Silane influence on bonding to CAD-CAM composites: An interfacial fracture toughness study

被引:15
|
作者
Eldafrawy, Maher [1 ]
Greimers, Laura [1 ]
Bekaert, Sandrine [1 ,2 ]
Gailly, Patrick [3 ]
Lenaerts, Cedric [3 ]
Nguyen, Jean-Francois [4 ,5 ]
Sadoun, Michael [6 ]
Mainjot, Amelie [1 ,2 ]
机构
[1] Univ Liege ULiege, Inst Dent, Dent Biomat Res Unit BRU, Liege, Belgium
[2] Univ Liege Hosp CHU, Inst Dent, Dept Fixed Prosthodont, Liege, Belgium
[3] Univ Liege ULiege, Ctr Spatial Liege, Surface Micro & Nano Engn Div, Liege, Belgium
[4] Univ Paris Diderot, UFR Odontol, Paris, France
[5] PSL Res Univ, Inst Rech Chim Paris, Chim ParisTech CNRS, Paris, France
[6] MaJEB Sprl, Liege, Belgium
关键词
Dental materials; Prosthetic dentistry; Dental prosthesis retention; Polymer-infiltrated ceramic network; Composite cement; High-temperature high-pressure; polymerization; Fracture mechanics; Notchless triangular prism test; Surface roughness; Biomaterials; RESIN CEMENTS; STRENGTH; SURFACE; GUIDANCE;
D O I
10.1016/j.dental.2019.05.019
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. To evaluate silane influence on the interfacial fracture toughness (IFT) of composite cement, with the two sub-classes of CAD-CAM composites, polymer-infiltrated ceramic networks (PICN) and dispersed fillers (DF), after hydrofluoric acid etching (HF) or airborneparticle abrasion (AB). A secondary objective was to correlate results with developed interfacial area ratio (Sdr) and surface wettability. Methods. Experimental PICN and DF blocks were cut into equilateral half-prisms, which were treated with HF or AB, then treated with an experimental silane or not and bonded to their counterparts with an experimental light-cure resin cement. After thermocycling, samples (n = 30 per group) were tested for IFT using the notchless triangular prism test in a water bath at 36 degrees C. Moreover, profilometry and contact angle measurement were performed on rectangular samples of each group. Finally, bonding interface was analysed by SEM. Results. PICN-HF treated with silane showed the highest IFT significantly. Three-way ANOVA revealed the influence of silane, material class and surface pre-treatment (HF or AB) on IFT (p <0.05). When silane was used, IFT was correlated with Sdr, while surface wettability was increased. Silane application significantly increased IFT for PICN but not for DF, while PICN performed better with HF and DF with AB. Significance. Silane increases IFT of composite cement with PICNs, but not with DF materials. Results suggest that silane increases the micromechanical bond by promoting resin cement spreading and penetration in surface roughness. This roughness is significantly higher for pre-treated PICNs than for DF due to their specific honeycomb microstructure when etched, which explains their better bonding properties. (C) 2019 The Academy of Dental Materials. Published by Elsevier Inc. All rights reserved.
引用
收藏
页码:1279 / 1290
页数:12
相关论文
共 50 条
  • [11] Influence of the Sintering Type in Ceramics Blocks for Cad-Cam
    Kreidler, Martin A. M.
    Oliveira, Osmir B., Jr.
    ODOVTOS INTERNATIONAL JOURNAL OF DENTAL SCIENCES, 2016, 18 (02) : 91 - 98
  • [12] INTERFACIAL FRACTURE ENERGY AND TOUGHNESS OF COMPOSITES
    MARSTON, TU
    ATKINS, AG
    FELBECK, DK
    JOURNAL OF MATERIALS SCIENCE, 1974, 9 (03) : 447 - 455
  • [13] CAD-CAM resin composites: Effective components for further development
    Yamaguchi, Satoshi
    Li, Hefei
    Sakai, Takahiko
    Lee, Chunwoo
    Kitagawa, Haruaki
    Imazato, Satoshi
    DENTAL MATERIALS, 2024, 40 (03) : 527 - 530
  • [14] Fracture resistance of endodontically treated premolars restored with CAD-CAM onlays
    Ozan, Gunce
    Eren, Meltem M.
    Dikmen, Benin
    Yildiz, Esra
    AMERICAN JOURNAL OF DENTISTRY, 2022, 35 (06): : 308 - 314
  • [15] Fracture Resistance and Microleakage of Endocrowns Utilizing Three CAD-CAM Blocks
    El-Damanhoury, H. M.
    Haj-Ali, R. N.
    Platt, J. A.
    OPERATIVE DENTISTRY, 2015, 40 (02) : 201 - 210
  • [16] From Artisanal to CAD-CAM Blocks: State of the Art of Indirect Composites
    Mainjot, A. K.
    Dupont, N. M.
    Oudkerk, J. C.
    Dewael, T. Y.
    Sadoun, M. J.
    JOURNAL OF DENTAL RESEARCH, 2016, 95 (05) : 487 - 495
  • [17] Assessment of interfacial fracture toughness in concrete composites
    Buyukozturk, Oral
    Lee, Kwang-Myong
    Cement and Concrete Composites, 1993, 15 (03) : 143 - 151
  • [18] Influence of different surface treatment on bonding of metal and ceramic Orthodontic Brackets to CAD-CAM all ceramic materials
    Haralur, Satheesh B.
    Alqahtani, Abdulrahman Mushabbab
    Shiban, Abdullah Saeed
    Alattaf, Zyad Muhammed
    Chaturvedi, Saurabh
    AlQahtani, Saeed M.
    Alqahtani, Nasser M.
    BMC ORAL HEALTH, 2023, 23 (01)
  • [19] Influence of different surface treatment on bonding of metal and ceramic Orthodontic Brackets to CAD-CAM all ceramic materials
    Satheesh B. Haralur
    Abdulrahman Mushabbab Alqahtani
    Abdullah Saeed Shiban
    Zyad Muhammed Alattaf
    Saurabh Chaturvedi
    Saeed M AlQahtani
    Nasser M Alqahtani
    BMC Oral Health, 23
  • [20] Effect of thermal cycling on fracture toughness of CAD/CAM materials
    Porto, Thiago Soares
    Roperto, Renato Cassio
    Akkus, Anna
    Akkus, Ozan
    Teich, Sorin
    Faddoul, Fady F.
    Porto-Neto, Sizenando de Toledo
    de Campos, Edson Alves
    AMERICAN JOURNAL OF DENTISTRY, 2018, 31 (04): : 205 - 210