PECULIARITIES IN THE STRUCTURE FORMATION AND CORROSION OF QUASICRYSTALLINE Al65Co20Cu15 ALLOY IN NEUTRAL AND ACIDIC MEDIA

被引:2
|
作者
Sukhova, Olena, V [1 ]
Polonskyy, Volodymyr A. [1 ]
机构
[1] Oles Honchar Dnipro Natl Univ, 72 Haharin Ave, UA-49010 Dnipro, Ukraine
来源
关键词
quasicrystalline Al65Co20Cu15 alloy; decagonal quasicrystals; structure; neutral and acidic aqueous solutions; corrosion resistance; AL-CU-CO; FE; MELTS; SOLIDIFICATION; PHASES;
D O I
10.2656.5/2312-4334-2021-3-07
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
In the present study, the structure and corrosion properties of quasicrystalline conventionally solidified Al65Co20Cu15 alloy cooled at 5 K/s were investigated. Structure was characterized by metallography, X-Ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy. Corrosion properties were determined by gravimetric and potentiodynamic methods at room temperature. The investigations performed confirm the peritectic formation of stable quasicrystalline decagonal D-phase that coexists with crystalline Al-4(Co,Cu)(3) and Al-3(Cu,Co)(2) phases in the structure of Al65Co20Cu15 alloy. According to energy dispersive spectroscopy, the stoichiometric composition of D-phase is Al65Co24Cu13. The susceptibility of the Al65Co20Cu15 alloy to corrosion significantly decreases with increasing pH from 1.0 (acidic media) to 7.0 (neutral medium). A corrosion rate of the Al65Co20Cu15 alloy in the aqueous acidic solutions (pH=1.0) increases in the order HNO3 -> HCl -> H2SO4 -> H3PO4. The mass of the specimens decreases in the solutions of H2SO4 or H3PO4 and increases in the solutions of FiNO(3) or HCl which relates to different rate ratios of accumulation and dissolution of corrosion products. The Al65Co20Cu15 alloy exhibits the highest corrosion resistance in the NaCl solution (pH=7.0) in which it corrodes under electrochemical mechanism with oxygen depolarization. The better corrosion resistance in sodium chloride solution is achieved due to the formation of passive chemical compounds blocking the surface. Free corrosion potential of the Al65Co20Cu15 alloy has value -0.43 V, the electrochemical passivity region extends from -1.0 V to -0.4 V, and a corrosion current density amounts to 0.18 mA/cm(2). Depending on media, two typical surface morphologies are revealed after corrosion of quasicrystalline specimens of the Al65Co20Cu15 alloy. In the H2SO4 and H3PO4 acidic solutions, clean specimens' surface due to its homogeneous dissolution is observed except for the more defective areas, such as boundaries of crystalline A(13)(Cu,Co)(2) phase containing less Co, which dissolve at a higher rate. In the HNO3, HCl or NaCl solutions, a porous layer on the surface is formed which is visually revealed as surface darkening. After staying in the NaCl solution, on the surface of the Al65Co20Cu15 alloy, the pits are also found due to preferential dissolution of components where the boundaries of Al-3(Cu,Co)(2) phase and flaws are located. Keywords: quasicrystalline Al65Co20Cu15 alloy, decagonal quasicrystals, structure, neutral and acidic aqueous solutions, corrosion resistance.
引用
收藏
页码:49 / 54
页数:6
相关论文
共 50 条
  • [21] Formation of a quasicrystalline phase in mechanically alloyed Al65Cu25Fe15
    Yong, X
    Chang, IT
    Jones, IP
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 387 (1-2) : 128 - 133
  • [22] THE EFFECT OF TRANSITION METALS ON QUASICRYSTALLINE PHASE FORMATION IN MECHANICALLY ALLOYED Al65Cu20Fe15 POWDER
    Mitka, M.
    Kalita, D.
    Goral, A.
    Litynska-Dobrzynska, L.
    ARCHIVES OF METALLURGY AND MATERIALS, 2020, 65 (03) : 1129 - 1133
  • [24] Tribological properties of Al65Cu20Cr15 quasicrystalline particles/Al matrix composite alloys
    Qi, Yuhong
    Zhang, Zhanping
    Hei, Zukun
    Yan, Li
    Dong, Chuang
    Mocaxue Xuebao/Tribology, 1998, 18 (02): : 129 - 135
  • [25] Mechanical properties of the Al65Cu20Fe15 alloy
    Larikov, LN
    Maksimenko, YO
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2000, 22 (08): : 64 - 66
  • [26] Peculiarities in Structure Formation and Corrosion of Cast Quasicrystalline Al63Cu25Fe12 and Al63Co24Cu13 Alloys in Sodium Chloride Aqueous Solution
    Sukhova, O., V
    Polonskyy, V. A.
    PHYSICS AND CHEMISTRY OF SOLID STATE, 2020, 21 (03): : 530 - 536
  • [27] OXIDATION INFLUENCE ON THE QUASICRYSTALLINE PHASES OF ALLOYS Al62.5Cu25Fe12.5 AND Al65Ni15Co20
    Jamshidi, L. C. L. A.
    Rodbari, R. J.
    Nascimento, L.
    Hernandez, E. P.
    Barbosa, C. M. B. M.
    MOROCCAN JOURNAL OF CHEMISTRY, 2018, 6 (03): : 445 - 454
  • [28] SHS of Al70Co15Ni15 and Al65Cu20Co15 Quasicrystals
    M. L. Busurina
    A. E. Sytschev
    P. A. Lazarev
    O. D. Boyarchenko
    A. O. Sivakova
    Yu. G. Morozov
    International Journal of Self-Propagating High-Temperature Synthesis, 2023, 32 : 215 - 220
  • [29] SHS of Al70Co15Ni15 and Al65Cu20Co15 Quasicrystals
    Busurina, M. L.
    Sytschev, A. E.
    Lazarev, P. A.
    Boyarchenko, O. D.
    Sivakova, A. O.
    Morozov, Yu. G.
    INTERNATIONAL JOURNAL OF SELF-PROPAGATING HIGH-TEMPERATURE SYNTHESIS, 2023, 32 (03) : 215 - 220
  • [30] 5-DIMENSIONAL STRUCTURE REFINEMENT OF DECAGONAL AL65CU20CO15
    STEURER, W
    KUO, KH
    PHILOSOPHICAL MAGAZINE LETTERS, 1990, 62 (03) : 175 - 182