基金
中国国家自然科学基金;
关键词
Zirconium carbide; Polymer precursor; Pyrolysis; Carbothermal reduction; LASER RAMAN-SPECTROSCOPY; PRECERAMIC POLYMERS; CARBOTHERMAL SYNTHESIS; SOL-GEL; CARBON; MICROSTRUCTURE; COMPOSITE; EVOLUTION; ZRC;
D O I
10.1016/j.ceramint.2015.02.039
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A soluble polymer precursor for ultra-fine zirconium carbide (ZrC) was successfully synthesized using phenol and zirconium tetrachloride as carbon and zirconium sources, respectively. The pyrolysis behavior and structural evolution of the precursor were studied by Fourier transform infrared spectra (FTIR), differential scanning calorimetry, and thermal gravimetric analysis (DSC TG). The microstructure and composition of the pyrolysis products were characterized by X-ray diffraction (XRD), laser Raman spectroscopy, scanning electron microscope (SEM) and element analysis. The results indicate that the obtained precursor for the ultra-fine ZrC could be a Zr O C chain polymer with phenol and acetylacetone as ligands. The pyrolysis products of the precursor mainly consist of intimately mixed amorphous carbon and tetragonal ZrO2 (tZrO(2)) in the temperature range of 300-1200 degrees C. When the pyrolysis temperature rises up to 1300 degrees C, the precursor starts to transform gradually into ZrC, accompanied by the formation of monoclinic ZrO2 (m-ZrO2). The carbothermal reduction reaction between ZrO2 and carbon has been substantially completed at a relatively low temperature (1500 degrees C). The obtained ultra-fine ZrC powders exhibit as well-distributed near-spherical grains with sizes ranging from 50 to 100 nm. The amount of oxygen in the ZrC powders could be further reduced by increasing the pyrolysis temperature from 1500 to 1600 degrees C but unfortunately the obvious agglomeration of the ZrC grains will be induced. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:7359 / 7365
页数:7
相关论文
共 50 条
  • [31] Ultra-fine zirconium diboride powders prepared by a combined sol–gel and spark plasma sintering technique
    Yang Miao
    Xiaojing Wang
    Paul Firbas
    Kun Wang
    Zhihua Yang
    Bin Liang
    Yi-Bing Cheng
    Dechang Jia
    Journal of Sol-Gel Science and Technology, 2016, 77 : 636 - 641
  • [32] Preparation and properties of Nd:YAG ultra-fine powders
    Chen Jiao
    Huang Xiaogu
    Wang Lixi
    Zhang Qitu
    JOURNAL OF RARE EARTHS, 2011, 29 (01) : 44 - 47
  • [33] RF plasma processing of ultra-fine hydroxyaptite powders
    Kumar, R
    Cheang, P
    Khor, KA
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 113 (1-3) : 456 - 462
  • [34] Preparation and properties of Nd:YAG ultra-fine powders
    陈娇
    黄啸谷
    王丽熙
    张其土
    JournalofRareEarths, 2011, 29 (01) : 44 - 47
  • [35] Creep Behavior and Fracture of Ultra-Fine Grained Commercial Purity Zirconium at Ambient Temperature
    Yang, Xirong
    Zhu, Zhen
    Liu, Xiaoyan
    Luo, Lei
    Zhao, Xicheng
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (03): : 815 - 819
  • [36] Creep Behavior and Fracture of Ultra-Fine Grained Commercial Purity Zirconium at Ambient Temperature
    Yang Xirong
    Zhu Zhen
    Liu Xiaoyan
    Luo Lei
    Zhao Xicheng
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (03) : 815 - 819
  • [37] Preparation Of BiFeO3 Ultra-Fine Powders
    Huaxue Tongbao/Chemistry Bulletin, (12):
  • [38] Sintering of ultra-fine iron powders under pressure
    Alymov, M.I.
    Myshlyaev, M.M.
    Fizika i Khimiya Obrabotki Materialov, 1997, (06): : 87 - 91
  • [39] Preparation and sintering behavior of ultra-fine Mo-30Cu composite powders
    State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China
    Cailiao Yanjiu Xuebao, 2009, 4 (363-368):
  • [40] Iron removal from ultra-fine silicon carbide powders with ultrasound-assisted and its kinetics
    Feng, Dong
    Ren, Quanxing
    Ru, Hongqiang
    Wang, Wei
    Ren, Shiyuan
    Jiang, Yan
    Liu, Baoyou
    Chang, Sixiao
    Zhang, Cuiping
    Yang, Yitong
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 247