Strength of the aluminium alloy 6082-T6 under high strain-rate conditions

被引:0
|
作者
Harrigan, J. J. [1 ]
Millett, J. C. F. [2 ]
Bourne, N. K. [2 ]
机构
[1] Univ Aberdeen, Dept Engn, Aberdeen AB24 3UE, Scotland
[2] AWE, Aldershot, Hants, England
关键词
plate impact; Hopkinson bar; 6082-T6; shear strength;
D O I
暂无
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
The measurement of shear strength via the use of lateral stress gauges has been shown to be a viable technique in a number of materials. An experimental investigation on the intermediate-rate behaviour and shock response of the aluminium. alloy, 6082-T6, is reported here. Results obtained using the lateral stress gauge technique show that the shear strength increases with impact stress. ne lateral stress behind the shock front is seen to be relatively flat, unlike many other face-centred cubic metals and alloys, where a decrease in lateral stress indicates an increase in shear strength. This unusual response may be a reflection of the high stacking fault energy of aluminium and its alloys resulting in a reduction of the work hardening (i.e. increases in dislocation and/or twin density). Further plate impact results show that the Hugoniot of 6082-T6 is in effect identical to that of the more widely known 6061-T6. Split Hopkinson pressure bar results are used to provide a fuller picture of the rate-dependant behaviour of 6082-T6 over a range of loading rates and conditions.
引用
收藏
页码:657 / +
页数:2
相关论文
共 50 条
  • [41] Dynamic load analysis of friction stir welded aluminium 6082-T6 joints
    Shukla, Himanshu
    WELDING INTERNATIONAL, 2025,
  • [42] High strain-rate fracture and failure of a high strength low alloy steel in compression
    Odeshi, A. G. d
    Bassim, M. N.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 525 (1-2): : 96 - 101
  • [43] Study on the fatigue strength of AA 6082-T6 adhesive lap joints
    Pereira, A. M.
    Ferreira, J. M.
    Antunes, F. V.
    Bartolo, P. J.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2009, 29 (06) : 633 - 638
  • [44] Investigation on Compressive Formability and Microstructure Evolution of 6082-T6 Aluminum Alloy
    Xu, Zhouli
    Ma, Huijuan
    Zhao, Ning
    Hu, Zhili
    METALS, 2020, 10 (04)
  • [45] Investigations of the microstructural response to a cold forging process of the 6082-T6 alloy
    Bouquerel, J.
    Diawara, B.
    Dubois, A.
    Dubar, M.
    Vogt, J. -B.
    Najjar, D.
    MATERIALS & DESIGN, 2015, 68 : 245 - 258
  • [46] Corrosion and passivation behavior of 6082-T6 aluminum alloy in NaCl solution
    Yang, Li
    Bai, Di
    Zhang, Chi
    Yang, Shoubing
    Wang, Dongxu
    Liu, Chaojie
    Ge, Tianqi
    Huang, Genzhe
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2023, 74 (04): : 622 - 629
  • [47] High strain-rate behaviour of a Tungsten alloy
    Cadoni, Ezio
    Dotta, Matteo
    Forni, Daniele
    1ST VIRTUAL EUROPEAN CONFERENCE ON FRACTURE - VECF1, 2020, 28 : 964 - 970
  • [48] Damage leading to ductile fracture under high strain-rate conditions
    J. P. Fowler
    M. J. Worswick
    A. K. Pilkey
    H. Nahme
    Metallurgical and Materials Transactions A, 2000, 31 : 831 - 844
  • [49] Strain rate effect and dynamic constitutive model of 7A04-T6 high-strength aluminium alloy
    Wan, Jun
    Zhu, Yong
    Zhang, Ying
    Zhao, Hui
    STRUCTURES, 2023, 53 : 1250 - 1266
  • [50] Damage leading to ductile fracture under high Strain-Rate conditions
    Fowler J.P.
    Worswick M.J.
    Pilkey A.K.
    Nahme H.