摘要
Al2O3 reinforced by SiC whiskers (Al2O3/SiC-W) was hot pressed to investigate the crack-healing behavior. Semi-elliptical surface cracks of 50 to 450 mu m in surface length were introduced using a Vickers indenter. The specimens containing pre-cracks were crack-healed at temperatures between 1000 degrees C and 1300 degrees C for 1h in air, and their strengths were measured by three-point bending tests at room temperature and elevated temperatures between 400 degrees C and 1300 degrees C. The results show that Al2O3/SiC-W possesses considerable crack-healing ability. The surface cracks with length of 2c = 100 mu m. could be healed by crack-healing at 1200 degrees C or 1300 degrees C. for 1h in air. The maximum crack size that can be healed for Al2O3/SiC-W is 2c = 200 mu m. Fracture toughness of the material was also determined. As expected, the SiC whiskers made their Al2O3 tougher.
引用
收藏
页码:276 / 283
页数:8
相关论文
共 50 条
  • [31] Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature
    Takahashi, Koji
    Kim, Byung-Soo
    Chu, Min-Cheol
    Sato, Shigemi
    Ando, Kotoji
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2002, 68 (07): : 1063 - 1070
  • [32] Crack-healing behavior under stress of mullite/silicon carbide ceramics and the resultant fatigue strength
    Ando, K
    Furusawa, K
    Chu, MC
    Hanagata, T
    Tuji, K
    Sato, S
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (09) : 2073 - 2078
  • [33] Strengthening of porous TiB2-SiC ceramics by pre-oxidation and crack-healing
    Zhang, Rubing
    Ye, Changshou
    Zhang, Yaoyao
    APPLIED SURFACE SCIENCE, 2016, 360 : 1036 - 1040
  • [34] Crack-healing behavior of silicon nitride ceramics under cyclic stress and resultant strength at crack-healed temperature
    Takahashi, K
    Ando, K
    Nakayama, S
    Murase, H
    Saito, S
    ADVANCED CERAMICS AND COMPOSITES, 2003, 247 : 275 - 278
  • [35] Surface crack in flexure (SCF) measurements of the fracture toughness of advanced ceramics
    Gettings, Robert J., 1600, American Ceramic Soc, Westerville, OH, United States (16):
  • [36] Improved Fracture Toughness and Crack Arrest Ability of Graphene–Alumina Nanocomposite
    V. R. Akhil Raj
    Komalakrushna Hadagalli
    Premanshu Jana
    Saumen Mandal
    Journal of Materials Engineering and Performance, 2021, 30 : 1234 - 1244
  • [37] Self-healing Ability of Structural Ceramics - A Review
    Madhan, M.
    Prabhakaran, G.
    TRENDS IN INTELLIGENT ROBOTICS, AUTOMATION, AND MANUFACTURING, 2012, 330 : 466 - 474
  • [38] Crack bifurcation in laminar ceramics having large compressive stress
    Hbaieb, K.
    McMeeking, R. M.
    Lange, F. F.
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2007, 44 (10) : 3328 - 3343
  • [39] CRACK ARREST FRACTURE TOUGHNESS OF A STRUCTURAL STEEL (A36).
    Ripling, E.J.
    Crosley, P.B.
    Welding Journal (Miami, Fla), 1982, 61 (03):
  • [40] Crack-healing behavior of hot-pressed TZ3Y20A-SiC ceramics
    Zhang, Xiu-Ping
    Ouyang, Jia-Hu
    Liu, Zhan-Guo
    Wang, Yu-Jin
    Zhou, Yu
    CERAMICS INTERNATIONAL, 2014, 40 (05) : 6611 - 6615